Designing a Large Slab Planer/Flattener -- 0 -- 
1/13

So I am in the beginning stages of trying to design a tool to ease the process of flattening large live edge wood slabs (up to 4'x8') There is a well known article in FWW about making a sled for a router and some rails for it to ride upon. I'd like to take that idea to the next level by using a huge face mill (6-10"?) and an industrial motor with variable speed control. Basically a super Router. I plan to build the sled out of steel and the rails out of steel or aluminum tubing and have bearings of some sort for smooth operation and movement in the X-Y axis....think CNC machine without the computer or automated controls; I would move the carriage manually, possibly with a hand crank and chain drive system.
Note: Lucas Sawmills has an attachment that does this same type of thing for their system, but that only works if I already have their sawmill, which I do not. I have a woodmizer.
The goal here is to have a stronger machine than a basic router that can cut more wood in one pass. It serves as a jointer/planer combo for slabs that are too big for my machinery. A shroud or hood for dust collection would be essential as well.
The part that I need to get advice on is the Motor-Mill combination. I figured on finding the biggest face mill that seems reasonable, with replaceable cutter inserts, and then have an arbor/collet type of adapter machined that would attach directly to the output shaft of the motor (Baldor Industrial). I could use a variable speed control for different woods. Issues that I see are determining the proper cutting rpm for such a large mill, reducing chatter and vibration, the interface between the motor and the cutter and sizing the motor appropriately.....I obviously want as clean of a finish as possible, similar to what I would get if i put this slab through a gi-nourmous planer, which I cannot afford.
Anyone with any ideas please let me know!
Thanks,
Muley
1/13 #2: Designing a Large Slab Planer/Flatt ...

By the time you invest your time, money and resources into this thing you could buy a used CNC and be done with it. I have a 4x10 CNC and flatten slabs using a 100mm cutter. takes longer to put the slab on the table than does it to surface.
1/13 #3: Designing a Large Slab Planer/Flatt ...

I have been using a CNC to flatten live edge slabs since '99. I use a spoil board flattener with insert tooling - it gets 'er done.
I wrote software to automate the process - including parameters for length and width along with the step down value per pass.
It's the only way to fly.
1/14 #4: Designing a Large Slab Planer/Flatt ...

Bruce and CNC, how much do you take off in a single pass with the spoilboard cutter? At what feed speed?
1/14 #5: Designing a Large Slab Planer/Flatt ...

Joe, I am using a 100mm insert cutter, Leitz. My feed rate is set to 6 meters per minute but I can slow that if needed using a dial on the CNC. Most of the slabs I get are NOT flat so the first several passes won't contact the whole slab. To start I use 10mm cutting depth but once I get to full surface it might be 5mm. I have a 4x10 pod/rail machine that will handle 7" thick, sometimes hot melt a 12" square piece of melamine under the slab at each end so that the vacuum cups have something to suck against. When I have a flat surface I'll turn it over and pry off the melamine and surface the other side.
I have to give credit to Brian Personette for helping me with the programming. Using a single tool path as a sub program, based on the part size it makes as many passes as required to surface the part. I only have to enter the part size. To achieve successive passes I stack the program and change the thickness on each stack.
I set the tool to cut zero depth and change the cut depth by changing the part thickness. In that way I can have a different depth of cut on each stacked program by making the material thickness different. My pods don't release until that last program in the stack is run.
I must say it makes a awful mess removing that much material, clean up is a pain. For my effort I charge a hundred and fifty dollars and up.
1/14 #6: Designing a Large Slab Planer/Flatt ...

Website: http://www.kswoodworking.com
There's a company in Australia that has designed and built what you're describing. See youtube demo link below.
Only one unit so far in the U.S., and it's installed at Newport Nautical Timbers in Bristol, RI. I've had them use it to flatten several slabs for me. The nice thing is that the router travels longitudinally, not crossways (like on a router sled) so you don't get blowout on the sides/edges.
They cost about $18k through a distributor in Canada.
YouTube Demo
0 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|