Solid walnut countertop -- 1 -- 
10/19

We've been asked to fabricate a solid 3" thickness walnut countertop. I'm thinking of using a "panelite" material for a core. (Basically a torsion box) with 1/8" solid skins. Adhesive would be titebond III or epoxy. The counter is 10' long so it seems a bit much (and possibly risky) to use all solid material.
10/19 #2: Solid walnut countertop ...

Bad idea. We have made thes by double laminating the edges for 6" to give the effect of 3" thick. you have to build the end grain to match at the short end of the rectangular butcher block. Top layer is 1.5" thick. Use additional blocks underneath as supports.
10/19 #3: Solid walnut countertop ...

How wide?
10/20 #4: Solid walnut countertop ...

I would not be surprised to see a bit of crowning across the width and also a major crack develop, especially if a dishwasher is underneath or near a sink. Risky idea.
10/20 #5: Solid walnut countertop ...

Dave,
I think we may use the option you suggest. I've used that method before and it works well. There's a bit of client education needed, of course, as they expect 3" thickness throughout.
Mike
10/20 #6: Solid walnut countertop ...

A torsion type construction has the ability to resist movement and keep weight within reasonable bounds. "End grain" the ends and add long grain along the sides and then 1/8" Walnut top and bottom. The drawback is the the gluelines at the ends will give away that it is not solid, but no one other than woodworkers may care. Dishwashers and other heat generating appliances should not affect it, either. It is always a good idea to line the underside near such appliances with heavy grade aluminum foil.
A 3" top top that is made of 8/4 x 3"+ plies will weigh a lot (over 200# if it is 24" wide), but be fast and solid. Plastic resin glue to prevent yellow glue squeeze out down the road. The width of each board will allow you to eat up all the lower grade walnut, since you just have to present a good edge to the top.
A 1-1/2" thick top with build up will be more time consuming - tedious in fact - but take less lumber - it will be a wash. Again the gluelines at the end grain will give it away, if that matters.
10/20 #7: Solid walnut countertop ...

Listen to Gene. Don't do it. The solid will crack, warp or both from being constrained by the torsion box.
10/20 #8: Solid walnut countertop ...

here is a pic. we did this in hickory so there is a lot of colour variation but the client loved it.
View higher quality, full size image (960 X 539)
View higher quality, full size image (960 X 640)
10/21 #9: Solid walnut countertop ...

I guess if you have to go the solid route, educate the client verbally, in writing, with lots of legalese. If "rustic" is acceptable down the road, they may be happy, If not, lots of luck. I'd bet Gene is right.
10/21 #10: Solid walnut countertop ...

Here is an image of a solid 4" thick Wenge top that is over 10' long. 8/4 flat sawn Wenge was ripped and turned for the thickness - same throughout.
We glued it with epoxy (wetting out both pieces), and had a few small cracks to touch up after finish, before delivery. Easy to mix up epoxy and some sander dust and fill, then scrape flat when cured. Put some good masking tape either side of the crack for easy clean-up and to avoid filling the grain with glue.
We also do tops as torsion boxes on stable cores and so we can do big, wide miters, curves, etc. Balanced, with 1/8" to 3/16" on both sides. Never a problem, except for those same damn hairline cracks. You just have to find and repair before delivery.
View higher quality, full size image (1944 X 2592)
10/21 #11: Solid walnut countertop ...

Neat looking. Did you hire a piano mover?
I like Wenge but always seem to get slivers from it.
10/21 #12: Solid walnut countertop ...

David,
How did you put that profile on the edge?
It looks beautiful!
Hastings
10/21 #13: Solid walnut countertop ...

The edge is done with a router and the largest round over and cove bits available. The cove bit requires a long shank. The inside corners are carved.
Yes, the thing required four people to move it. And yes. Wenge will give you splinters just by looking at it. Once it is sanded and finished, it looks great.
10/31 #14: Solid walnut countertop ...

According to the people I asked about them, they are a real ball-ache, becuase you have to oil them frequently and they get cut/chipped easily. No-one I spoke to thought they were a good idea after buying them.
There are apparently other alternatives besides granite and wood - different types of stone etc.
11/12 #15: Solid walnut countertop ...

gorgeous (solid) tops, I'll come back & post some pics of mine after I get some work done today...)
I do SOLID wood tops for the vast majority of my jobs. always SOLID. never any fake "skinned" garbage
My tops & the beautiful solid wood tops above are professionally made pieces.
complete understanding of the species (mc, etc). proper adhesive choice...
Its an art,
asking how to make a 12/4 fine wood top is akin with asking how to build a piano soundboard... no disrespect intended, but you should sub this part out, to an experienced craftsperson
If you choose to do it yourself, the best chance you'll have is with Festool Dominos & powdered urea resin glue (talk to Sal at monster woodshop about your prroject)
do you have industrial clamp rack or press with sufficient capacity?
11/12 #16: Solid walnut countertop ...

here's a vanity top with undermount Kohler Verticyl lavs, species is (face grain) German Beech 1-7/8" finished thickness, finish is dye stain/wiping stain/glaze/Conversion Varnish (cat'd sesler between steps).
11/12 #17: Solid walnut countertop ...

island top 54" width 8/4 German Beech , undermount hammered copper prep sink; /dye stain/light distress + Waterlox Original
(all 6 sides!)
IIRC, there are about 70 14mmx140mm Dominos.(PUR "brown glue" throughout )
assembled in sections in Quick clamp rack, then final assessment in an old, manual 12ft Black Bros case clamp.
View higher quality, full size image (3264 X 2448)
View higher quality, full size image (3264 X 2448)
View higher quality, full size image (3264 X 2448)
11/12 #18: Solid walnut countertop ...

previously described Vanity top, + copper sink in 54"w island top
View higher quality, full size image (3264 X 2448)
View higher quality, full size image (3264 X 2448)
View higher quality, full size image (3264 X 2448)
11/12 #19: Solid walnut countertop ...

where's your job located?
1 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|