Today's
Sponsors:


Finish Systems

Firth Maple Products

FORDAQ

FormWood Industries

Freeborn Tool Company

Fuhr International

Fuji Spray

Gabbiani Machine

Gary M. Katz

Global Hardwood Flooring

Glue Machinery Corporation

Goby Walnut Products

Graco, Inc.

Granite Road

Grayson Ferguson Woodworking Inc.

Great Lakes Kiln Drying Association

GreCon

GUHDO

Hanson and Leja Lumber Company

Hardwood Council

Hardwood Store of N.C. Inc.

Heartwoods, LLC

Her-Saf

Hermance Machine Company

High Point Grinding - Total Saw Solutions

Historical Plus Wood

CNCROUTERSTORE.com

CNT Motion Systems

Colonial Saw

Construction Programs and Results

Cook's Saw Mfg.

COOLwoodworkingstuff.com

Country Saw & Knife, Inc.

Courmatt International Inc.

CP Adhesives

CSH Custom Service Hardware Inc.

CTS Manufacturing Inc.

CustomMade.com

Cutlist Plus

D.S. Brown Machinery

Dancer Lumber

Delle Vedove USA, Inc.

Delmac Machinery Group

Delta

Denray Machine

DeVilbiss

Dispoz-A-Blade

Diversi-Tech

DMC

DODDS

Don Hall & Associates

Donald Dean and Sons

Durable Wood Products

E.W. Tooling Inc.

Eagle Machinery and Repair Co.

ECabinet Systems

Edge-It Edgebanding

Edwards Wood Products

Electrophysics

Elias Woodwork & Manufacturing

Elkom North America

Emerald Hardwood Floors

Endeavor Hardwoods

EnRoute WOOD

ETemplate Digital Measuring

ETK International

EX-FACTORY

Excel Dowel and Wood Products Inc.

Extrema Machinery

ez-Router

FastCap




Splicing Pre-Finished Crown Molding       Tips for getting a tight joint on pre-finished crown molding splices.

Question
Since factory finished crown seems to only come in 8' lengths, a lot of splicing must be done. I have always tried to match up shade and grain patterns, and even cut the long compound cuts to follow grain, if possible. As time passes, though, I've seen these glued and nailed splices open up or overlap many times. Some suggest butting splices with some spring in the fit so they can't open up, and it looks no worse. What are you doing to splice? If you insist on compound cuts, is there some standard as far as the angles used? Hope someone out there can help me with this messy deal. If you use only full length sections custom made on your moulders, sit on your hands… that is not a luxury we all have.

Forum Responses
(Cabinet and Millwork Installation Forum)
Add a biscuit and plenty of glue and you will be hard pressed to see the joint open up.



I agree. Biscuits or dowels are a great way to make that butt joint. You need that snap fit for the pressure to clamp the joint. We have been suggesting that type of joint when using the Copemaster. It allows you to pressure fit your coped joints. It is easier on paint grade but if you can line it up on the pre-finished, it will never open. Hot water, a toothbrush and compressed air makes the glue cleanup quick.


A quick note on clamping... Two small screws into the back of the molding can be rubber banded across to provide clamping pressure while the glue dries. Just make sure to locate the screws in the thicker part of the molding. Remove prior to installing.


We've been pre-assembling all our field splices for years. I've never found a better method, especially for long runs down hotel and condo corridors, and for stain-grade stuff, like alder, that only comes in 10 ft. lengths, or even for mahogany on walls over 16 ft.

Before hot-glue, we assembled the joints from the back of the molding, but now we hot glue a piece of 3/8 or 1/4" plywood (about 2 ft. long and ripped just narrower than the back of the crown) to the back of the inside corner cut (we make all our splices compound miters so there's more glue joint and the angled cut hides better than a vertical joint). Then turn the molding right-side up, spread Titebond on the miter joint, hot glue the plywood, and press the other piece of molding into the hot glue on the plywood backing and line up the miter at the same time. I like to do this with the material on my miter saw, so I can hold the splice against the fence and keep both pieces in a straight line. If you're still worried about the backing, you can shoot some 5/8" staples through the plywood into the crown, then let the spliced-length sit for a little while before cutting it to length. We usually grain-match the material for splices before doing anything else, make up all the splices, then start cutting. By then, the first pieces are pretty dry.




I use a butt joint and assemble with pocket hole screws from the back. Faster and more durable than any method described here (in my opinion).


I've never been able to position the two pieces perfectly so the joint is perfectly flush once the screws go in. My clamps just don't hold well on the profiles. And besides, a lot of the crown I install isn't thick enough for pocket screws, especially the MDF stuff. And butt joints... they sure show up more than compound-miter splices. I know that polyurethane molding manufacturers recommend butt joints, but I think I'll stick to my method for wood moldings.


We are all talking about pre-finished crown, right? I take into consideration where the joint would best be placed and which direction the 45 should angle. I cut my crown upside down against the fence and cut both pieces at 45's. I try and color/grain match as best I can and put one piece up. I then cut the other piece a little long and dry fit it and make any adjustments if needed. I then glue the snot out of it and put it up, having a damp rag handy to wipe off the excess glue. Surface nail if necessary, micro pin if painted. Use touch-up pencil as necessary (I have a broad selection), but try and get as close as possible so as not to have to use it. Another thing I sometimes do is use a matching magic marker touchup pen to color edges before I put them together. Sometimes that helps a little. Don't know if it's the best way, but that's how I've been doing it for a long time and I can't remember ever having a joint open up.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Architectural Millwork

  • KnowledgeBase: Architectural Millwork: Moldings




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    RR4 Box 265A
    Montrose, PA 18801

    Contact WOODWEB













  •   Home » Knowledge Base » Knowledge Base Article