Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Quartersawing for Bows       Whether for archery, a chuck wagon, or a fiddle, bow-making starts with quarter-sawing. October 14, 2006

Question
A neighbor brought me a white oak log and he needed some bows ½” thick by 2-1/2 wide. I cut three cants 2-1/2 by 7 and started cutting his bows. Two out of the three started crowning and one stayed straight. I'm sure there is some technique that explains this. I am new to this and I am trying to learn when quartersawing is necessary and when it is not. Any information is appreciated, as well as links to other sites with a good description and diagram for quartersawing.

Forum Responses
(Sawing and Drying Forum)
From contributor A:
I sawed some bows years ago. I found out later that sawing wasn't the best way. Growth rings are used to rive (split) the wood to make a bow. The idea is to keep as many of the fibers of the wood intact as possible. Some are split, shaved and glued to make laminated bows. Some are carved and rived from a single log. Based on what I've learned, quarter-sawing would go against the making of a good bow.



From contributor B:
What kind of bows? Like the bows in the bed of a wagon that hold up the canvas? Like the bow an archer uses to shoot an arrow? Like a bow a fiddler uses to play a fiddle? Bows for a wagon are best flat sawn from clear wood and steamed bent as soon as possible. Bows for shooting arrows are quartersawn oversized with the grain running straight down the board then the bow split from the blank. Bows for fiddles are taken from quartersawn boards and local boys like the butt cut near the trunk for the best grain.


From the original questioner:
These were bows for a chuck wagon, and we did have good luck bending them that day. The problem I was having was that the cants were moving on me while I was sawing the bows. After I realized the problem I turned them 90 degrees and was able to get a consistent cut down the cant. Where can I get some more info on quartersawing techniques?


From Dr. Gene Wengert, technical advisor, Sawing and Drying Forum:
Search here at WOODWEB using the word QUARTERSAWING.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Sawmilling

  • KnowledgeBase: Woodworking Miscellaneous

  • KnowledgeBase: Woodworking Miscellaneous: Bending Wood




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.