Machining a Chamfer in Aluminum Plate

      Carbide bits designed for wood will work acceptably well in soft non-ferrous metals. August 15, 2011

I need to put a 45 chamfer on aluminum. The chamfer is only 5/16" by 5/16". Can I use a carbide tipped chamfer bit run at slow speed to make the cut? Or do I need to use an end mill? Whatever bit I use, I can use it in a router or in my milling machine. The cost of each is roughly the same ($32). The chamfer must be perfect, that is exactly 45 to either edge of the aluminum plate. The plate is 3/4" thick and 6061-T6.

Forum Responses
(Solid Wood Machining Forum)
From contributor R:
I've done it both ways. The carbide router will work fine. I learned by experimenting. I can pretty much work all non-ferrous with standard wood tooling. Negative hook blades on the saws are designed for non-ferrous. That's another option as well - table saw!

From the original questioner:
Thank you, and away I go.

From contributor J:
Use the router bit, but do it in two passes. One shallower, and then one to get your final depth. Those chips will be hot too.

From contributor R:
The chips aren't that hot. A face shield would be best. The heat from the chips will make you flinch. For a straight cut, the table saw is great. Chances are you already own a negative hook blade from your radial arm or chop saw. If using a router table, you might want to put a cloth filter on the motor top, as this is the air intake and could suck some aluminum chips in, which are electrically conductive.

Non-ferrous can be done with many standard woodworking tools. I've even jointed aluminum and brass. There's another option for your chamfer. It doesn't get close to hot enough to set anything on fire, but keep the dust collector off for your own peace of mind until you see this for yourself.

From contributor D:
A regular carbide tipped 45 degree chamfer bit with a bearing is much easier than the end mill. We sell many wood designed bits that are used on aluminum or other soft metals; they work fine and are much cheaper than having one made with less hook for aluminum. We do, however, make custom bits for large industrial shops that require long runs.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Solid Wood Machining

  • KnowledgeBase: Solid Wood Machining: Tooling

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article