Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Sleigh Bed Construction Issues       Sleigh beds are traditionally made with veneers, but in this case a customer is asking for "solid wood." This brings up a discussion about wood movement and construction methods. November 26, 2006

Question
A client has asked me to build a sleigh bed in solid mahogany, and he insists on solids throughout. The headboard and footboard will be some 60" wide by 40" high, grain running vertically, and curved. I am scratching my head on this one. How can I fabricate this curve, make it pretty consistent, and minimize hand tooling?

Forum Responses
(Furniture Making Forum)
From contributor T:
Think about a stave core door, only this core will have a curve to it. Draw side profile full scale showing the sleigh, use drawing as pattern and make flush trimming jig, rough out on bandsaw the profile/curve into core blocks, then flush trim, glue up into panel and veneer.



From contributor L:
I'd be concerned that sawn to shape would leave too many short grained sections. If I tried that job, my starting guess would be to resaw the stock and vacuum-press laminate it on a form. I'm not sure that I could stack and place 60" sheets, so I'd consider narrower panels joined after lamination. But that's a lot of additional material and time, and it is not clearly consistent with the demand for solid wood.


From contributor B:
A 60" wide solid wood panel is probably going to move close to an inch in width seasonally in a place like the Northeast. I am sure there has to be something to hold the mattress in place, which has to attach to the head/footboards, which may constrain this movement. I predict a self-destruct cycle of less than two years. Also, solid wood, when sawn into thin strips/sheets and glued back together, is not much different then annular rings on a tree held together with lignin.


From contributor H:
I too gave thought to wood movement when I read this post. However, he did say it was to be made of mahogany, which is one of the most stable woods. If he uses vertical grain mahogany, that would be even better. This is, of course, assuming it is SA mahogany rather than a substitute.

60" is substantial width, though, and I'm not sure just what movement he'll see with the mahogany over that distance. Also, given that it is to be curved, any wood movement could cause strange effects along that 60" width. Customers always want things that cannot be reasonably done with wood! Perhaps it's time for a wood movement lesson with the customer.



From contributor W:
I realize that vertical grain is nice and wood movement is the problem. For the solids, how about using 60" long strips glued up on a form to make the curved shape, ala coopering? Or brick lay up 20" and 30" pieces. Make sure you are using reasonably color-matched lumber. Are you going to stain the final piece? Talk with the customer about the problems.


From contributor D:
I'll go in a slightly different direction and mention that it is far better to have the customer put their faith in your ability to make the best product the best way. The worst experiences I have had is when a customer has told me how to do what it is I do. Today, I tell them I know what we are doing, and the best thing is to let us simply do it. The reference to solid wood is probably the result of a perception of veneer being cheap along with substrates somehow being cheating. Both views are easily supported by observation in today's big world of bad furniture.

Do a bit of research on sleigh beds (as you are here by posting), determine the best way to build the best bed, and confidently propose to your customer what you want to do and why.

More specifically, stack laminating wide bandsawn 12/4 boards, 40" long, of pattern grade Honduras to get to 60" wide will simply not yield a very attractive surface, considering all the material and labor. One reason sleigh beds were/are made is to show the maker's skill in laying fancy veneers on curved surfaces. To do otherwise would be to miss the point of the design.



From the original questioner:
When my customer first approached me with the request for "all solids," I started into my usual sermon about why veneer is good and the misconceptions that give it a bad rep. His argument was that he wanted to feel confident that he could work on it down the road, refinish it or whatever, and he was afraid of veneer. I had almost cooked up a method of bent laminations in a vac press, in, say, 10" widths, and then joining those. Reading these responses has me thinking, though. Maybe I can get him to agree to veneered panels if I can order heavier thickness veneers. I think Certainly Wood sells special thickness veneers. Thanks.


From contributor P:
I think that there is a way to do it using the bent laminations and vacuum press. We do this with chair slats all the time. We normally glue up a 6" wide x 24" long curved panel and then cut it into slats, but on some of the designs, we glue two of these panels together edge to edge to make a wider back splat. Works fine. We generally use (4) 1/8" laminations per slat. So you could make a whole bunch of these, bend them to the desired profile, and simply glue them edge to edge to make the 60" panel. The difficulty would be in putting any kind of top rail over this panel, but since the panel is curved, it would be quite strong. It could be glued directly to the side rails. 1" of movement in a bed is no big deal, as long as the slats and slat supports were sized to accommodate it. Mattresses are squishy and don't need to fit very precisely in a bed frame. It would also end up being a weird looking bed, very stripy - but it would certainly be all solid.


From contributor K:
If the customer is dead set on solid wood, then design around the material. How about curved solid slats, either sawn or laminated depending on the degree of curvature, separated by spaces or joined to make a closed panel with unglued splines? I believe Chris Becksvoort wrote an article in Fine Woodworking using this approach a few years ago.


From contributor L:
I'd have to agree with contributor B. You could resaw 1/8" thick solid wood to whatever height your bandsaw will cut and individually laminate them to your curved core. You could refinish it 10 times over the next 200 years and still have plenty of wood left. Or refer to Christian Becksvoort's sleigh bed in Fine Woodworking #124, June 1997.


From the original questioner:
Thanks for the suggestions. I looked up the FW article by Becksvoort and it looks interesting. One big difference that I notice, though - Becksvoort's bed has horizontal grain in the head/foot board. The one my client wants has vertical grain. I'll have to study that article further.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Furniture

  • KnowledgeBase: Furniture: Custom Furniture




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article