Today's
Sponsors:


Vintage Wood Products

VortexTool Co. Inc.

VyTek

W. Moore Profiles, Ltd.

W.L. Fuller

Wagner Electronic Products

WalzCraft Industries

WEIMA America, Inc.

Weinig Group - USA

Western Dovetail

Williams and Hussey

Wisconsin Knife Works

WMIA

WMMA

Wood Doctor's Rx, LLC

Wood Technology Inc

Wood-Mizer

WoodCabinetDoors.Com

WoodenBoat

WoodFinder

WoodJobs.com Search Consultants

WoodLINKS

Woodmaster

WoodPlanet Inc.

WoodSprayGuns.com

WOODWEB

Woodworker's Supply/woodworker.com

Woodworker's Directory

Woodworking in America

Wright Timber

Specialtytools.com

Speed Sander

Spink Lumber

Sprayguncaptain.com

Stefani

Steve H. Wall Lumber Co.

Stiles Machinery

Stiles Shop Solutions

Stoneys Hardwoods

Super Source Tooling Inc.

Supergrit Abrasives

Superior Wood Products

T-Tool USA LLC

Target Coatings

TaylorCraft Cabinet Door Company

Techno CNC Routers

Template Services

The Veneer Store

Thermwood Corporation

Tiger Wood Ltd.

TigerStop

TigerwoodDecking.com

TimberKing

Timesavers Inc.

TMS Machinery Sales

Tomlin Architectural Millwork

Tooling on the Web

Toolstoday.com

Top Drawer

Touch Up Solutions LLC

Tractivity

TradeJobPlacement.com

TradeSoft

Trakware Systems Inc.

TRB Flooring Company

Tropical Hardwoods

True North Cedar

Ubidmachinery Inc.

UC Coatings Corp.

Unique Building Supples

Unique Machine & Tool

University of Wisconsin

UWMO Auctions

VacDry Kilns

Vacuum Pressing Systems, Inc.

Vacuumpods.com

Valspar

Vecoplan LLC

Vector Art 3D

Vectric Ltd.

Veneer Systems Inc.




Mahogany Supply and Varieties       More info on what "Mahogany" really means, and information on the availability of various types. April 6, 2007

Question
I build period reproduction furniture. I use a lot of genuine SA mahogany. I am trying to match the no longer available Cuban or Santa Domingan mahogany used in the 18th century. Does anybody have experience with any of the African mahogany substitutes for genuine mahogany, such as utile or sapele? South American mahogany is becoming very scarce and very expensive in our area. It is especially hard to find thicker stock. Anyhow, the lumberyard is pushing utile as very similar with just lighter color that can be dyed to look like genuine. I am very concerned about using this for period furniture that contains hundreds of hours with carvings, veneers and inlays. My inclination is to order the real mahogany and pay shipping charges on top.

Forum Responses
(Architectural Woodworking Forum)
From contributor E:
The African mahoganies I've seen are just not the same. More coarse, not the same grain or coloring.



From contributor L:
Sapele looks pretty close; the graining is a little more pronounced.


From contributor C:
What we refer to as Honduras mahogany is always available in the better pattern grade in most thickness FAS rough 5.50 and up. Sapele is more like the typical Honduras from 15 years ago, but very similar. I usually buy 40-50% extra to allow for picking and choosing to assure decent grain match-ups. African mahogany is similar in some boards, but I notice more variation in color and weight than I would ideally like.


From contributor D:
If you are doing period reproduction, then the Cuban would be first choice, then Honduras. I would stay away from the others since they are not mahogany except in the minds of the marketers.

Cuban is somewhat available in Florida after the big storms take down trees, but it is not inexpensive. We buy a lot of 10/4 and 8/4 Honduras from a great source, but they - like others - are not taking new customers on the mahogany. We can all hope Brazil gets it together and returns to exporting the Honduras they have been holding. Hey, if we normalized relations with that oh so evil Cuba, then we would have easier access to the Cuban mahogany. Politics!



From contributor K:
I have been seeing good supplies of Spanish cedar in my area. Have you tried it?


From contributor J:
I've been experiencing the same issues with mahogany. It's been explained to me that there are different species of "African Mahogany" - some nice and some not so nice. For what it is worth, I have had pretty good luck with Okoume when it comes to hardwoods.


From Professor Gene Wengert, forum technical advisor:
There are only two African mahogany species. The Latin names (genus and species) are Khaya grandifoliola and K. senegalensis.

Okoume has the name of Aucoumea klaineana, so it is not even in the same genus as African mahogany. Its properties are not that close either.

Sapele is Entandrophragma cylindricum.

"Tropical Timbers of the World" by Chudnoff is online. Many local African names are often difficult to relate to Latin names; further export names may not be easy to relate either. The names are so variable and sometimes locally creative too.



From contributor F:
Spanish cedar is becoming tight and Honduras mahogany may not be available at all by the end of 2007. Check out the endangered species and CITES lists to avoid surprises.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Buying

  • KnowledgeBase: Lumber & Plywood: Wood Identification




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article