Today's
Sponsors:


Vintage Wood Products

VortexTool Co. Inc.

VyTek

W. Moore Profiles, Ltd.

W.L. Fuller

Wagner Electronic Products

WalzCraft Industries

WEIMA America, Inc.

Weinig Group - USA

Western Dovetail

Williams and Hussey

Wisconsin Knife Works

WMIA

WMMA

Wood Doctor's Rx, LLC

Wood Technology Inc

Wood-Mizer

WoodCabinetDoors.Com

WoodenBoat

WoodFinder

WoodJobs.com Search Consultants

WoodLINKS

Woodmaster

WoodPlanet Inc.

WoodSprayGuns.com

WOODWEB

Woodworker's Supply/woodworker.com

Woodworker's Directory

Woodworking in America

Wright Timber

Specialtytools.com

Speed Sander

Spink Lumber

Sprayguncaptain.com

Stefani

Steve H. Wall Lumber Co.

Stiles Machinery

Stiles Shop Solutions

Stoneys Hardwoods

Super Source Tooling Inc.

Supergrit Abrasives

Superior Wood Products

T-Tool USA LLC

Target Coatings

TaylorCraft Cabinet Door Company

Techno CNC Routers

Template Services

The Veneer Store

Thermwood Corporation

Tiger Wood Ltd.

TigerStop

TigerwoodDecking.com

TimberKing

Timesavers Inc.

TMS Machinery Sales

Tomlin Architectural Millwork

Tooling on the Web

Toolstoday.com

Top Drawer

Touch Up Solutions LLC

Tractivity

TradeJobPlacement.com

TradeSoft

Trakware Systems Inc.

TRB Flooring Company

Tropical Hardwoods

True North Cedar

Ubidmachinery Inc.

UC Coatings Corp.

Unique Building Supples

Unique Machine & Tool

University of Wisconsin

UWMO Auctions

VacDry Kilns

Vacuum Pressing Systems, Inc.

Vacuumpods.com

Valspar

Vecoplan LLC

Vector Art 3D

Vectric Ltd.

Veneer Systems Inc.




Duplicating a black lacquer finish       Methods and products for achieving a good black laquer finish. March 20, 2001

Question
What is the best way to duplicate a black lacquer finish?

Forum Responses
Here is what I like to do with lacquer: Use black or dark gray primer to prep the surface and get it smooth. When this is sanded perfectly smooth, shoot a double coat (wet on wet) of gloss black N/C lacquer. When this is dry, I use a couple coats of a high-grade (tabletop or bar top lacquer) gloss topcoat. This system will give you much better mar-resistance and depth. Pigmented products mar easily compared to clear gloss.

Bob Niemeyer, forum technical advisor



Recently I had a job in black where I used Sherwood's Vinyl Basecoat product. (I think the cat# on the black is pb63.) What a wonderful product for doing black finishes! I may never use primer and pigmented lacquer again. It's a thin product. For opaque black, you spray it on in barely wet coats, then follow with your clear topcoats. It reaches a full opaque color, if you want, or degrees in between.

What amazed me is how this product colors in the pores of an open-grained wood without the use of a primer or wood filler. Of course, if you want a filled grain appearance on an open-pored wood, you'd still need to use a filler or primer.



What type of primer do you recommend for black lacquering?


You can make most sealers black by adding Huls or CreaNova 844 Lamp Black colorant. This includes most vinyl sealers.

Bob Niemeyer, forum technical advisor



Sherwin Williams makes a very good black primer/surfacer for nc lacquer. Clawlock also comes in black for catalyzed lacquer. On nc lacquer, I don't like clear coating as it tends to gray out the black and also makes it difficult to touch-up.


Emron by Dupont "Featherfil" is another primer/sealer that is a great product. It fills the grains, and leaves an excellent base, for any coating, including polyurethane and polyester. Use a respirator.


I have used ML Campbell's Microton black dye stain as a base coat. I apply numerous coats via spray application until the desired opacity is achieved and then topcoat with one thin coat of water white vinyl sealer. Too much sealer will give you a cloudy appearance. Topcoat with virtually any clear, depending on the end use of the piece. I usually use Krystal and the durability is outstanding and I don't have the problem of a soft coating as seen with traditional black lacquer.


The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor A:
I use ML Campbell's Magnamax Gloss tinted black. I sand to 180 grit, spray first coat, sand, spray second coat, sand, then apply two coats of Magnamax clear gloss, sanding between coats. Finish by rubbing out top coat... an awesome look!



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.