I am building some drawers for a customer that have 32mm holes in the bottom for pegs that are adjustable for stacking plates in to prevent them from moving. This is a new feature that ladies seem to love for their cabinets. I used my line borer to drill 5mm holes in a grid 32mm apart for the pegs which will be 1" wood dowels with a 5mm steel pin inserted in the dowel. My problem is I don't know where to get 5mm pins for the dowels that are at least 2" long or longer that I can cut to length. Anyone know of a good source?

Forum Responses
(Cabinetmaking Forum)
From contributor B:
This isn't going to work as I understand it. You are drilling a 5mm pattern in your drawer bottom, and my guess is it's 1/2" to 3/4" thick? You are planning to put the pin into the dowel and stick that into the 5mm hole? Save the headache and use a conformat screw through the drawer bottom into the dowel. You can get comformat screws that will go through your 5mm hole into a 4mm pilot hole in the dowel. If you still want a 5mm pin, use a sex bolt sleeve. Recess that into your dowel and you won't have to cut anything.

From contributor J:
Or better yet, just order the stuff that Hafele sells. It's on page 996. It has a threaded stud and a lock nut that goes on the bottom. They also sell the drawer bottoms pre-bored.

From the original questioner:
I have built a couple of these before using 1/4" holes (hand drilled) and dowels, but the thought of drilling hundreds of holes in 6 drawers did not appeal to me. That's why I opted for the 5mm holes with my line borer.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Cabinetmaking

  • KnowledgeBase: Cabinetmaking: Custom Cabinet Construction

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2017 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article