      Cooling solutions tend to make the table slippery and interfere with vacuum holding ability. Here are some tips for working with metal on the CNC. April 16, 2009

Most of our machining is wood and plastic related, but lately we have been trying some non-ferrous metals. The double sided masking tape we use in addition to the vacuum holds parts nicely, but when we are working with metals we have to use coolant. We are only using soapy water, and working on a sheet of plastic to keep our MDF spoilboard dry, but as soon as the water gets to the tape, the parts move. We have tried spray-glue and contact cement, with very poor results. Any ideas on holding down small parts cut out of sheets of aluminum or copper using water coolant?

Forum Responses
(CNC Forum)
From contributor B:
Seems to me your best (and perhaps only) bet would be to onion skin the parts.

From contributor R:
Depending on the software you are programming with, you may be able to leave tabs to hold the parts to the web. I know that Alphacam and Microvellum can do this; I'm sure others can as well. If your software can't do it within the program, it should not be too hard to add then in a thin sheet application.

From contributor M:
Speeds and feeds, cutter geometry, cutter diameter, machining strategies and cutter fluid application become considerably more critical when cutting aluminum and copper. There are many reasons, but essentially the "bandwidth" of cutting parameters (constant surface footage, material removal rates, chip loads, tool edge life) is much smaller and finite for metals than for wood and plastic. It becomes much more sensitive to the conditions of the particular setup and application.

You mentioned a soapy water solution. I am unsure of the method of delivery, but I would recommend a soluble oil solution (1 part oil - 20 parts water) delivered via pneumatic mister.

Also, typically you should be running in an rpm band of less than half that of normal wood and plastics machining. Chip load would be cutter specific. Tabbing would also be recommended on smaller parts.

From contributor A:
It may not be the answer you are looking for, but one more option would be to subcontract the job to a laser or plasma shop. I have seen thousands of very tiny parts nested on a sheet, like special washers smaller than a dime with intricate detail cut on a laser. No side force, no movement.

From contributor O:
Have you tried air for cooling? A nozzle directed at the point of cutting with one of those articulated stiff air lines.

From contributor A:
Here's an idea - may be practical or not depending on how small is small for your parts. Perhaps you could use a plastic or metal tray - could be the size of your spoilboard, half that size, or just slightly larger than your parts to contain the water for coolant. Then use a double sided pod or a custom shop made pod stuck to the bottom of the tray or to a half inch block glued to the bottom of the tray. The gaskets may provide a good water seal and keep the parts stuck. You would only need to make the tray once and it would keep the water contained for you as well.

From contributor K:
Rather than using any liquid, I would purchase a cold air gun. The brand I use is Vortec. It uses vortex tube technology to lower the compressed air temp around 75 deg lower than ambient.

From the original questioner:
Thanks for all of the ideas. I have kind of hybridized my approach, using a combination of several methods. First I had a new aperture machined so I'm only putting out mist. Second, I have switched to an acrylic film tape that is double sided. Third I have built a wet-dry shop vac attachment to suck up any extra liquid, as the pooling was compromising the tape more than anything. This last suggestion from contributor K, however, is really interesting. I checked out the vortex site and sub-zero spot cooling looks like about the coolest thing I've seen since we started running the CNC. Thanks for the help. I'm running a few more tests tomorrow!

From contributor S:
Try tabbing the parts and using a downcut bit.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Computerization

  • KnowledgeBase: Computerization: CNC Machinery and Techniques

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2017 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article