Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Paint Finish on Melamine       Will paint adhere to melamine? With scuff sanding, yes, say people who have tried it. July 22, 2005

Question
Is it possible to paint melamine? I have to make some painted cabinets, and I was thinking of using melamine particleboard. Another cabinetmaker said that he uses melamine and paints it. Is this possible? Any input would be appreciated.

Forum Responses
(Cabinetmaking Forum)
From contributor S:
Do you want to paint it because you want the interiors to be melamine?



From the original questioner:
I want to paint the interior a different color. It will be a bookshelf unit. The adjoining cabinets will have doors on them. I want all the cabinets to match in color. I could use wood or MDF, but I want to use melamine if possible.


From contributor J:
Have you tried adhering any material to a melamine surface? It’s not a porous environment for any kind of covering.


From contributor D:
A scuff sanding of a melamine surface creates and excellent and paint able product.


From the original questioner:
I tried a test piece. I sanded the melamine with 220 and it sanded nice, then I applied two coats of acrylic lacquer. It seems to be working fine. I will let it set for a few days and see what happens.


From contributor P:
If you paint the melamine you'll still have an edge to deal with. Many people have had great results painting PB after priming with clawlock.


From the original questioner:
There won’t be an edge to deal with if a face frame is used.


From contributor A:
Why use melamine if you want to paint it? I would suggest using MDF. They offer pre-primed stock, and if you’re looking to save a step check with your supplier, using melamine for a core to paint seems like a lot more work than is needed.


From contributor P:
I use melamine to from time to time, but the best use I have found for it in my little shop is as work surfaces and platens in the vacuum bag. The reason for this is that it cleans really easy as very little adhesives sticks to it. You probably are going to have a problem with the finish pealing off. It may not happen right away, but it will happen soon.


From contributor T:
It works fine for us with some sanding on the surface to be painted. Our supplier also sells a 1-side melamine/1-side paint able panel that's great. It’s great for applying HPL or veneer if desired.


From contributor M:
Given the proper time and money quantity, any of the major board manufacturers (Panolam, Uniboard, Tafisa, etc.) can produce melamine with one color on one face and a different color on the other face.


From contributor S:
To the original questioner: I love to paint over plastic since it is so stable compared to wood with regard to humidity, etc. But it has to be scuffed for the paint to adhere. Have you thought about using solid-color Formica to match your colors and solid color PVC tape to hide your black edges? You could easily have Formica pre-laminated to your board to take care of the interior color.


From the original questioner:
The color is a paint match and there is no laminate to match. I painted a test piece and it seems to adhere well and looks great.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: General

  • KnowledgeBase: Finishing




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article