I just finished and installed a set of cherry cabinets. I used a dye stain than stained with regular stain I have a couple of cabinets that came out a little lighter.I can darken them by rubbing a little stain over them I am talking about the frames not the doors they are OK. My question is is there anything in a aerosol that i can spray over my pre-cat lacquer or is my only choice to brush my pre-cat on over my stain. I can't use my spray gun in the house. Thanks

11/17/15       #2: adjusting cabinet color ...
jonmcay Member

Mohawk has spray aerosols that I always used to get the color I want. The problem is this is best done at the shop. There is a smell factor with using aerosols in the house.

11/17/15       #3: adjusting cabinet color ...
Mastercabman

+1 on the Mohawk
They have various toners you can choose from.
If it's just small areas,I wouldn't worry about the smell
Just open a door/window
Aerosol spray evaporate pretty fast
I have Used Mohawk spray can many times and works very well

11/18/15       #4: adjusting cabinet color ...
RobertJ

If you have never used a spray toner, practice first. You don't get a second chance to correct color matching at this stage of the game.....if you can, duplicate what you have now with another door.

11/18/15       #5: adjusting cabinet color ...
Chris

Sorry I didn't make myself clear I can get my color toned in right by staining back over my cabinet what I was asking is is there any thing in a clear finish I can use for a top coat over my Pre-cat lacquer. Over night I thought about buying me one of those air brush spray guns and put my lacquer in it. I can't bring my regular spray gun in the house.

11/18/15       #6: adjusting cabinet color ...
Paul Snyder  Member

Website: finishing.tips

You could get a portable spray set-up if it's something you can use enough to justify the expense. HVLP turbine sprayers are handy for this application.

In a real pinch another option is the Preval aerosol spray bottle set-up. Pour your own finish/paint into the bottle along with a little extra thinner and attach it to the aerosol can. They sell them at your local home centers and paint stores. It's a good idea to have extra aerosol cans just in case.

Be careful not to exceed the maximum dry film thickness (DFT) for the pre-cat your using. If the finish gets too thick it will crack within the first 1-2 years.


View larger image

11/18/15       #7: adjusting cabinet color ...
Rick Mosher

Mohawk also has precatalyzed lacquer in different sheens in aerosol cans. I have also used the preval sprayers but you have to really thin down the material to keep them from spitting and that can effect the sheen.

Mohawk precatalyzed aerosols.

11/18/15       #8: adjusting cabinet color ...
Mastercabman

Rick you beat me to it!
The preval are nice but you do need to thin pretty good
They suggest at least 20%
Mohawk precat aerosols are very nice
Dries fast and turns out real nice
If you are worry about smell/voc,I use my Festool.or Fein vacuum with HEPA filter and suck up over spray
You could also get a low cfm spray gun and a small compressor
Or get a turbine system

11/18/15       #9: adjusting cabinet color ...
Rick Mosher

For small areas I have also used my airbrush with either an air power pack or a CO2 canister set up with regulators.

11/18/15       #10: adjusting cabinet color ...
Chris

Thanks guys this is real helpful I am getting right on it.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)