Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Sawing and Drying Sycamore       Sycamore is attractive and useful, but moves drastically while drying. Here's good advice on how to minimize movement and make the most of each board. June 27, 2006

Question
I am sawing some sycamore for a customer and he's wondering what to use it for. Can anyone tell us the best uses for this wood and any particulars for sawing and drying - also how hard does it become and is it stable?

Forum Responses
(Sawing and Drying Forum)
From contributor A:
Quartersawn it is beautiful but not always easy to get good ray fleck. It was historically used for drawer carcasses because it is very stable but with its interlocked grain it makes a nice accent wood for projects.



From contributor B:
We use thousands of BF of Sycamore for gunstocks.


From contributor C:
Quarter saw for sure. I may be wrong disagreeing with contributor A, but I thought that even quartersawn sycamore was not particularly stable; same as flat sawn maple. Flat sawn sycamore is notoriously unstable and I have a potato chip shaped box lid to prove it. This probably does not matter for smaller items like gunstocks.


From contributor B:
We have found the Sycamore to be extremely unstable during drying (it goes nuts), so we have to weight it down. After it has dried it seems quite stable but we keep it in a constantly controlled area. We have never had the sycamore show any signs of instability after it was dried to 6% MC and made into a gunstock and finished.


From the original questioner:
To contributor B: What dimensions do you saw your gunstock material? I also heard it is unstable but it seems stable after drying. I wonder if that goes for flat sawn also.


From contributor B:
We quarter saw 2-3/4" thick; after drying and planing it will be 2-1/2" thick.


From contributor D:
I cut 800 bf or so of sycamore about a year ago. I tried to quartersaw as much as possible because it resembles European plaintree, and Australian lacewood. I immediately stacked and stickered the wood (not knowing how unstable it was while green) and put a lot of weight on top of it. I left some of the slab wood laying around for bowl blanks and it all warped, cupped, and twisted to an extreme. It was like putting a 15" wide oak board in the sun and coming back in a couple of months.


From the original questioner:
To contributor D: How did the wood you weighted dry and how did you weight it?


From contributor E:
To contributor B: Might we get some information or pictures on the gun stocks? I would be interested in a Hawken stock - something different.


From contributor F:
Quartersawn is best but when I saw sickymore I always saw it 2-1/2 times thick. When dry, I split in half and plane down. It seems to have less waste this way and gives me a flat side to start planing on.




From contributor F:
I still think spalted is best and even if you let the logs lay a bit, they saw easier and stay flatter.




From the original questioner:
To contributor F: You are saying if I want 4/4 I should saw 10/4, let it dry and saw in half and plane to 4/4?


From contributor B:
Here is a picture of a Sycamore gunstock.




From contributor D:
I weighted the top of the stickered pile with concrete blocks and whatever was heavy and laying around at the time - something like 100 pounds or so, evenly distributed across the top. The pile was approximately 12" wide by 8' long and 5' tall (other piles of wood were on the sides of this one so the tall piles weren’t tipsy).

Sawing the boards extra thick and then resawing when dry will work great, but is it worth your time? If you sticker the pile right, your final yield of lumber will be fine. If you do saw thick and then resaw you will be releasing tension in the wood and the resawn boards will warp, twist and cup a bit, depending on how the tree grew.



From contributor F:
Is it worth your time? That depends on what you are getting for the lumber and how much you have to waste. Then there is the size issue and what sells the best. Since I sell the sickymore stock from 1/4 thick to over 4 inches thick there are lots of sizes to store and stack. Taking a 2-1/2 inch thick board back to the mill to split takes little more time than it would have taken to saw it the first time it was on the mill, not to mention the time saved at the planer. They dry flatter thicker and I can shave off two or three thinner boards if needed and you could never dry a sickymore board thinner than 3/4" flat. How much time is saved by stickering half the number of boards? How much time is saved not having to pile weight on top and then removing it to get a board out? How much time trying to tell someone you do not have ¼” thick scroll saw stock? I would guess it is each man’s call.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Sawmilling

  • KnowledgeBase: Primary Processing: Air Drying Lumber




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article