I would like to know if water-based polyurethane is as hard a finish as oil-based poly. If so, which brands are recommended?

Forum Responses
I have heard mixed info on this, but I have recently switched to water-based poly almost exclusively. It seems the same to me, although I don't make bartops. I really like that it dries to the touch in under 10 minutes.

I have all brands and, using a brush, they all seem very close(including the el-cheapos). Hydrocote has one that "ambers" a little, like oil-based.

I usually tint the first coat of water-based poly with Trans-Tint amber liquid dye to give it some color.

There is ABSOLUTELY no comparison. I am a professional woodworker and have tried just about every waterborne out there. They are definetly not as strong as oil based, however, in low-wear areas and areas away from cleaners or liquor (bartops), they are acceptable. Also, on light or white stains, waterborne does not yellow.

If you are going to use a waterborne I recommend Varathane; it is a floor finish which does not become cloudy and seems to hold up pretty well to abrasion, but not chemicals or liquor -- like all waterbornes.

This is one topic on which I have to say something. I've had to use waterbornes since the early eighties on the West coast, before moving to the Midwest. I have used and still use a two-component waterborne that uses an aliphatic poly-isocyanate catalyst, and trust me -- this product offers durability which is very close to the two-component, solvent-based systems. In fact, it has shown better lightfastness and abrasion resistance.

There are waterbornes which are just as good as their solvent-based counterparts; what's missing is the acceptance of the users of these products, who must adjust their systems and techniques when switching to water-based products.

By the way, these high-durability, water-based polys are not products you can buy at the hardware store. At least, not yet.
Bob Niemeyer, technical advisor

Here's the problem: Most off-the-shelf, hardware-store waterborne poly is a mixture of polyurethane and acrylic resins. The acrylic resins are cheaper and handle better -- that is why they are added -- but they are less durable. However, there are some straight waterborne polys available.

Like all tools and materials, some brands are better than others. I can tell you that I have seen and have run some tests on a variety of coatings, and there are definitely waterborne polys on the market that equal the performace of their oil-based cousins. There are also some that clearly fall below the typical oil-based poly.

Another respondent made mention of cross-linked waterbornes. These typically perform on par with their equivalents, i.e., acid cats and conversion varnishes. Again, there are quality differences between brands, and some are outstanding.

For whatever reason (and there are many) the quality and endurance range of waterborne poly coatings is currently wider than that of the oil-based ones.

Incidentally, the waterborne revolution in the U.S. was led by the flooring industry, and some of the best products still come out of that sector.

The comments below were added after this Forum discussion was archived as a Knowledge Base article (add your comment).

Comment from contributor C:
As the previous writer points out, the waterborne polyurethane revolution was pioneered by the wood flooring industry. I would also note that the top of the line waterborne wood floor finishes cannot be bought in a retail store and I doubt they will ever be available in that location. Therefore, I would be very hesitant to use anything that came out of a box store. Waterborne finishes are much more expensive and have a high learning curve. Invariably, the complaints ususally are a result of poor application or working with waterborne finishes in the wrong parameters.

Since I live in Georgia, I am not under any pressure to use the more expensive waterborne products. However, I use nothing but waterborne products because of the exceptional durability, phenomenal drying and curing times and because they make for a much safer and healthier work environment. I feel very confident that in years to come, the question most contractors will be asking is why it took them so long to put these products in their product line. They are worth every dime you pay for them.

Comment from contributor J:
The comment about Varathane above is true. However, there are new technologies on the market that are using new cross linking resins that flow out and give you an equal hardness to oil based poly's. I recommend Deft's Waterborne clear wood finish. After using their brushing lacquer for years I found this to be a great alternative. I also like that I can spray it without thinning.

Would you like to add information to this article?
Interested in writing or submitting an article?
Have a question about this article?

Have you reviewed the related Knowledge Base areas below?
  • KnowledgeBase: Finishing: General Wood Finishing

  • KnowledgeBase: Knowledge Base

    Would you like to add information to this article? ... Click Here

    If you have a question regarding a Knowledge Base article, your best chance at uncovering an answer is to search the entire Knowledge Base for related articles or to post your question at the appropriate WOODWEB Forum. Before posting your message, be sure to
    review our Forum Guidelines.

    Questions entered in the Knowledge Base Article comment form will not generate responses! A list of WOODWEB Forums can be found at WOODWEB's Site Map.

    When you post your question at the Forum, be sure to include references to the Knowledge Base article that inspired your question. The more information you provide with your question, the better your chances are of receiving responses.

    Return to beginning of article.

    Refer a Friend || Read This Important Information || Site Map || Privacy Policy || Site User Agreement

    Letters, questions or comments? E-Mail us and let us know what you think. Be sure to review our Frequently Asked Questions page.

    Contact us to discuss advertising or to report problems with this site.

    To report a problem, send an e-mail to our Webmaster

    Copyright © 1996-2016 - WOODWEB ® Inc.
    All rights reserved. No part of this publication may be reproduced in any manner without permission of the Editor.
    Review WOODWEB's Copyright Policy.

    The editors, writers, and staff at WOODWEB try to promote safe practices. What is safe for one woodworker under certain conditions may not be safe for others in different circumstances. Readers should undertake the use of materials and methods discussed at WOODWEB after considerate evaluation, and at their own risk.

    WOODWEB, Inc.
    335 Bedell Road
    Montrose, PA 18801

    Contact WOODWEB

  • WOODWEB - the leading resource for professional woodworkers

      Home » Knowledge Base » Knowledge Base Article