Tricky Cutting-Board Glue-Up

      A clever cutting board provides lessons about gluing end grain. October 20, 2005

How would you approach gluing up this item? It appears that they glued the end grain together. Will that hold up for a cutting board abuse, or is there a trick to how they mate these together?

Click here for full size image

Forum Responses
(Finishing Forum)
From contributor A:
I'd build the three sections then join them together with loose tenons. If you don't have a way of making accurate mortises, then you could use two rows of biscuits or two blind splines. I wouldn't count on gluing the end-grains together.

From contributor B:
The board is glued up into one section, cross cut twice, a segment is flipped, then reassembled. Use what you like for the parallel grain laminations, then use top grade epoxy for the end grain. Add blind splines if you like. I have a lot of test pieces that are merely end grain to end grain, sitting out in the rain trough, growing algae and rotting, with the glue joint still intact. Experiment first with the epoxy end to end, realizing that it likes to soak into end grain.

From the original questioner:
After looking at the picture for awhile I realized that it was cut after being glued up, but I had already posted the question. But I was still concerned about end grain issue. Thanks for glue advice, I'll give it a shot and see how it comes out.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Knowledge Base

  • KnowledgeBase: Adhesives, Gluing and Laminating

  • KnowledgeBase: Adhesives, Gluing and Laminating: Glues and Bonding Agents

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article