Quartersawn mahogany, or is it?

      An architectural woodworker seeks specifications and industry guidelines for what constitutes truly quartersawn mahogany. March 5, 2000.

Q.
I am having a small argument with my supplier as to whether or not the 3000 BF of Honduran mahogany I just received is truly quartersawn.

Some of it is, and obviously so.

The manager insists that mahogany is not truly "quartered and then sawn." He says that, as the wood comes out of the kiln, workers choose pieces for pattern grade and quartering characteristics. He says this is what you get when you order quartered Honduran mahogany.
This grade was the spec for a federal courtroom in Nashville, and I am feeling my way through this. I am not happy, and my feeling is that most of this wood is crap: wild grain, non-straight, etc. It takes off pretty good and pretty consistently as we saw it.

Any thoughts or responses? We could hire an independent lumber grader to come to check the wood, and if it is indeed correctly graded his services would be at our expense.

A.
Regrading is done under certain rules and if the grade is off by more than 5 percent, you are home free!

The definition of quartersawn varies. Some people, including the U.S. Forest Products Lab, say that a piece is quartersawn when the rings are between 45 to 90 degrees with the face; otherwise it is flatsawn. The common definition in the industry is 75 to 90 degrees is quartered, 45 to 75 is rift. The National Hardwood Lumber Association has a slightly different definition: the ray fleck "must show well."
Gene Wengert, forum moderator



Just my opinion as a (former) lumber inspector for an importer. Sounds to me like what you got is what is commonly sold as "quartered" mahogany - it will include true quartered boards as well as rift sawn ones. Given your need with architectural requirements, you should have placed an order specifying exactly what you required - of course, the cost would have been more as well.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Architectural Millwork: Custom Millwork

  • KnowledgeBase: Primary Processing: Lumber Grading

  • KnowledgeBase: Wood Engineering: Wood Properties

  • KnowledgeBase: Knowledge Base


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2020 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article