Question
What is the definition of sterile lumber? What are the common methods? How long does it last?

Forum Responses
There will be some variation, but it is lumber that has been heated for some length of time (several hours or longer) to 130 degrees F or higher. The wood is sterilized until it cools back down, at which point it can be reinfected if conditions are OK.

Gene Wengert, forum technical advisor



You may have heard about the new rules for softwood lumber in crates and pallets going to Europe. All softwood lumber used in crates and pallets must be marked with a stamp certifying that the center of the boards has reached 56C and been held at that temperature for at least 30 minutes. The USDA has published charts for various wood and temperatures that show how long it takes to reach 56C in the center. Inspectors will spot check your operation and they will look at procedures and you will be allowed to continue to stamp. Hardwoods are not involved yet but it appears they will be according to conventions being adopted by the United Nations. The crate wood can be sterilized by fumigation but it appears that the rules may be changed to just temperature.


Today I received a copy of heat treating standards in Australia. This process some believe could become the standard in Europe also - a minimum 74C (165F) at four hours for every inch of thickness. This temperature at the core will kill all stages of insect life. Would it really take that long? Would this also affect finish dimension? What about strength? They do not classify the wood as hard or soft, but "any timber" that is used in distribution - pallets, crates, etc.



Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?


Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Lumber and Plywood

  • KnowledgeBase: Lumber & Plywood: Storage

  • KnowledgeBase: Primary Processing: General

  • KnowledgeBase: Primary Processing

  • KnowledgeBase: Knowledge Base


    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.



    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2019 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB











  • WOODWEB - the leading resource for professional woodworkers


      Home » Knowledge Base » Knowledge Base Article