Cost-effective CNC melamine drawer boxes?

2/17/18       
Gene Davis

How cost-effective can my design be, which involves blind-dado fronts and backs, full dado captive bottom, edgebanded top edges (no ends)?

By necessity, my design is such that every front and every back needs to be flipped to complete the CNC cutting.

When it is all said and done, is there still a nice savings when compared to doing these d'boxes this way, versus using 5/8 baltic birch, dovetailed?


View higher quality, full size image (803 X 652)

2/17/18       #3: Cost-effective CNC melamine drawer ...
JM

Only suggestion I can make is forget the grrove for the bottom on the CNC. Just set up a small tablesaw with a dado. It will be much faster than flipping the sheet.

2/17/18       #4: Cost-effective CNC melamine drawer ...
rich c.

I'd think a dowel drawer would be just as strong and faster to make.

2/18/18       #5: Cost-effective CNC melamine drawer ...
Dan cook

I agree a dowelled drawer is much quicker and holds itself together once assembled. Ther are no visible fasteners and construction is solid. Been doing it that way since the early 80’s. Never a complaint or failure with a drawer.

2/18/18       #6: Cost-effective CNC melamine drawer ...
JP Member

Mozaik has a drawer option like that. I didn't want to flip sheets so I haven't tried it. Plus you would have to leave them in clamps until they set.

Like the others I use dowels.
Dovetails in solid drawers.
For less money metaboxes.

2/18/18       #7: Cost-effective CNC melamine drawer ...
Gene Davis

The CNC shop we use is routinely making drawers exactly like this, and I'll find out whether they flip parts to cut the dados in the front and back, or do it on another machine such as a table router or table saw.

Dowels are out of the question as they would require edge boring, something the CNC shop is not set up to do.

The drawerbox shown in the original post was for pairing with 3/4 Blum 230 standard slides. We've another design the CNC can cut that adds the rear notches and 6mm hook holes for matching the drawer to Blum Tandem slides.

2/18/18       #8: Cost-effective CNC melamine drawer ...
JM

and another option, dont dado the front and the back. Cut them short and run the bottoms the full length from front to back so its only captured in a dado on the sides.

2/18/18       #9: Cost-effective CNC melamine drawer ...
Gene Davis

Here is an image of sixteen drawer parts nested for CNC cutting, using two sheets each of 1/4 and 5/8 melamine. The drawers are 4-1/2" high and for a 24" wide cabinet.

I'm thinking it would be faster and easier to take the 32 parts that are the front and back sides and zip them across a table saw with a stack dado blade, than positioning one at a time for flip cuts on the CNC.


View higher quality, full size image (1046 X 937)

2/18/18       #10: Cost-effective CNC melamine drawer ...
JP Member

You can do flip side cuts easy enough. Do the whole sheet at once.

I use qualified tenons on my cases. You do the flip operations first, then turn the sheet over and cut everything else and cut the parts out. Everything is done that way.

I just didn't want to do flip side operations on drawer parts.
Then those tenons either have to be clamped or shoot a few brads in to hold them while the glue drys.

You could position them one at a time for flip side operations, but that would be crazy:)
Typically I only do large parts seperate with flip side. Here is an example, I have dados and shelf pin holes on both sides of a center partition. Just bump the part up to the locating pins and turn on the vacuum.


View higher quality, full size image (820 X 412)

2/19/18       #11: Cost-effective CNC melamine drawer ...
Jared Emery

I do 3/4 plywood drawer boxes, edgebanded on the top edge. They're cut along with case parts so they don't increase the material needed by much, and assembled with Hafele's Rafix flush cam. Drawers go together quickly and self-square with the bottom fully captured. No horizontal boring needed, and yes we flip sheets, but we do that anyway for a few of our cabinet parts and the software is smart enough to minimize the number of sheets so all the parts that need it are nested together. On a 40 sheet job, maybe we flip 4 sheets.

2/21/18       #12: Cost-effective CNC melamine drawer ...
Gene Davis

OK, the word is back from the CNC guy, and he confirms he does these regularly, each front and back being flip positioned for groove cutting on reverse side, and that all goes quickly and precisely, no chipping, no problem.

So here is a look at the details, in Sketchfab, which you can open, spin around, zoom as you wish, and inspect.

As can be seen, this box is detailed for the notch and hook hole needed for Blum Tandem slides.

Click here to see in Sketchfab

2/23/18       #13: Cost-effective CNC melamine drawer ...
Derrek

Website: http://closetdr.com

We build our boxes very similar to this. We run them in 3/4" material with the rest of the job. To avoid the flip, fronts and backs are 3/4" shorter and the bottom is full length of drawer. Bottom is screwed into front and back from bottom with a couple screws. We have guides aligned so that screw that holds it in place goes into dado on bottom.
Running the dados takes some time on the cnc, but makes assembly a breeze

2/26/18       #14: Cost-effective CNC melamine drawer ...
Derrek

Here a video on how we build boxes

https://youtu.be/Q9dEiUIhwCw

2/26/18       #15: Cost-effective CNC melamine drawer ...
Gene Davis

That's a helpful video. Thanks.

We'll go ahead and re-think the drawerbox assembly used when 3/4 Blum Standard slides are used.

When using Blum Tandem undermounts, we need the 1/2" inset for bottoms, and also that back end notch and hook hole, so I'm not sure how 5/8" through-end bottoms will work, but we'll revisit that, too.

2/26/18       #16: Cost-effective CNC melamine drawer ...
Derrek

The drawers in the video require no flip on the sheet. We build cabinets in a similar manner also and no flip is needed..

We talked about doing undermounts and they have some different requirements, my cabinet vision guy said he has done them with a 3/4" bottom and added a route to the bottom for clearance. Our solution was we dont do undermounts.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello
    Today's Sponsors
    • Better Vacuum Cups, Inc.
      Vacuum Cups for All CNC Routers As Well As Many After Market Parts for Your CNC
    • Carter Products
      Band Saw Guides, Blades, Wheels, Tires, Line Lasers and 2D Projectors, Wide Belt Sanding Accessories, Vacuum Holding Systems and More
    • Colonial Saw
      North American Supplier of Striebig Panel Saws, Lamello Specialty Tools and a Wide Range of Saw and Tool Grinding Machinery
    • Cabinetshop Maestro
      Web-Based Project Management Software for Custom Cabinet Shops - Manage Jobs from Prospect to Punchlist Through Scheduling, Task Management, Time Tracking and Communication
    • Biesse America
      Woodworking Machinery - Machining Centers, Edge Banders, Feeders/Stackers, Panel Sizing Centers
    • Safety Speed Manufacturing
      Economical Vertical Panel Saws, Panel Routers, Edgebanders and Widebelt Sanders
    • NEMI
      Products For CNC Machines - Digitizers, Tool Setters, Vacuum Pods, Vacuum Cups, Vacuum Tables, Vacuum Chucks and Software
    • CP Adhesives
      Supplying Quality Adhesives to the Woodworking Industry
    • iBiDMachinery
      The Nation's #1 Used Woodworking Marketplace - Buy and Sell Woodworking Equipment with iBiD!
    • Impact Search and Placement
      Professional Employment Recruiting Specialists
    • SAMES North America Corporation
      Precision Spraying Solutions From Pumps To Complete Application Systems-Design and Manufacture of Process Equipment Including Airspray, Airmix, Airless, Rexson Dispense, Electrostatic and Powder Coat
    • Template Services
      Professional Moulding Design and Template Making Service
    • Vexor Custom Woodworking Tools, Inc.
      Custom and Standard Router Bits, Shaper Cutters, Profile Knives, Multi Profile Insert Tooling and More

    Become a Sponsor today!