Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: spray room layout

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

spray room layout

2/12/19       
frank Member

hey guys. family custom shop 46 yrs old 20 guys. we are moving for the first time...so i have a chance to redo shop flows.

we ran 2 spray rooms primed in one , fed all cabinets through it , carry them in, prime, sand outside in shop, bring back in prime again, bring out, sand again, then bring them to second spray room and top coat. i let the guys create this setup as i was so busy in other parts of the business.

what i do not like after finally looking at the process is so much handling of the cabinets, in , out etc..and they are big for the most part being custom.

in the old days when we were founded we would spray a cabinet sealer (no painting back then) sand it in place, then top coat it. no moving it in , out ie: handling multiple times.

so finally i want to for the new building go back to basics and do this:

bring in 3-6 cabinets, prime them on the horses, sand them in place, reprime, sand, then top coat. so essentially you are focusing on 3-6 cabinets for a long time ..but i'm thinking i save on handling and get them to the next department sooner than trying to spray the entire kitchen at once.

thoughts?

2/12/19       #2: spray room layout ...
mauricio poli Member

Hello !
It is very important to sand far away from the spray booth, to do not contaminate the environment.
You could use rails to move the furniture one side to another.
Good Luck

2/12/19       #3: spray room layout ...
Leo G Member

Put the cabinets on carts, not sawhorses. Handling is easy.

2/13/19       #4: spray room layout ...
Shane

I second carts.... particularly old school cotton mill carts... find them in close out auctions

2/13/19       #5: spray room layout ...
Leo G Member

I use 3 1/2" casters on a 2x4 laid sideways covered with 3/4" MDF. I have mostly 2x4 carts but one 2x3 and three 2x5 carts for bigger cabs. I believe I currently have 16 carts and at times I need a couple more.

2/13/19       #6: spray room layout ...
TomB

It's more about flow. When we added on to our finish building, I made a circular flow to our process. Cabinets come in the finish area on the south. Booth is in the NE corner, has a side door to a drying room in the center so you can keep spraying while other stuff is drying. Then out of the drying room to the shop area on the south for sanding, then back in the booth for 2nd coat (etc), drying room, then on the northwest is a final assembly area. From there it is ready to ship and gets put in the shipping area to load in the trailers. Each room can be shut off from the other rooms by large sliding doors. We put everything on carts so it's easy to move from one space to the next. One person (with backup sanding help as needed) can keep the system full all day.

2/13/19       #7: spray room layout ...
frank staltaro Member

thanks guys for the replies.

watching cabinets get primed then handled only to be brought in and out even on carts (my cabinets range from 24" to 130" in length) drives me nutz.

i will try to finish a group of cabinets in place. and see how it goes as far as quality and productivity. i will be also switching to full water based and they claim it does not attract dust like the previous solvent based material.

2/13/19       #8: spray room layout ...
Adam

You will spend more time cleaning the spray both between coats as you would rolling the cabinets in and out.

Regardless of size, once a cabinet is placed on the carts, moving them is a one man operation.

There are other good reasons for having the carts on wheels for other operations as well.

2/14/19       #9: spray room layout ...
frank Member

Adam and others;

i get the dust and contamination concern.
with a powerful fan i am expecting blowing off the cabinets in between coats to have all dust eliminated. in fact i believe blowing a sanded cabinet off in the spray room will mean a cleaner cabinet than doing it in another room of my shop and as it transports back in that it gets dirty or damaged on its way back in.

i find my people once a set of primed cabinets are carted off there is little concern to the speed of sanding these things. then the carting is a excruciating thing to watch in itself.

my belief is instead of looking at 15 primed cabinets in various levels of preparation far from done because you are attacking 15-20 cabinets at once while my hardware department guys are waiting even on one cabinet to be finished; i can have 4 cabinets that were focused on not handled 3x to be sent finished to the next department with far less lag in between shop flow. i look forward to honestly seeing how this idea works and will post.

2/14/19       #10: spray room layout ...
Leo G Member

When I'm spraying more than a couple of pieces I get to go in circles. Meaning that by the time I'm done spraying I can start over again with the first piece because it's dry enough for scuffing and the next coat of finish.

You need to find out what that timing is and that is the amount of cabinets that need to be sprayed before you start the circle again.

In your case, like mine, you build cabinets that vary in size greatly. So it might have some advantage to have a countdown clock in the sprayroom that indicates the first cabinet is dry and the circle should start over again.

That way you are spraying the minimum amount of cabinets and keeping everyone busy at the same time. Then your hardware guys will have things to do.

3/16/19       #11: spray room layout ...
Kevin

Frank.
There is a very good reason why most of the comments you are getting from professional finishers is contrary to your proposed solution. I would spend more time listening to these guys and less time convincing yourself that leaving a cabinet in one place until its finished is the way to go.
It seems to me that something your not taking into consideration is the dry time.
If you prime a set (lets call it 6) cabinets - you then have to wait for the primer to dry 30mins to an hour. Now this may be ok in your book - but in that time i could have sprayed almost 4 more sets while that first set was drying.
If you are moving to a new building and have the ability to change your layout - consider the following setup - it will give you that "one piece flow" your looking for but will not stop.


View higher quality, full size image (830 X 655)

3/16/19       #12: spray room layout ...
Kevin

I understand that the above layout is not ideal for all situations. But the concept of having the parts move through different zones with areas between to allow for flash/dry/cure should give you a different way to look at things as far as setting up your new room.

3/16/19       #13: spray room layout ...
Kevin

another thought. if your guys in the hardware department dont have anything to do because they are waiting on your bottleneck to finish the cabinets -- maybe you should cross train those guys and they can go help scuff the primer to advance the finishing department. Always attack the bottleneck.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)