Total Finishing Supplies

Professional Finishing

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Kremlin vs HVLP Finish Quality

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Kremlin vs HVLP Finish Quality

6/24/19       
Jordan Member

Looking to get some feedback on the Kremlin Airmix AAA vs conventional HVLP when it comes to finish quality. I mostly do custom pieces so I am not doing high volume. Typically spraying one piece at a time, 2-3 times a month. The price of the Kremlin is not an issue and the main goal is to get the highest quality finish I can. Question is, will I notice a difference in quality stepping up to the Kremlin? Any other methods/products I should be looking at? Currently using a DeVilbiss Tekna Pro conventional gun. Thanks all!

6/24/19       #2: Kremlin vs HVLP Finish Quality ...
Pat

The general answer is no. The main reasons for going to AAA are speed, convenience and the ability to spray with a lightweight gun at any angle (although this can be achieved with a pressure pot).

There are exceptions, I'm sure, depending on what you're spraying, your booth, etc., but a good quality conventional rig can achieve results just as good as AAA.

For the record, I use an AAA for almost everything and I love it.

Cheers,
Pat

6/24/19       #3: Kremlin vs HVLP Finish Quality ...
Jim Clark

Just for everyones info:
DeVilbiss makes a bag kit to fit most all top
cup HVLP guns where you can use a plastic
bag inside the cup which enables you to
spray upside down and never spill, also
making clean up much easier.
1 qt. Zip-Lock freezer bags works just as
good as the Devilbiss bags.

Reference
https://www.ebay.com/p/DeVilbiss-Dev-EZ-Liner-Kit-OMX70K48/1511821738

6/24/19       #4: Kremlin vs HVLP Finish Quality ...
herb johnson

for a the best finish give me a binks 7 gun or a devilbiss mbc gun

there is reason they are still being made after about 40 years

good luck
herb j

6/24/19       #5: Kremlin vs HVLP Finish Quality ...
Nick

+1 for what Herb said.

6/25/19       #6: Kremlin vs HVLP Finish Quality ...
Jordan Member

Great info, thanks all! I'm going to look into that mbc gun.

6/29/19       #7: Kremlin vs HVLP Finish Quality ...
Big Kremlin Fan

Spraying for almost fifty years now. I still have maybe five or six Banks Model 7 guns. Learned to spray with them and would sworn nothing could ever be better.

Well, guess what? I've never picked one up since the day I first pulled the trigger on my Kremlin AAA about 10 years ago. It fits the hand like a glove, an extension of your fingers and super light. Minimizes overspray by tons. Finish levels out much superior to any Binks #7 ever did. The savings in lacquer volume have paid off my Kremlins in less than one year.

Kinda drifted here, I believe the question was Kremlin vs HVLP, so not sure how Binks Model 7's came into the picture, but I figured I'd respond to that part of this thread. And I respect every person posting here - we're all family and that's big in my book! So, that's my story and I'm sticking to it!

7/1/19       #8: Kremlin vs HVLP Finish Quality ...
Robert M  Member

I'll second "Big Kremlin Fan" !!

Not been spraying for.....50yr, but, 20 ;o) !
Regardless time (past experience), in my noble opinion, no comparison as for ease & virtue of spraying with a AAA ( kremelin or CAT or....any brand for that matter !!)
Sure, gravity guns with a 3M ppm is flexible and gives a fare to excellent spray finish.
I'm one of those who stand by,,,,,,it not the equipement that make the finish, it's the who.....how YOU adjust to your equipement & material !
Sure, no debate here, AAA are best for many reasons ( 1st, the least for over spray, therefore, less bonce back in tight corners or closed space) second, spray is better by a pressure pump pushing fluid vs air pressure (gravity or siphon) .
All & all, 99% of AAA owners / users will tell ya.....stay with a gun VS AAA, unless it's a budget restriction thing !!

All the best

7/8/19       #10: Kremlin vs HVLP Finish Quality ...
Kevin

I would never use a kremlin AAA if my production goals consisted of one piece every couple months.
The ammount of cleaning and maintenence of the fluid line and seals would kill the entire concept.
I am a huge kremlin fan. But the quality youre looking for can be achieved with a $20 harbor freight gun and proper application knowledge.
Buy a pump if it makes u feel better, but a very nice spray gun and properly applied mechanics will solve your limited production rate much more suitably.
Use the proper solvents to meet the desired effect on your coatings.
Air assisted airless is a production must.
But its overkill for a couple projects a year.

7/8/19       #11: Kremlin vs HVLP Finish Quality ...
mastercabman

I agree with Kevin on this one
Pumps are great and expensive so you need to put your investment to work
So if you spray a lot and you need speed the pump is going to be your best choice
I also don't do a whole lot of spraying
I use CAT guns(PPS and pressure pot)and I get excellent results
Maybe if I get a descent size job I'll invest in a pump

7/8/19       #12: Kremlin vs HVLP Finish Quality ...
Nick

Small projects 2-3 times a month, with the quality of your finish being #1. I would mate a Binks SG2 2 quart pot, 15-20' of air/fluid line and either a Devilbiss Compact or Teckna Pro-lite pressure feed gun and a assortment of needle/nozzles. Retail new this will set you back around a $1,000.00, but last for years and years...if you keep them clean.

7/21/19       #13: Kremlin vs HVLP Finish Quality ...
Denny J

I ran AAA sprayers for nearly two decades ranging from Asturo to CAT to Merkur and I love the way they operate and spray but around 6 months ago when I switched to 2k poly my rep dropped off a Titan 655d diaphragm airless to test. It has a hopper on top which is so much nicer than the pickup tube and it is smoother than the typical piston pump airless plus you can use a 25' 1/8" hose which is actually more ergonomic than the twin hose AAA.

I actually sold both of my AAA and replaced them with the Titans and their cost is under $700 each.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)