In this issue:
Featured Project
This writing arm Windsor chair goes from
raw material (rounds of wood) to
finished product in a very nice step-by-step...
http://www.woodweb.com/galleries/project/posts/4271.html

|
This issue of the WOODWEB Update is
sponsored in part by
C.R. Onsrud, Inc.:
Manufacturer of CNC routers, inverted routers, and routing accessories
Web highlights:
- Video Demos Online
- Machine Specifications
- 24 Hour Parts and Service
- User Testimonials
www.cronsrud.com
|
Hot Threads
With a short list of pros for waterbased
poly, this finisher hopes to
outweigh the one big con he's experiencing: blushing. Can you offer advice
on eliminating this defect?
http://www.woodweb.com/cgi-bin/forums/finishing.pl?read=751177
Scribing a skirt board to a set of installed
treads and risers... without a
tape measure... Think it can't be done? Think again, my friend! The
excellent photos and instructions in this thread will make you a believer.
http://www.woodweb.com/cgi-bin/forums/aw.pl?read=751455

The beginning stages of a built-from-scratch
bandmill are documented in
this video series.
http://www.woodweb.com/cgi-bin/forums/sawdry.pl?read=750628
Any suggestions on a graceful start to this
stairway? The newel and
balusters are in the design stage...
http://www.woodweb.com/cgi-bin/forums/aw.pl?read=751650

Recent Additions to
the Woodworkers Directory
The following companies recently created
free web pages at the
Woodworkers Directory. Create yours at:
http://www.woodindustry.com/woodworkers/index.html
kd3 decorative arts ltd.
http://www.woodindustry.com/woodworkers/Master/10508.html
Premier EuroCase
http://www.woodindustry.com/woodworkers/Master/10509.html
Michael Greco, Cabinetmaker
http://www.woodindustry.com/woodworkers/Master/10510.html
Web Marketing 101
Is search engine optimization dead? Well,
I think it's getting there. Look
specifically at the 2010 - 2013 comparisons in this article to see how
SEO has changed. Bottom line - build the best site for your customers.
Period. Shared by Jim Roberts of Roberts WebForge.
Be the Result
that Google Wants to Rank
Knowledge Base Highlights
See a complete list of the most recent additions
to our Knowledge Base at:
http://woodweb.com/Resources/RSMostRecentKBArticles.html
Three months after the job, doors finished
with waterborne conversion
varnish are blushing. The culprit turns out to be ammonia in a household
cleaner.
http://www.woodweb.com/knowledge_base/Troubleshooting_Blushing_on_Cabinet_Doors_in_Use.html
This conversation amounts to a nice overview
of the decisions and
experiences involved in transitioning a shop to CNC production.
http://www.woodweb.com/knowledge_base/Introduction_to_CNC.html

Here's a long thread full of advice for spraying
the insides of drawers.
http://www.woodweb.com/knowledge_base/Troubleshooting_a_Rough_Finish_Inside.html
Exterior doors exposed to weather take a
beating. Here's an interesting
discussion of how to detail wood door panels in a replacement and repair
situation.
http://www.woodweb.com/knowledge_base/Weather_Detailing_for_Replacement_Exterior_Door_Pa.html
This thread answers the question of why
holly and teak are paired in
boat decking (below decks only), and continues with a folkloric and historic
discussion of teak for boatbuilding — including on nuclear submarines.
http://www.woodweb.com/knowledge_base/Holly_and_Teak_for_Boat_Decking.html
Cabinetmakers ponder the pitfalls that may
lurk in a proposal to glue 1/8"
steel to MDF for cabinet doors.
http://www.woodweb.com/knowledge_base/Gluing_Steel_to_MDF.html
Video Pick
Italpresse features a variety of videos on
press systems. To view the
videos, click on the link below and scroll down to Italpresse's video
link:
http://www.woodweb.com/VideoLibrary/VLAlpha.html
To UN-subscribe, change your address, or
contact WOODWEB, follow the
instructions at the end of this message. Replies to this Update mailing
will
not reach WOODWEB.
Find out how to promote your company on
the Web. If you're a supplier to
the wood industry, visit WOODWEB's Media Kit:
http://www.woodweb.com/MediaKit/MKindex.html
If you're a woodworking professional, visit
the Woodworker's Directory:
http://www.woodindustry.com
View past WOODWEB Updates at:
http://www.woodweb.com/update_archive
The WOODWEB Update is Copyright (c) WOODWEB,
Inc. 2013
http://www.woodweb.com
|