furniture base on euro cabinets
2/17/16
what is the best way to build furniture base for euro style cabinets and install them?
2/17/16 #2: furniture base on euro cabinets ...
We cut the desired profile into a piece of base moulding, usually in the center, then add a 3/4 x 2 nailer to its backside top edge, leaving it to the installer to miter the assembly. Sometimes if the moulding is tall enough you can get an angle screw gun in there from underneath. Otherwise we'll pin nail from inside if it's a visible interior, or screw down if a drawer box would cover the screw head.
2/17/16 #3: furniture base on euro cabinets ...
Vague, but here goes: make a base...4 feet and an apron and install to wall
2/20/16 #4: furniture base on euro cabinets ...
If you want a screwless and nailless option, cut a strip, run a groove with a slot cutter along the whole edge, and screw it flush with the front edge of the cabinet, on the underside. then run lamello/biscuits on the back side of the base. After cutting the base to your lenghts you can just glue in place. I attached a picture in case my explanation doesn't make sense
View higher quality, full size image (3264 X 2448)