Method for estimating air-drying times of lumber
Published information on estimated air-drying times of lumber is of limited usefulness because it is restricted to a specific location or to the time of year the lumber is stacked for drying. At best, these estimates give a wide range of possible times over a broad range of possible locations and stacking dates. In this paper, we describe a method for estimating air-drying times for specific locations by optimizing a drying simulation using existing experimental air-drying times for northern red oak, sugar maple, American beech, yellow-poplar, ponderosa pine, and Douglas-fir. The results of the optimization are simulation parameters that make it possible to estimate the air-drying times of these species regardless of when they are stacked, in any location where average tem- perature and relative humidity are known, and for lumber of any thickness dried to any moisture content. 2001
This article is in PDF format (file size: 313 kb).
To download this article, right click on the link immediately below
and choose "save target as". To view the article, left click the link
immediately below.
(Download the latest
Acrobat Reader if required.)
Method for estimating air-drying times of lumber (2001)
Published information on estimated air-drying times of lumber is of limited usefulness because it is restricted to a specific location or to the time of year the lumber is stacked for drying. At best, these estimates give a wide range of possible times over a broad range of possible locations and stacking dates. In this paper, we describe a method for estimating air-drying times for specific locations by optimizing a drying simulation using existing experimental air-drying times for northern red oak, sugar maple, American beech, yellow-poplar, ponderosa pine, and Douglas-fir. The results of the optimization are simulation parameters that make it possible to estimate the air-drying times of these species regardless of when they are stacked, in any location where average tem- perature and relative humidity are known, and for lumber of any thickness dried to any moisture content.
Author: Simpson, William T.; Hart, C. Arthur
Source: Forest products journal. Vol. 51, no. 11/12 (Nov./Dec. 2001).:p. 56-63 : ill.
Citation: Simpson, William T.; Hart, C. Arthur 2001. Method for estimating air-drying times of lumber Forest products journal. Vol. 51, no. 11/12 (Nov./Dec. 2001).:p. 56-63 : ill..