Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Quick-drying wood stains       Wood stains which dry fast and foster good grain definition. February 12, 2001

Q.
I am a woodworker and furniture refinisher. What type of wood stain can I use to bring out the rich grain of the wood but still dry quickly enough to seal and finish my project in the same day?

A.
There are several different types of wood stains currently available. The conventional lacquer stains are basically colored lacquers that dry very quickly and could be used for your fast turn-around schedule. A draw back of the lacquer stains, however, is that they do not penetrate into the wood fibers to provide good grain definition and if a finished piece is scratched through the finish, the bare wood will be exposed.

NGR alcohol stains are another type of quick drying finish commonly used on furniture; their liability is poor fade-resistance in direct sunlight. Conventional penetrating oil stains provide good grain definition and richness of color. However, most oil stains take a relatively long time to dry before the subsequent sealer and topcoats may be applied. Otherwise you often get blushing and/or solvent entrapment, bubbles, in the sealer.

A recent formulation is an oil stain that combines the best properties of both lacquer and penetrating oil stains. The new 15 Minute Oil Stains give penetration into the fibers of the wood surface, resulting in excellent grain definition and richness of color. Their working time is more than sufficient to obtain a uniform staining job when applied by wiping or brushing or spraying, followed by a wipe. Their fast release of solvents, however, allows the sanding sealer to be sprayed over the stained surfaces in only 15 minutes. These 15 Minute Oil Stains will allow you to complete your projects within your time constraints while providing you with a finished piece of which you can be proud.

Woodrow "Woody" Sanders is the Technical Information Director at Sampson Coatings, Inc.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Finishing

  • KnowledgeBase: Finishing: General Wood Finishing

  • KnowledgeBase: Finishing: Refinishing

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.