Thick Finish -- 1 -- 
5/3

I have a table a widow wants me to re finish for her. The table is a knotty pine that was made by her late husband.
Any finish I can do, but what she wants because I have never done one.
She wants like you see at bars and fancy restaurants. Where it is a HIGH gloss finish, that seems to look really Thick.
What is used to create a finish like this?
5/3 #2: Thick Finish ...

Those finishes are a PITA to use. They are a pour on finish which gets applied just as it sounds. Since they go on so thick they take a long time to dry…..a long time where you have to try your best to keep a dust free environment. Forget who makes them as I avoid them like the plague, but if you search for "pour on bar finish", you'll find it.
good luck,
JeffD
5/3 #3: Thick Finish ...

Its a 2 parts epoxy
You can flood the surface to make it thick,very thick!
I did a project like that long ago with beer bottle caps in the table
Turn out pretty good
But you do need to watch for dust/dirt and flying insects!
This stuff dries slow
5/3 #4: Thick Finish ...

I also like to add that it is pricey
"System three mirrorcoat" is a popular brand
5/4 #5: Thick Finish ...

I built some of those types of restaurant tables back in the day and we used polyester resin. Just like they use for surfboards (which I also made). You could also go with the epoxy though it is nasty stuff and not as easy to work with. One trick is to "stabilize" the wood with the epoxy(west system makes a nice product) and then top coat w/polyester resin. You need to use 2 types of polyester resin. Laminating for the build coats then add surfacing agent to the laminating resin so you can sand it and finally a gloss resin coat which is really hard. And to get that really nice glossy finish you have rub them out. Lot's a work make sure you get paid.
my2cts
5/4 #6: Thick Finish ...

Forgot to add the one thing nice about the polyester is it does dry faster than the epoxy. Though you have to be careful with catalization or you can get it too "hot" with a thick coat and it'll crack and discolor.
good luck
5/4 #7: Thick Finish ...

I did this on a 40' long bar in a winery tasting room back in the late 80's, I used a product called 'Enviro-lite' (most likely a polyester resin), worked great...1/2" deep pour,4-5 hours for a good set...I remember pulling hundreds of fruit flies out with a tweezers for for first couple of hours until it set.
5/5 #8: Thick Finish ...

Website: profinisher.blogspot.com/
I would just spray a polyester sealer like Ilva's TG1323 and then topcoat with a 2k urethane. Much more control of the edges this way, I spray conference tables this way all the time.
High Gloss Conference Table
5/6 #9: Thick Finish ...

Thank you Rick!!
just jim
1 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|