Today's
Sponsors:


Royce Ayr Cutting Tools

RT Machine Co.

Safety Speed Cut

Sand-Rite Manufacturing

Sandman Products

Sawmill and Woodlot Magazine

Schultz Forming Products

SCM Group USA, Inc.

SCM Group

SCM

Sears Trostel Lumber Co.

Shade Dri

Shomaker Lumber Company

ShopBot

SII Dry Kilns

Silvaris

Simantech

Single Source Cabinet Supplies

SIS Machinery

SK-USA

SketchList

SlipCon USA, Inc.

SnapDragon Associates, LLC

SNX Technologies

South State Machinery

Southeast Tool, Inc.

Sovereign Machine, Inc.

North Pacific Lumber

Northstate Hardwoods

Northtech Machinery

NPO BARS

O'Shea Lumber Company

Old Mississippi Brick and Heart Pine Company

Omnitech Systems

Onsrud Cutter

Open the Door Products

Opti-Sand

Optisol for Project Scheduling

Original Saw Company

Osborne Wood Products

Paragon Enterprises

Patton Cabinet Doors

Peninsula Hardwoods

Penn Sylvan International

People Logic Software Corp.

Pinske Edge

Pioneer Lumber Company

Pioneer Millworks

Plogic Solutions Ltd.

Pond Cove Paint

Porter-Cable

Precision Drive Systems

Premium Specialty Hardwoods

Prime Estimating and Software Services, LLC

Primo Woodworking Machinery

Pro.Woodworker.com

Pro100

Professional Hardware & Supply Co.

Professional Machinery Group

PYTHA

Quality VAKuum Products, Inc.

Quick Machinery Company

Quickscrews International Corporation

QuickScribe

QuikDrawers

R&R Drummond, Inc.

R.A.W.

R.D. Billhofer Company

Rangate

Rawles-Aden Lumber Corp.

RazorGage

Rex Lumber Company

Riethmiller Lumber

Ritter Manufacturing Inc.

Rockler Woodworking and Hardware

Roger Shaw and Associates

Rose Machinery

Routech

RouterCAD




Steaming Walnut       If you do it properly, steaming walnut brings color to the sapwood without destroying the figure in the heartwood. May 11, 2005

Question
Is there any detailed literature on steaming walnut, including chamber construction, boiler sizes or perhaps another way of generating steam, and step by step instructions? I'm looking to steam 2000 to 3000 bf of 4/4 at a time.

Forum Responses
(Sawing and Drying Forum)
From contributor K:
Why would you want to ruin wood like that? The steamed walnut that I see in some of the large commercial kiln outfits around here looks like garbage. A milk chocolate brown that has no discernable character. Most of my customers, including some high end manufacturers of specialty products, specifically request me not to steam my walnut.



From the original questioner:
I agree with you, but this is for one of my biggest customers, who uses it for low end high production promotional pieces where quality takes a back seat to quantity. He in fact is requesting I look into it to boost his production and minimize his losses in sapwood.


From Gene Wengert, forum technical advisor:
If properly steamed, walnut will have beautiful color. The problem is that some people do not steam properly and get the wood too hot or too cold. There are many steamers that do a beautiful job. For more details, see US Dept of Agric Handbook No. 528, "Drying Eastern Hardwood Lumber." It was published in 1976 and is now out of print. This should be available through all libraries - interlibrary loan if they do not have it themselves. If you are a member of the NHLA, contact Dusty Moller there and he can probably make a copy of the steamer pages or may even have some extra copies.


From contributor D:
When you do steam, I suggest that you put an RTD or two in the wood and then heat only as hot and as long as needed to change the color of the sapwood. I think you'll find that you do not need to get the wood as hot as many people believe and the color of the heart wood won't be changed.


From the original questioner:
Please forgive my ignorance. What is a RTD?


From contributor D:
They are solid state devices (resistance) for remote temperature sensing. They are accurate, rugged, fairly cheap (about $60) and can be read by a variety of instruments.Also, they need no special wire for extensions and can be extended 1000's of feet and still give an accurate measurement (if they are 3-wire).


From Gene Wengert, forum technical advisor:
RTD = resistance temperature device. Often the device is in the shape of a round wooden pencil with a small piece of platinum wire at the tip (but inside so you cannot see it or damage it easily). The resistance of the platinum wire changes with temperature in a predictable manner, so if you know the resistance, you know the temperature. We use three wires, so that the resistance change in the wires (for whatever reason) can be accounted for and not incorrectly influence the reading of the platinum wire resistance.

Incidentally, the steaming chamber must be at 100% RH. The wood must get to about 180 F for best color development and this means that the temperature in the steamer must be around 210 F. Cooler temperatures work, but they take longer and do not get as good color (although even 180 is pretty good with a wood temperature of 160 or so).

Note that you may have run-off from the steamer and this run-off is a pollutant in every state, by federal law. The fact that some states do not enforce the law still does not make polluting with the run-off okay. The run-off is an herbicide.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Primary Processing: Kiln Operation




    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2009 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.