What is the best miter saw setup? -- 3 -- 
7/24

Is the Festool worth it?
7/26 #2: What is the best miter saw setup? ...

Website: http://morantzcabinets.com
I am looking at the new virutex combo chop saw and rip saw. our work is mostly ultra modern here in south florida and I do not need a large crosscut capacity and I need to rip toekicks and fillers. this can replace my 12" Makita crosscut and bosch table saw. Harold.
7/26 #3: What is the best miter saw setup? ...

How do you like the Makita chop saw?
7/29 #4: What is the best miter saw setup? ...

Pat, We've got an old Makita 14" miter saw that has been very durable. Not a match to our Omga though.
7/29 #5: What is the best miter saw setup? ...

Website: http://morantzcabinets.com
Pat, the chop saw is a 12" sliding model. had it for years and it is great. We used to do alot of crown mouldings, but now that are work is all modern, its kinda big for just 4.5" toekicks and 2" top trim. The new Virutex model is a chopsaw with a table top and fence that uses the same blade. It should be adequate for our needs to rip fillers and toekicks as well as crosscut, all with one tool. Harold.
7/29 #6: What is the best miter saw setup? ...

Yea Larry but how portable is the Omga?
7/29 #7: What is the best miter saw setup? ...

Portable is a relative term. In this case relative to how big your gorilla is! It's too heavy but really accurate. We've got a variety of miter saws. Biggest capacity is a DeWalt slide, but you have to hold your mouth just right when cutting. That just might be the nature of the ones with all the adjustments.
Are you setting up an install van?
7/29 #8: What is the best miter saw setup? ...

Yes, I need to get a miter/slide saw.
I don't like anything Dewalt makes.
The short list is Makita, Bosch, Festool
Unless I hear otherwise I have a hard time seeing the value of a Festool.
I like almost everything Makita makes, and the Bosh jigsaw and the Bosh portable table saw.
The new Bosh slide miter saw is neat as it uses a hinge system instead of tubes. But not sure it is the go to.
7/30 #9: What is the best miter saw setup? ...

I owned the Bosch 12" dual glide for about 4 years. After fighting the dust collection with homemade shrouds even while hooked up to the vacuum I sold it off to help fund the kapex purchase. I didn't think the dual glide could be beat until I got used to the dual laser setup and accuracy of the bevel gauges. I'm about two months into the kapex and love it. The lasers wrap around non square moldings making it literally a walk up and cut scenario on the first try.
I'd give the kapex a shot, they give a 30 day money back guarantee.
Josh
7/30 #10: What is the best miter saw setup? ...

Thanks Josh
7/30 #11: What is the best miter saw setup? ...

Yes, Festool is worth the money. I have bought Hitatchi, Dewalt and Makita saws in the past few years. I got sick of adjusting fences at least once a month. I bought my Kapex 18 months ago and have never had to adjust anything, it is always dead on. I am going to buy another one to put in the trailer for installs. The best thing is, I don't have to have these conversations every years as to what saw I should try.
7/30 #12: What is the best miter saw setup? ...

Thanks Daryl
7/31 #13: What is the best miter saw setup? ...

I don't know about the laser aspect but most 12" saws I've used are about the same except......I like to pull the guard up a little bit with my thumb to see exactly where that blade is hitting. Sometimes 32's count. The dewalt guard is built so I can do that easily. The others that I've used aren't.
7/31 #14: What is the best miter saw setup? ...

Thanks Joe, cept I hate all things Dewalt, I will say though the newer ones have a shadow line that is quite handy.
7/31 #15: What is the best miter saw setup? ...

I bought the festool Kapex for the shop , was not impressed with the accuracy. One thing it does it kept its value on the second hand market. For onsite we have dewalts 717. In the shop we are going to the Omga saws . These dewalt 717 are as accurate as the Kapex. Maybe I was expecting too much from the Kapex , due to the success we have had with all the other festool tools
8/5 #16: What is the best miter saw setup? ...

What Dan said. The kapex has slop (side to side) like all the rest of the saws so the user must learn to use the saw and not pull to left or right as saw comes down into the cut. It excels at dust collection though. The lasers are nice I guess but I'm used to the sneak up method anyway. I have an omga chop saw for the very important cuts. I'd get the kapex for dust extraction alone though. Other than that, I've been perfectly happy with a makita 10". 12" adds too much blade wobble. Add blade stabilizers and you're left with a 10" capacity blade plus or minus.
8/5 #17: What is the best miter saw setup? ...

Thanks for all of the feedback.
I looked at the Kapex today.
The rep said that the saw is commonly horsed and not allowed to go at it's own pace which created/contributes to the slop.
The dust collection appears to be very effective.
The lasers are awesome and would be great for odd angles. I particularly like how fine the lines are.
The controls are also awesome particularly the micro adjustments.
Another factor is the weight as it is very light.
Although an intangible there is something about using German made machinery that makes it pleasure to use.
BTW you guys aren't saying you use an Omga in the field are you?
8/6 #18: What is the best miter saw setup? ...

Check out the little Makita slider. It has a lot going for it as an install saw: light, very accurate, no deflection on the little blade.
The capacity is plenty for a typical install, and beveling only one direction never bothers me. I've finished site built stairs with it just fine.
The dust collection is very good too, at least as good as the Kapex.
I tried the Kapex, but returned it before 30 days. The only thing I liked about it were the large bevel scale, and the counterbalanced head when setting a bevel. A nice saw, but nowhere worth the money. Buy 3 little Makitas for less money...
Good luck,
Mark
8/6 #19: What is the best miter saw setup? ...

Thanks for all of the feedback that was very helpful.
I bought the Makita 10" sliding miter saw with a Bosh stand.
8/7 #20: What is the best miter saw setup? ...

Hitachi C10FSH is my favorite. I have had one in the shop 9 years now and millions of cuts and still accurate.
8/9 #21: What is the best miter saw setup? ...

I have two of those Hitachis, one for 10 years as well, and have yet to use another saw I like better.
8/9 #22: What is the best miter saw setup? ...

We had two of those hitachi saws , they were stolen in 08 , and not quite sure why we never replaced them , they were great saws,. One thing we did learn was we didn't need a 12" saw all that often. We have one if needed but a 10" we found is more accurate due to the smaller blade .Evven though we use the best blades possible there is more deflection in a 12" which causes a bad cut in certain woods.
The Kapex was great in terms of dust collection and a few other options.
8/10 #23: What is the best miter saw setup? ...

I'm in the market for a new saw as well. The Festool is out of my price range.
Out of all of the new ones I liked the design and stiffness of the Milwaukee 12" slider. I have been using the 12 for 15 years and have a couple of Forrest blades so I won't be going for a smaller one.
The hinged Bosch wasn't stiff when fully extended.
I've never liked Makita chopsaws. Any other worth while options? Does anyone have any real world experience with the 12" Milwaukee?
8/10 #24: What is the best miter saw setup? ...

So far the survey says:
1 Virutex
2 Omga (but you have to have a strong helper)
3 Kapex
2 agin the Kapex
2 Dewalt
1 agin the Bosh
3 Makita (not including me)
3 Hitachi
1 agin the Makita
8/18 #25: What is the best miter saw setup? ...

I have the Festool in my home shop and I like it. I found DeWalt saws to be the worst. The fence doesn't come straight from the factory and the blade slides to the side if you try to trim less than 3/16" off the end of a board. The biggest reason I bought the Festool was for the dust collection. The other reason was that I had confidence that the fence was going to be straight. I don't mind adjusting the saw for a square cut, but that becomes impossible with a crooked fence.
8/18 #26: What is the best miter saw setup? ...

Website: http://www.resourcewood.com
I bought the Kapex for its light weight portability and portable dust collection. It does not travel well or at least I would not call it rugged . Too many plastic parts for such an expensive saw. I had to replace parts the first year because it could not take riding in my trailer folded in the vertical stand. I now travel with it laying down and adjust the bevel adjustment to rest against other parts so it is not changing position when going over rough roads.
8/18 #27: What is the best miter saw setup? ...

One more for and agin the Kapex
8/19 #28: What is the best miter saw setup? ...

I had the kapex but sold it. As others have mentioned, dust collection was excellent. Accuracy was pretty good. My biggest issue was the handle/trigger/button configuration. I just couldn't get used to the vertical style handle, felt very akward to me. Maybe I've just used the dewalts too long. I kept on a rather tall table, so that may have contributed.
8/19 #29: What is the best miter saw setup? ...

The natural position for the arm and hand is in the vertical position.. Dewalts seem awkward to me. LOL Everybodys diffirent.
I think this is another one of the Dodge,Ford,Chevy,Toyota type deals
My Toyotas have never failed me but Chevy and Ford sure have.
9/12 #30: What is the best miter saw setup? ...

If I were ever to buy another SCMS I would buy the Bosch Glide. The Kapex has too much flexure for my liking. Ive owned three bosch SCMS and currently use the 5412L but if I ever upgrade it will be to the glide.
9/13 #31: What is the best miter saw setup? ...

just sold my kapex would never stay square and after 5 years needed new motor and gear box tried 2 new glides both sucked had to much play in the glide and the tables where not flat
bought the 780 dewalt works great dead on and holds it and love the light versus the laser
11/18 #33: What is the best miter saw setup? ...

The comments about a 12" VS a 10" blade not having as good a cut get me. Unless there is slop in the arbor/pivots the blade change of 1" in radius really shouldn't matter. We don't install so our OMGA is for shop use. It is 300mm (12"+-) The cut is very nearly slick, both sides of the Leuco blade. It has been used as the main miter saw in a production shop for 15 years. Miter adjustments are easy and stay where put. A tad heavy @ about 50's.
3/29 #34: What is the best miter saw setup? ...

I do not sell tools or work for Milwaukee, I have a cabinet shop and another shop where we do all our finishig. I could talk for an hour about all the great qualitys of the 12" Milwaukee.
Number one reason I chose that saw over all the other competitors including the kpex is the stiffness is superior to all of them. The sideways movement of your slide saw is where you win or loose on the quality and accuracy of your cut!
You can instantly compare the saws if you can test them all in the same place.
The key test is to bring the head all the way towards you, lock the slide, lower and "pin" the cutting head in the down position. Now grab the front adjusting knob ( left -right ) pivot control. With your other hand grab the cutting head . Hold the base firmly while moving, testing the cutting head for deflection!!
Milwaukie is stiffer, has less deflexion then any of them. The kapex design with their wide spread bars should have been the winner. Not so.
I can't believe how handy the digitial readout in one thenth of a degree is in speeding/adjusting my cuts . Let alone being able to return confidetly to my previous cut. Dust collection works great.
There are two mitersaws that beat the Milwaukee for stiffness, but they are in the $2500 to $3500 range and usually you only see them in shops.
A little late to the party.....
Just my two cents.....
3/29 #35: What is the best miter saw setup? ...

Oh yes , I forgot to mention it has 2 lights, one on either side of the blade. The trouble with lasers are that in low light conditions the line is so wide and bright you no longer have a fine line for accurate cuts! Not all of my job sites are well lit. In commercial work often your ahead of the electricians.
just jim in Las Vegas
3/29 #36: What is the best miter saw setup? ...

Good to know, if it had been 8 months ago I would have considered it.
Generally Milwaukee was a good brand but these days I go with Makita.
But I do agree with you about the stiffness which is not going to happen with a single pivot point. To achieve that you have to have an A frame design IMO.
3/29 #37: What is the best miter saw setup? ...

Previously the winner was makita. And for that reason makita is the saw I owned and enjoyed. I really wanted them to win again as there new saw had a 15" slide. But not as stiff as the red saw. The Bosch was silky smooth and a truley new design, but once again not as stiff.
Years ago when our shop had a radial arm saw. No matter how I adjusted it, it would not hold square. I bolted the base to a cement wall. Then with a 3/4" sheet of plywood made into a triangle with the one side anchored to the wall just above the saw . I attached the arm to the plywood and forced it to cut square. That's all it would cut but it was worthless for anything else anyway.
If our work looks bad so do we.....I hate poor quality tools.....
3 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|