Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: 2k poly safety/ respiration etc

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

2k poly safety/ respiration etc

12/1/18       
Butch Souter

Wodering what people who use a 2 k poly such as Verde or polarion are doing for protection/ Have heard that stuff can can be sneaky bad for you/
Currently use conversion varnish mostly . Have played with the Verde a bit and do like the way it works, builds and ends up. Don't want to die using it ( or worse)
Thanks in advance

12/1/18       #2: 2k poly safety/ respiration etc ...
chris

i spray Ilva 2K urethane.
i wear tyvex coveralls, gloves and use a supplied air breathing system.
used to spray mac krystal but hated the lingering smell.

12/1/18       #3: 2k poly safety/ respiration etc ...
Leo G Member

Make sure you have good air flow. Wear clothes that won't allow overspray to get to your skin. If you don't have a supplied air system then change the filter in your respirator every day. If you have a whiskers get clean shaven so the mask works as good as possible.

Occasional spraying with 2K poly you'll have a hard time injuring yourself unless you are blatantly using unsafe spraying practices.

If 2K will be your primary system and you are in the both most days, then the Tyvek coverall and supplied air is the safest way to go.

12/1/18       #4: 2k poly safety/ respiration etc ...
Leo G Member

I'd take the odor of MLC Krystal over Polarion any day. LOL

12/2/18       #5: 2k poly safety/ respiration etc ...
CraigM

I spray a lot of 2K. I used to use an Allegro air supplied system, but switched to the 3M one with a VersaFLo mask and I like it a lot better. I also use Tyvek coveralls and nitrile chem resistant gloves.

12/3/18       #6: 2k poly safety/ respiration etc ...
Adam

The regular 3m carbon filters work for iso's. But they don't work for very long. In the safety sheet it says that you will not be aware(smell) when the filter stops working. That is why Leo mentioned changing the filters daily.

They have very good properties. I'm curious what people are spraying frequently enough to have a supplied air rig.

Interestingly the iso's are only really dangerous if you aerosol them. You can brush 2k linear poly marine paint(Awlgrip) without the full hazmat kit. That stuff is really old school and has a very high amount of iso. The paint is incredibly durable.

12/3/18       #7: 2k poly safety/ respiration etc ...
the google

we probably spray five gallons a month but use a supplied air set up. 3m mask connected to a bullard belt, hose, and pump. it is a comfortable set up, but dragging the hose around is not much fun. tyvek suit and gloves, too. beats dying, though.

i have been told that with good air circulation (fan) the iso's, provided you aren't standing downhill, get pulled away quickly enough to not be a serious health concern. i'm not sure i believe it, but our finish supplier told me this.

we spray in an automotive paint booth.

12/4/18       #8: 2k poly safety/ respiration etc ...
DannyB Member

As adam says, iso is a bit weird. It reacts *very* quickly with the moisture in air (that's why the can of catalyst doesn't survive long once opened, unless you bloxygen it or have a way to re-vacuum seal it).

It is also heavier than air.

The upshot is that, assuming a very good supply of air, your main risk due to inhalation is from bounceback/etc.

Still not worth playing around with (I would always use supplied air), mind you, but it's not like formaldehyde or other things that are still there 10 minutes later.

As also mentioned, brushing/rolling is very safe - all studies i've read show no measurable quantity reaches the breathing zone due to how fast it reacts.

I use a 3m ultimate fx full facemask with an allegro pump.
I didn't like the allegro mask as much.

3m makes a converter for the mask that twists on where the filters normally go, so you can swap between filters and supplied air really easily.

They also make a converter that does both filter and supplied air, using the filter when supplied air is not present.

12/18/18       #9: 2k poly safety/ respiration etc ...
JM

We are using a product by Alcea and they have a catalyst that is free of iso.

The catalyst we use is 9981/A699 along with Primer FB1090 and pigmented top coat 531A/MSBB

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)