Question
How do you notch the drawer backs for Blum Tandems? I'm a one man shop, so volume is low. Iím constructing dovetailed boxes, so leaving the back short is not an option. I presently make a couple passes on the tablesaw dado blade after assembly. It works, but itís not the best. Is there a better way?

Forum Responses
(Cabinetmaking Forum)
From contributor J:
Thatís how I do it. I have a saw dedicated to doing just that operation. With a good dado set this works just fine.



From contributor D:
I haven't used it much, and I am sure it can be refined, but the pictured sled works well. It can do overlay and inset backs. The front dadoed piece is replaceable and adjustable for material thickness (prevents chip-out on overlay backs).


Click here for higher quality, full size image



From contributor M:
A jig saw and chisel is short and sweet, unless you're using plywood. I notch mine after assembly. Two quick cuts with jig saw and pop out the piece with a chisel.


From Contributor G:
When cutting dadoes for drawer bottoms just raise the blade and cut through the back panel removing the whole bottom. It makes it faster and easier to assemble drawers and solves the notch problem. I have done this for years and it works great.

From Contributor W
Member

We do the same as GP.


From contributor S:
The quickest way I found to notch the drawer bottoms without any special setup is to use the Fein with a blade size close to 1.25 wide.


From contributor C:
I use the band saw with a clamped on stop to fence. Itís pretty fast.


From contributor R:
I have never notched mine. After I run the grove for the drawer bottoms, I take all the drawer backs and cut off the bottom portion up to the top of the groove. I then assemble, slide in the drawer bottom, staple it in place, and drill the two holes on the back for the tandems.

From Contributor E

Click to View Member Profile Member Contact Info Shop Gallery Categories

That's fine to cut the back off at the grove if it's a doweled or butt jointed drawer, but if it's dovetailed you're going to see the pin without a socket for it to go into. How are you guys building your drawers if you are just cutting the back off at the groove?


From the original questioner:
Maybe I've been over-thinking it. For the low volume I have I'm going to try the jig saw or Fein - makes sense and sounds simple. I'm with Contributor E though - with dovetails it looks goofy to cut off the bottom of the drawer back.

From Contributor F

Click to View Member Profile Shop Gallery Categories

If you cut the notch in the dovetailed drawer after glue up there is no pin missing when notched. Walzcraft makes dovetailed drawers less expensive than I can buy and mill the maple to 5/8. Completely notched, lacquered, assembled, and shipped. I've never been disappointed with them in 20 years.


From Contributor U:
I made a jig that clamps to the side of the drawer boxes. I use an up-cut spiral router bit. Then I tilt the box on its front and I have two holes in the jig that drills the holes in the back of the drawer box with the same router setup.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: General


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2019 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article