Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Spraying Existing Kitchen

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Spraying Existing Kitchen

2/24/17       
Paul S.  Member

I'm bidding a job to spray coat a client's small kitchen which is now a light stain on maple raised panel doors. It's factory finished; probably with conversion varnish. In my shop I spray solvent based lacquer and haven't use waterborn finishes. My supplier says to use Chemcraft Aquaprime Basecoat 550-1600 and Fuhr 260 topcoat custom matched to the customer's selected color. I'll do the doors and drawer fronts in the shop and the faceframes and end panels on site after masking. It's a townhouse so I'll just vent the fumes. Do you think these products will give me a good result? Any other suggestions to avoid major problems? I welcome all of your help. Paul S.

2/24/17       #2: Spraying Existing Kitchen ...
RobertJ

Should not have to worry about venting with waterborne lacquers. But you do have to protect the surrounding areas from dryfall and make sure all vents (heat registers & cold air returns) are tightly sealed.

Masking is tedious and time consuming; price accordingly.

Degrease all surfaces.

Watch for drips....waterborne is notorious for runs.

2/24/17       #3: Spraying Existing Kitchen ...
nick

I do this fairly often (3 kitchens in the last 3 weeks) and I have done for this for many (lots of manys) years.
I'm not familiar with the products you mention so no comment there.
if your not familiar with the product or WBs; your customer's cabinets are the place to start...get some product and spray some scrap pieces in the shop so you can get a handle on it.
Definitely vent; there are a lot of solvents in most WB material (the stuff i sprayed this week ran between 250 to 275 grams of VOC per liter, that's 25 to 27%) use a box fan on high to pump air into the work area and one on high in the exhaust window (take the screen out or you'll be paying for a new one) it's not a bad idea to bring along some booth filter medium. Also venting gives you control over where your overspray goes.
Masking is a PITA and time consuming. I usually get a quart of something brushable since I use mostly SW products I get some Pro-classic in the color and sheen of my spray finish to paint the edge banding on euros or for the inside edge of faceframe cabs, this way your customers don't have to empty the cabs...they like that.
I usually use a Turbine HVLP set-up when spraying finishes on-site; compact so easy to transport and set-up. works well with WB's (no shearing so less micro-bubbling) provides clean warm air and a high transfer rate so less over-spray and less mess.

2/25/17       #4: Spraying Existing Kitchen ...
Nick

Whoops! that was suppose to read "NOT the place start"!

2/27/17       #6: Spraying Existing Kitchen ...
denny jahnz

I tried the aquaprime about 6 weeks ago. Couldn't get it to spray out if anything I had. Try it first.
Personally I have been using zinsser fastprime2 for a primer. Very cheap. Blocks stains and has great adhesion.

2/28/17       #7: Spraying Existing Kitchen ...
Paul S.  Member

I'm concerned with getting a good bond to the old finish. Nick, do you scuff sand to start or do you use any kind of bonding agent? Denny, what kind of equipment were you trying to spray the Aquaprime through?

2/28/17       #8: Spraying Existing Kitchen ...
Denny J

I first tried a Graco AAA with a 413 tip. Plugged immediately every time I tried to spray it. Then tried an accuspray model 10 GP with PPS and a primer tip. It would spray initially but slowly lose material flow as the screen got packed. Next used a primer gravity gun with PPS and got the same. Lastly bought a brand new Graco 390 airless and had marginal results with that. Lots of plugging of tips until I just quit.

This was after I had thinned the gallon out with maybe 16 oz of water on the advice of the rep. So the airless was rinsed out and it sat for a few weeks. Went to use it again and had failed pump packings in about 8 gallons of paint. Tore it apart and found that the same stuff in the primer that was plugging tips also plugged the upper check ball passage enough that material could barely flow through.

If you get it to spray it looks like a wonderful product but I haven't found anything that works and the rep has not been able to give me anything that helps make it better.

2/28/17       #9: Spraying Existing Kitchen ...
Nick

when I clean/degrease I use Dirtex (the hand pump bottle) Spray it on then scrub with a maroon Mirlan pad before wiping off , this way you get your cleaning and scuffing done at the same time.

2/28/17       #10: Spraying Existing Kitchen ...
Bart

After cleaning I use Zinsser Bin shellac base primer/stain blocker. Shellac sticks to just about anything and is a good barrier coat. Hit it with maroon synthetic steel wool. Then I mist coat on GF white undercoater or sanding sealer. Then a full coat and finally two top coats of GF poly clear or pigmented. You can use the rattle can for Euro cabs or face frames.

good luck

3/1/17       #11: Spraying Existing Kitchen ...
Paul S.  Member

Bart, What is your cleaning procedure?

3/2/17       #12: Spraying Existing Kitchen ...
Bart

Paul I use TSP or 409 (I don't like to use solvents as it may break down the existing finish that just opens another can of worms), the maroon synthetic, sandpaper to ease any dents (some you have to bondo) and some elbow grease. I rely on the shellac primer to seal in potential adhesion issues.Don't be afraid to squirt some of the pieces twice with the shellac primer. A light (320-400) scuff and synthetic steel wool them. The key is don't put a real wet coat directly onto the shellac.

good luck

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)