Green White Oak -- 2 -- 
8/25

We have a customer building a green white oak timber frame home. The millwork and doors are kiln dried rustic white oak. He is using a clear oil finish on everything. The green wood in the frame takes the oil very light and hardly changes color while the millwork darkens quite a bit with the oil.
Would this be because the wet wood is not absorbing the oil? I know there are a few species of white oak. We tracked down the origin and the timber frame is Ohio and the KD material is New York and Penn.
I think it looks fine but the owner is trying to figure out if any solutions to make the KD material lighter. I am thinking in time everything will even out but no experience with wet wood.
Thanks
Joe
8/26 #2: Green White Oak ...

I'd be surprised that the oil is drying on the wet oak.
8/27 #3: Green White Oak ...

It dries. Here are pictures of his front door with one of the beam cutoffs. As you can see the door wood varies a lot in color with some pieces close to the beam.
After seeing the doors they are ok with it.
I am just wondering now what the timber frame will look like when it ages. Darker I would guess, but I have no experence with natural finished White oak.
I did find a picture of fresh cut white oak and it is very white colored.
View higher quality, full size image (3264 X 2448)
View higher quality, full size image (3264 X 2448)
8/27 #4: Green White Oak ...

Joe,
I think common logic would confirm your suspicion that the oil is not soaking in. If the wood fibers are saturated with water there is no place for the oil to go. As a result it just sits on the wet surface where on a microscopic level it mixes with moisture, thins out and lightens.
Personally I don't think there is any chance of darkening the wet beams until they dry out somewhat. I suppose you could try a very dark stain but that sort of thing is probably just looking for trouble in the long run. You also might have a little better luck with a water based stain but I've yet to see one that worked as well as an oil stain.
Good luck,
BH Davis
8/28 #5: Green White Oak ...

Looks like different oak species for sure. Over 400 kinds of oak, so no surprise. All wood darkens with age, except for walnut. It will darken, but will likely never reach the depth of color in the doors. They almost look closer to red oak to me.
8/28 #6: Green White Oak ...

I also wonder if the kiln drying could affect the color of the oak. I probably should post this on the sawmill forum.
The customer is comfortable with it now so moving on. I still wonder about it though. We have used quite a bit of white oak but never seen the light color the beams are. Except for sapwood.
8/31 #7: Green White Oak ...

The green oak should be dry enough on the surface to take a light stain within a few days, but I would hold off on final oil coats.
You ought to pick up a little Minwax Golden Oak to try on the new wood. I think it will have just enough color to get you back in the ball park.
I didn't recall any mention of the new beams having any sapwood. If there is any sapwood, it will surely be whiter than heartwood, and always will without a stain.
9/1 #8: Green White Oak ...

Keith,
I did suggest golden oak to the customer. They said they tried that and was darker than the oil. It does look like the golden oak era to me also..
The rustic white we are using have some sapwood and those boards match perfect. The beam in the picture however is all heartwood. I would guess the beams have been cut for a year or so. The house has been under construction for 6 to 8 months.
9/2 #9: Green White Oak ...

There are 20 species of white oak that are in the commercial market. The color varies from one to another. In fact, the lighter color is more unusual tan the door's darker color. The color does not change when kiln drying very much, especially on the interior. You certainly can get surface dirt, mold, and sunlight darkening. Drying really hot when wet can also darken the wood, but this also creates cracking.
9/4 #10: Green White Oak ...

Thanks Gene,
I was hoping you would offer an opinion.
I dropped off some doors at the job site and snapped a phone picture of the beams with T&G rustic oak we milled. I think it is already starting to blend and personally I like the contrast.
View higher quality, full size image (1280 X 960)
9/6 #11: Green White Oak ...

That's nice work Joe. It's always tricky having customers around while a job is in-process. Folks tend to get attached to the look of unfinished wood. Can't say I blame them, really. Glad it worked out.
9/10 #12: Green White Oak ...

I didnt see it in the other replies but perhaps mentioning to the customer that if he matches the color for move-in day it likely wont match in 5 years even if they were the identical species. They are building a structure that will change drastically over the next 5 years and it would seem patience would be imperative. I'd think the only rational solution would be to allow the timber frame to dry substantially THEN match IT to the KD woodwork.
Having been a GC for a long time I deal with this kind of stuff so often its nauseating. It would seem to me chasing a match today is going to guarantee a mis-match for the rest of the homes life.
9/10 #13: Green White Oak ...

The customer is highly involved in the project. This was a given from the start so it is a T&M job including all consulting time. They are actually a pleasure to work with and appreciate good craftsmanship.
This was curious to me also as never seeing white oak that color. They are ok with it now.
We have a natural spruce timber frame in our own home with natural VG fir doors and windows and white pine millwork. It is like night and day when new but all goes to the same mellow color with age. I also have a #3 white oak strip floor and it has darkened a little but not a lot of change compared to the pine and fir.
2 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|