4'x12' walnut table top options -- 0 -- 
1/12

I'm bidding on a conference table for a local company. They would like a 4' wide by 12' long table with a couple of box leg bases. Top will finish around 1.5" thick.
I'm having difficulty finding 13'+ long boards to make it out of. I'm considering either end gluing boards, kind of like a hardwood floor, or running the boards across the width so I only need 4' long boards. If I go widthwise though I'm worried about wood movement over 12 feet and how that night affect the bases which are connected by a double trestle under the top. I calculate 1.6" of movement in the Midwest where I'm located and this seems like way too much to handle even with clips attaching the top.
Any thoughts or suggestions?
1/12 #2: 4'x12' walnut table top options ...

Website: http://www.awwtx.com
13' stock is available, but generally at a premium. If the customer is expecting continuous runs, then bid the job based on the cost of the material. If the cost is above their budget, offer the alternative of butt joints which would be somewhat less expensive. Building the table out of 4' shorts as opposed to long lengths would be a disaster in my opinion, you'll have end grain showing all along the edges and it will not be attractive.
Feel them out for their budget and see if you're able to meet their expectations and make a profit, otherwise make a bid and be prepared to walk away. That table, properly constructed, will not be cheap.
1/13 #3: 4'x12' walnut table top options ...

There is a reason one almost never sees a solid wood walnut table 12 feet long. They are usually veneer over MDF or some other substrate.
A table with the boards running width-wise might work, I have seen some, and they are not ugly, but once again, there is a reason one doesn't see them every day,
Splitting it into two 6' tables that meet in the middle is one approach - makes production and moving that much easier, and in theory, one can find nice 6' walnut boards much more readily than any 13 footers.
1/13 #4: 4'x12' walnut table top options ...

I helped build some solid walnut tables about that size for a university law library.The tops were made from 6/4 walnut, #1 Common grade, with a "rustic" finish.
The owner of the shop couldn't find any 12' long walnut locally here in the Midwest. The walnut he did find was very expensive.He contacted a mill in Tennessee, who did have some 12' long stock. He found that it was actually cheaper to buy it from the mill, rent a truck, and drive it back.
He found the mill through Woodfinder, so I would suggest you try them also.
Good luck with your project!
Rick W
1/14 #5: 4'x12' walnut table top options ...

Website: http://thomasdiel.com
Not a criticism but when I saw the 1.6" my mouth opened so ran it through my wood widget app and at extremes flatsawn walnut 48"w @ 80% @ 100F down to 35% @ 70F yielded -1.091" so you not completely off but any shrinkage over and 1" bring ups a Seinfeld laugh.
I have also had the fortune to do 3qty live edge walnut last couple years- 2 that were those sizes and the slab prices were reasonable but went through local small dealers and two were air dried w major checks that were bow-tied and resin filled. Just make sure you have a pin moisture meter handy.
For budget minded clients you might suggest 5/4 glue up infill with 8/4 long grain edging with 8/4 bead board ends which keeps cost & weight down and keeps it flat? Have not done this in walnut but a couple oak lately.
fyi - My website has been having issues lately, so if your not able to get thru you not the only one!
1/14 #6: 4'x12' walnut table top options ...

If we do one that size we use 1.5" mdf for the form with a walnut veneer and solid walnut edge. You can order some very nice grains from Certainly wood and have it laid up.
1/14 #7: 4'x12' walnut table top options ...

Thanks for the notes. To clarify, the 1.6" was over the 12' if I ran the board the short way. With normal midwest numbers, I only get .5-.6" over the 4' width.
The customer doesn't want veneer as they are buying this table to replace a veneer one that has fallen apart. Appears they just hired someone who didn't know what he was doing for the original table, but they're stuck on solid wood.
I thought about a breadboard end, but at 1/2" of movement, I don't think this will look too good. I can handle the movement in the construction no problem, but the appearance of 1/4"+ sticking beyond, isn't too appealing. This would actually be my preference as wood would be cheaper and the added end support would be great.
I found 12' stock, but figure I'll only get about 11.5' out of it after trimming. I was able to find slabs that were 14' that I can rip down and have a lot of waste though. I'm planning to present to them an 11.5' table and a 12' option with the 12' option being about $3000 more due to the wood.
I'm also presenting a 12' option with two 6' pieces joined in the middle. Not as appealing, but much easier to move around for me and the wood is far cheaper too. I figure a couple of large T bolts will hold it and I have a third middle leg already due to some media they want run from the floor through the table.
1/14 #8: 4'x12' walnut table top options ...

Maybe a design change that will help to hide the movement , if you design the top with bread board ends that are wider than the top maybe enough so when the top shrinks or grows you still have a wider bread board end .Look at Greene & Greene furniture they used a spline of contrasting color at this intersection as an embellishment as opposed to trying to hide it .
1/14 #9: 4'x12' walnut table top options ...

cabinet shop next to me asked for a large walnut top from me. i priced lumber to bid but found lumber liquidators offered 25 x 144 butcher block tops for a fraction of what my wood cost was. true not a custom boardroom quality conference table, but he bought 2 tops cut joint on his slidèr glued together to make his 4x12. he was happy.
1/14 #10: 4'x12' walnut table top options ...

Butcher block or cutting board? I would guess the latter, the difference being that true butcher block has the end grain up.
Actually, I think that might make a very good looking table. Since the long grain would be vertical, over the 12' length of the table there would still be considerable seasonal movement, but that can be managed with proper base design.
1/17 #11: 4'x12' walnut table top options ...

IMO a top that big out of solid is wasteful and foolish no matter how you slice it. If they have a hang-up you need to educate them. What about having a pro lay-up with 1/16th walnut veneer. Might be a compromise.
1/18 #12: 4'x12' walnut table top options ...

It is wasteful to make a table out of wood? You are kidding, right? You know that wood grows on trees and there are 3 trillion trees on the planet, right? And this is "Woodweb", right?
Which reminds me - I need to sharpen my chainsaw - they aren't going to cut themselves down...
1/19 #13: 4'x12' walnut table top options ...

I meant wasteful money wise. Also consider the weight. But if that's what they want....
1/19 #14: 4'x12' walnut table top options ...

I am sure the buyer appreciates you looking out for his budget, but that is his concern, not yours.
1/19 #15: 4'x12' walnut table top options ...

Be concerned about this. #1 you gotta source that timber Difficult. #2 You have to glue line rip large planks. Nightmare without heavy equipment. #3 you have to glue it up and figure out how you are gonna plane something that big. Does Jason have a 48" anything? Do they even make anything that big?
1/19 #16: 4'x12' walnut table top options ...

A CNC would do the trick.
1/20 #17: 4'x12' walnut table top options ...

Website: http://thomasdiel.com
So, I did mean breadboard ends in my above post not beadboard, my bad.
On the straightline rip - I have had great glue joints w Festool track saw especially with the secondary glue-ups that are to big and cumbersome to pull off w/ a joiner - tablesaw combo. So gluing is a matter of clamping and clamping flat. I don't see a problem, besides the last glue-ups are so wide you would card scrape, hand plane and sand anyway with dominos spaced on 8-12" centers, no biggy. Thick veneer would be OK but your trading labor for materials at that point if you doing it right with balanced panel construct. Depends on the client and usage, I've seen too many veneer tops gouged beyond reasonable repair, hope you have a good burn in kit.
1/22 #18: 4'x12' walnut table top options ...

Thanks everyone for the help.
Turns out the customer thought they had a 14' deep service elevator that was really only 10' deep and so the answer was pretty simple in that the top was going to have to be two pieces. Kind of unfortunate as I was really liking the bread board design, but this will work too. Will end up with three legs so the center leg can support the two pieces joined together with T bolts.
I would have used a festool jaw to rip the boards if I went with 12' boards, but with just 6' ones now, I'll use the jointer. Dominos work great to bring it all together and I have a 25" planer so I only have to worry about cleaning up one glue line and with dominos and doing it right, it shouldn't be more than a few thousandths.
Getting the two top pieces to match in the middle with the T bolts could be a little trickier, but with some time, I should get this very tight. If there are any tricks out there, I'm all for it though.
The three legs will be connected with a couple of 8" wide trestles that will hide the cables as well and I'll attach the legs to the top with those small metal table top clips to allow for movement.
Thanks again for the help and suggestions.
0 -- 
Post a Response to this thread
notify me of responses to this topic
|
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|
|