Question
I am getting ready to finish MDF paint grade cabinet doors. Should I use a urethane based paint or would a pigmented lacquer give me sufficient coverage and durability?

Forum Responses
We use pigmented lacquer all the time on MDF with great results. Pay extra attention to the raw edges when priming and sanding because it really soaks it up. I usually prime the raw areas first, then sand lightly. Prime and sand as usual, then two topcoats. When you prime, use as little thinner as possible. The primer will not seal the edges if it is thinned too much.



Rather than priming the edges of MDF, you will find better results 'sizing' them. This is a mixture of wood glue and water at about a 1 to 1 ratio that can be brushed on the MDF edges with a disposable paint brush. This step is done prior to any finishing and will need to be lightly sanded after the mixture sets up. You will need to first remove all machining marks (saw or jointer) before you apply the sizing or else you chance sanding it all away in the process of removing the machining marks. Sizing also works well to seal porous end grain.


We use products specifically for MDF. We have found Campbell makes a product called Clawlock and Chemcraft makes a product called Plastoprimer. We like the Plastoprimer better as it does not shadow when spraying. These products are both catalyzed. Generally two prime coats followed with one topcoat looks great.


You can also use drywall compound to seal the edges. Thin it down just a little, smear it on and sand it smooth, then prime. Works great.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing

  • KnowledgeBase: Finishing: High Speed Production

  • KnowledgeBase: Woodworking Miscellaneous

  • KnowledgeBase: Woodworking Miscellaneous: Woodworking


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2017 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article