Spraying CV Over Pre-cat Lacquer

12/09/2014


From original questioner:

Can CV be sprayed over pre-cat lacquer?

If not, what steps need to be taken to prepare for cv. I have a piece I built some time ago that is showing wear and need a more durable finish on it.

From contributor Ke


Nope. Strip it to bare wood and then spray with CV. otherwise, just clean, scuff, clean and respray with Lacquer.

From contributor Le


General rule is never spray a harder finish over a softer one.

From contributor Bi


Thanks guys!