Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Sapwood and heartwood       Questions on sapwood and heartwood of pecan and hickory, and how-to instructions for quartersawing. April 4, 2001

Q.
1) Some types of hickory (maybe pecan) have a very large variation of colors between the sapwood and the heartwood. When milling this wood, does it make sense to separate the sapwood from the heartwood?

2) What is quarter sawing?

3) What do most people do with cherry sapwood?

Forum Responses
With hickory and pecan, the sapwood is white and the heartwood is brownish. This is normal. Sometimes, hickory will have stronger color variations due to improper handling and drying. Pecan color is not as pretty (in many people's eyes) as hickory. There are 4 species of each; they are not usually separated in the lumber market, but all 8 are sold as hickory (legally).

Quartersawn refers to the angle of the rings (when viewed from the end grain) to the face of the lumber. Often flatsawn has the rings at 0 to 45 degrees and quartersawn is 45 to 90. Sometimes quartersawn is called vertical grain.

Sometimes, riftsawn is also used for quartersawn that is 45 to 65 (or so) and then quartersawn is 65 to 90. This definition varies from mill to mill.

Gene Wengert, forum technical advisor



With cherry, do people separate the sapwood from the heartwood and if so, is the sapwood desirable at all?

How would you go about quarter sawing on a band mill?



With cherry, heartwood is more desirable. I believe you can leach some of the color from the heart to the sap with steam.

To quartersaw on a band mill,

1) Level your log so that the pith of the log is level, and cut in half.
2) Turn 90 degrees and split again. You may have to cut the two halves separately.
3) You should now have 4 pie shaped cants. Role three off the mill.
4) Dog the remaining cant flat side down and saw a board from the bottom of it. For instance, if you are sawing 4/4", set the scale at 1".
5) Remove the board from the bottom of the cant, and roll it to the other flat.
6) Cut and roll until you are left with a piece too small to get another board. I sometimes try to square this last part up for a turning blank or table leg.
7) Repeat with the remaining 3 cants.



My method is a little different. Before I cut the log into quarters, I first remove 4 slabs by rotating 90 degrees at each turn, and then rotate 45 degrees to complete the quartering. This gives me a flat surface at the bark edge of each quarter, which will then lay flat against the bed. Next, I remove the tip of the wedge, leaving a small flat of about 3 or 4 inches. This small flat is then turned against the dogs and the clamp fixed against the other (barkside) flat. Sawing proceeds from the top down until the clamp interferes, and the piece is then turned over to repeat the top down procedure.

This method results in several 90 degree (premium) quartered boards in the middle with a range of 'rift' sawn boards on either side.



Most cherry sapwood will be stained to match the heartwood in the finishing process. However, with time, the stained sapwood will not darken to the extent of the heartwood, and the contrast will become apparent. Likewise, if steamed, the cherry may look fairly good initially, but time will highlight the difference. (This is not true with walnut, possibly because the heartwood does not darken much with time.)

I cannot recall a commercial operation that separated cherry sap from heart or took special care to eliminate sapwood. It is normally not a defect to have sapwood, except that export markets will require its removal, which also means more waste and higher prices for the remaining lumber.

Gene Wengert, forum technical advisor



What does 4/4 and 8/4 mean?


Regarding sapwood, as long as it is solid wood, it is not considered a defect. When building anything from cherry or walnut, I rip off the sapwood and get to a good solid heartwood edge. The sapwood does not darken over time and I do not stain my woods, so the sapwood sticks out in the final design like whipped cream on a chocolate sundae.

I have steamed walnut boards packed right tight to each other for about a week and it softens the transition a bit, but I don't like the loss of color in the heartwood as a result of steaming, albeit a more even chocolate brown color.

4/4 = 1" thick
8/4 = 2" thick

The dimensions vary from sawyer to sawyer. I ask mine to cut at 1-1/4" on specialty woods, and I usually get a rough milled board around 1-1/8 or so and after drying, I can plane out almost always right at 1". My customers like the added thickness, and it gives me a fudge factor, should the board cup, warp or twist a bit more than I expected.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Buying

  • KnowledgeBase: Primary Processing: General

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Sawmilling

  • KnowledgeBase: Knowledge Base




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article