Thick Veneer Bar Top -- 4 -- 
3/30

Last year I built a very large bar top out of solid 8/4 Zebra Wood - against my better judgement but trying to please a very good client. It looked absolutely awesome the day it was installed. You know what's coming... 6 months later it's coming apart in slow motion. I don't need to troubleshoot what went wrong- it's probably a poster child for how to design and build a bar top with the absolute maximum potential for failure. What I do need to do is replace it, so I'm hoping for a reality check on a replacement that will let me sleep at night.
Here are my basic thoughts and questions (see photos and drawings):
- A base layer of 3/4 plywood or MDF (or particle board?). It sits on a very narrow center wall, so stiffness/flatness of this layer is critical.
- A second layer of 3/4 plywood or MDF (or particle board?) that gets a veneer top. I'm thinking it should be screwed but not glued to the base layer to accommodate any movement between the two layers?
- A veneer of 1/16 thick Zebrawood planks. This is to get the look of the glued up boards of the original, something I don't think is possible with paper-backed veneer. My thought is that this is thin enough to be stable and thick enough to be durable. I don't know if Titebond III is a good choice, or something more rigid like Unibond. I also don't know what substrate would be most stable to glue it on - plywood, MDF or particle board.
- Built in 8 or 10-foot sections in my shop, sanded and finished all 6 sides and assembled on site with splines and countertop bolts.
- I have heard many times that these assemblies should be balanced with veneer on the bottom as well, but I'm thinking that wouldn't apply to this double-layer substrate?
Any suggestions or cautions you may have are welcome. After watching the original $16,000 bar top self destruct, I really need the replacement to be bulletproof. Thanks in advance.
View higher quality, full size image (480 X 640)
View higher quality, full size image (1512 X 404)
View higher quality, full size image (1574 X 883)
3/30 #4: Thick Veneer Bar Top ...

need more info. no reason it would fail, except maybe- bad attachment, bad glue, dramatic change of moisture between shop and or on jobsite, lumber defects etc. I've made a lot of tops like that 8/4 and thicker. the edges always look different when veneered, even thick veneer. against all forum advice i have fabricated many tops with ply core, 1/4 plus thick veneers both sides pressed with moisture cured urethane flooring cement. 1/8 veneers I've used titebond II or even contact cement , for decades and have not had to replace a top.
3/30 #5: Thick Veneer Bar Top ...

Very sad to hear about that top coming apart.
Your plan is sound. Here is what we would do:
A solid core of MDF at whatever thickness you need it to be, minus 1/8". Then apply the waterfall edge band with the 1/16" veneers, then the top and bottom with the 1/16", preferably at the same time.
You want to have a balanced panel, with equal finish on both sides to keep everything nice and flat. Edge band after the faces may catch clothing and start to pull off, so it is better to have the face over the edge band.
The faces should be edge glued and taped into a single piece when laid. The edge glue will help keep joints from opening while being laid and pressed. We use a vacuum bag. Glue? low/no water. I'd lean towards polyurethane or Unbind 800. Not epoxy - unless the wood demands it. I have no track record with Zebrawood.
The method we use allows nice win miters and other details that can't - or shouldn't - be done in solids. But you can now teach that class, eh? Best of luck.
3/30 #6: Thick Veneer Bar Top ...

What is the size of the top in plan?
3/30 #7: Thick Veneer Bar Top ...

Thanks for the comments so far. The main reason for the failure is wood shrinkage. I warned the client that I really needed a few months for the lumber to reach a good MC before starting to machine it and glue it up, but that just wasn't an option. Also the boards are glued up perpendicular to the length of the bar, maximizing the number of joints and cross-grain shrinkage. The whole point of doing it that way was to get the dramatic end grain showing. I expected those problems, but I hadn't figured on the S-shape of the bar adding extra resistance to shrinkage and exacerbating cracking, checking and joint failure. The radius of the two curves tightened measurably due to shrinkage. Kind of fascinating to watch in a sort of train wreck way.
The bar top is 23" plus 4" drink rail, a full 2" thick at the front edge. I can't imagine trying to handle 2" thick MDF, which is why I thought a build up was more practical. Plus it allows for the integrated drink rail. If I need to balance the assembly with a veneer on the underside, does it really need to be the 1/16 Zebra planks as well? That's double the material expense and labor for something that won't be seen. Would HPL on the underside suffice, or must it behave identically to the Zebra wood?
I take your point about having the face overlap the edge band. Zebra wood tends to get brittle when thin, so when I trim the end grain of the face flush to the front edge, there may some minor splintering and tear out. Applying the edge band last would hide these defects.
3/30 #8: Thick Veneer Bar Top ...

You can use end grain slices for the edge band, but you will not be able to match them to the face grain. I don't know that most people would read that as what is going on. I think they see wood, they feel it, and they enjoy it. Only us anal retentive types worry about some of these details.
I know the safe thing to do is to balance with the same species/cut/source material, but the veneer shops will back with a lesser species that has the 'same characteristics'. Good luck there. The expense may be cheap insurance unless you can match the characteristics.
I understand you want this one bulletproof. I have been there.
You could do the build up, but still use the balance backer thick veneer, but I would not trust 3/4" or maybe even 1" MDF to support itself over time. 2" could warrant a torsion box, but then only if weight was critical, and it won't be once it is in place. A torsion box would certainly complicate everything, for a little weight savings. Plywood can save some weight.
The drink rail could be separate and set into a machined rabbet on the underside of the top. And the edge band on first, then the faces will be better for resisting catching.
You could go to 1/8" both sides and edges. That would give you a good solid corner to ease hard to prevent any snags. Those hard square corners get hit and then they open a bit.....
As for that slo mo train wreck - any photos? The best thing to do with your pain may be to share it.
3/30 #9: Thick Veneer Bar Top ...

I've done a fair amount of work with zebrawood veneer. Make-up your core thickness by gluing each layer together, there won't be any movement between layers. I apply veneers in a vacuum bag. Show veneer on edges and top face, and veneer the bottom with something less expensive like maple. This will keep the piece from warping. The other thing I'd like to point out is Zebrawood is open grained. So, in a potentially wet situation from a bar you may want to fill the pores and then topcoat. For this application I would use a UF glue, though you could use Titebond I since this is essentially a flat glu-up.
3/30 #10: Thick Veneer Bar Top ...

I'm with David on this one, edge band first. Substrate marine ply. Grain fill the Zebrawood to fill pours. For sure a balance veneer, look for something that has about the same movement. That has to be the widest glued up board I've ever seen.
3/30 #12: Thick Veneer Bar Top ...

You asked for train wreck photos, so here are some. The shrinkage has manifested in only a handful of places, as long sections have shrunk but stayed together as complete units, only failing where the adjoining section is prevented from being dragged along (if that makes sense). It seems that the transitions from straight section to curves are the worst. Here is the worst of the lot, pictures taken on 10/27/15, 12/2/15, and 1/13/16.
View higher quality, full size image (480 X 640)
View higher quality, full size image (480 X 640)
View higher quality, full size image (480 X 640)
3/30 #13: Thick Veneer Bar Top ...

Here's the bar soon after installation on 9/3/15, before the grief began.
View higher quality, full size image (480 X 640)
3/31 #14: Thick Veneer Bar Top ...

Is that the only place it cracked?
3/31 #15: Thick Veneer Bar Top ...

That's by far the worst split, but there are about 6 other noticeable ones. Plus several sections of 3-4 boards that have crowned a bit so that the original long flat expanse is somewhat hilly now.
At first I thought I could wait out the shrinkage until it was all done, then clean up the splits, draw them back together, sand things flush again and re-finish. But the scattered sections that are crowned, cupped, warped, etc. are just too much to hope to ever get the whole thing flat and straight again. And who knows when the summer humidity comes if it might begin to swell and start growing again.
3/31 #16: Thick Veneer Bar Top ...

Those are painful to look at. Good work, gone bad. Do you know the initial moisture content when you worked the wood? How about the MC today? A quick look at the Shrinkulator shows a 20' long (wide) top will move over 1.5" with a 2% change in MC. That demands a floating mounting method. The mention of cupping across width tells you that the initial MC was too high - too late.
I would be sure the veneer is of the proper MC as well as all the materials, acclimated together in the same room for a couple of weeks.
For the record, miters would most likely never succeed long term in solids like that. However, the curves and straights can work if they were mounted in such a way as to let the top move - expand and contract with the inevitable changes in RH in the room.
4/1 #17: Thick Veneer Bar Top ...

Website: http://www.factoryfurniture.co.uk/
You want to have a balanced panel, with equal finish on both sides to keep everything nice and flat. Edge band after the faces may catch clothing and start to pull off, so it is better to have the face over the edge band.
4 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|