Subject: Re: UV cure of shellac?

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

UV cure of shellac?

1/4/17       
Brian Burns  Member

Website: lessonsinlutherie.com

Hello All,

Some 50 years ago I built an ultraviolet drying cabinet for an oil violin varnish that I was making. It worked like a champ on the linseed oil based finish, but that soft coating killed the treble response of three classical guitars before I realized that I should be using the traditional hard finish, shellac.

Having spent a couple of days looking for info on UV "sun tanning" of wood to darken its color, I remembered my UV drying box. Has anyone tried using UV to speed up shellac's long cure time?

Cheers,

Brian Burns

1/4/17       #2: UV cure of shellac? ...
MichaelH

Website: http://properwoodfinishing.com

Different mechanics as with a traditional U.V. cure finish. The alcohol in the shellac makes it a fast dry, solvent release finish. Heat will help providing that you do not hit it with to much where it will skin the top over and cause you solvent pop. Any cheap automotive paint jobber can sell you a quartz heater that is adjustable to the work surface.

1/5/17       #3: UV cure of shellac? ...
RobertJ

My wife has her nails done with Shellac, and it cures under a UV light box.

Can you find one to fit a Violin????

1/5/17       #4: UV cure of shellac? ...
Brian Burns  Member

Website: lessonsinlutherie.com

Hello Michael and Robert,

Michael I do use moderate heat, and keep the air moving to speed the cure of my shellac. In my googling around I ran across a number of sites that use UV for drying shellac on fingernails, as Robert mentions, and I thought that perhaps someone had tried it on a larger scale.

According to a local expert on finishing---he studied finishing to be a museum curator---shellac takes a lot longer than most people think to cure up hard. Over a long period of years it cross links, and is no longer soluable in alcohol, and I wouldn't want to speed up that process!

Robert, received wisdom is that an oil varnish is the best finish for a fine violin, because it damps out some of the high frequency screechiness. For a plucked instrument like a guitar that's bad, hence the use of shellac, at least on the soundboard.

The best source of UV info I found was Solacure. I had a long conversation with the owner---an electric guitar enthusiast. He has a UV kit for drying oil varnish on a violin in a day instead of a week. I know that is accurate, as I did it myself back in the early 1960's.

Cheers,

Brian

http://www.solacure.com

1/5/17       #5: UV cure of shellac? ...
Rick Mosher

I worked with UV finishes and they are very popular with the guitar making community. As well as floor finishes and architectural millwork.
Most of the places I have checked out are using a polyester system. The finish is made by adding an activator to the original finish, not all finishes can be changed. You need to check that out with a supplier. I was amazed at the speed of such a system, I could do a fully filled, fully cured and buffed piece in one day!

The equipment to do the finish is pretty expensive but the results are amazing. You can buy cheaper curing lights but they are not the way to go. Google guitars and UV curing and you will see several companies using them. Write them an email I am sure they will be helpful, the Luthier forums are good as well.

Luthier Tips du Jour

1/5/17       #6: UV cure of shellac? ...
Brian Burns  Member

Website: lessonsinlutherie.com

Hello Rick,

Thanks for the response!

I make traditional Spanish classical and flamenco guitars which are particularly sensitive to the type and quantity of finish that is used on them. We nylon string (formerly gut string) guitar builders are always struggling to conserve treble response, because the nylon strings don't give us much high frequency sound power to work with.

French polished shellac will build up a nice gloss at a couple of mils thick, and most importantly, it is quite hard and low in acoustic damping. It's not very durable, though better than shellac's reputation would indicate, provided that you use de-waxed. We put up with its lack of durability in exchange for the improvement in tone quality and responsiveness of the guitar. It's readily repairable as it's 100% burn-back.

Ervin Somogyi, one of the best steel string builders alive, has his guitars French polished, and says that even steel string instruments sound better when finished with shellac.

Cheers,

Brian

1/5/17       #7: UV cure of shellac? ...
Rick Mosher

I don't build guitars so I can't tell you what is best or not. I have made it my business to never believe anything anyone says until I have tried it myself. I particularly like doing the "impossible."

I suggest giving it a try and see for yourself if it works or not. There are a lot of custom guitar makers using it and I'm sure they are all concerned about the sound as well.

This could be your chance to show Ervin Somogyi a new trick. :)

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)