Anyone use ML Campbell Aqualente Pigmented Lacquer? -- 0 -- 
12/10

I'm interested in anyone's experience with ML Campbell's Aqualente Pigmented Lacquer. It has a viscosity of 35 - 45 sec through a #4 Ford cup which will work well with my gravity feed HVLP conversion guns, and it is KCMA rated which should make it a good product for use on a bathroom cabinets. But I'm interested to hear anyone's opinion whose actually used it. Liked it, hated it, words of advise or caution, alternative products you liked better and why. Any alternatives have to be WB, because I'm not set up to handle solvents. Thanks.
John
12/11 #2: Anyone use ML Campbell Aqualente Pi ...

I am only set up to do waterborne also. I started with ML Campbell's Aqualente and still use it because their supplier is local.
The pigmented Lacquer has been fine, but I hate the Stain blocking primer. Once it is mixed and thinned to the proper viscosity, it does a very good job, but it is a royal pain to mix once it has set for even a very short period of time even after thinning. I have broken stir sticks trying to get the caked material off the bottom of the can. The ML Campbell reps have suggested using a drill with an attachment for mixing it, but that really causes a lot of micro bubbling.
I have used Val Spar's Zenith products. Their primer is much better for thinning and mixing. The pigmented lacquer is as good as ML Campbell's, but their supplier are not local.
I wouldn't count ML Campbell out just because of the primer until you try it though.
12/11 #3: Anyone use ML Campbell Aqualente Pi ...

Thanks Joe. That's really good to know about their primer. I'm not sure I can even buy Valspar products, although I've wished I could several times as it looks like they have several great products.
John
12/14 #4: Anyone use ML Campbell Aqualente Pi ...

I've used the pigmented (and clear) Agualente since it came out, and ML Campbell's prior WB products (Polystar/Ultrastar) before that. It's my go-to product for pigmented, way better than the old stuff. I have no problems with the primer. Yeah, it's thick, but sometimes you want that for good build/scratch filling. Durability seems pretty good, though I suspect it's probably a notch below solvent-based CV.
12/14 #5: Anyone use ML Campbell Aqualente Pi ...

THanks for the info. Pat. I just checked on the Agualente Stain Blocking Primer PIS and the viscosity is 40 - 50 sec through Ford #4 cup. That should be the sweet spot for my 1.8 mm gravity feed HVLP gun, without thinning. Or am I missing something, since I've never used it?
John
12/14 #6: Anyone use ML Campbell Aqualente Pi ...

1.8 tip should work with thinning. If not, go to a 2.0.
Cheers,
Pat
12/14 #7: Anyone use ML Campbell Aqualente Pi ...

Hi John,
I have never been able to get the viscosity to 40-50 through a Ford cup right out of the can. Your probably going to see it much higher right out of the can. You will need to thin it just to get it to 40-50.
I have had to thin all ML Campbell products to get them to the viscosity they recommend. Changing the tip helps some.
I have used CAT CPR guns with 3M's PPS. Never a gravity gun. I now use a CAT AAA pump. All required thinning to get to the correct viscosity.
12/14 #8: Anyone use ML Campbell Aqualente Pi ...

Joe,
What tip are you using on your AAA? I have the same rig and use a 309 or 311. I don't spray the primer with the AAA. I use a turbine HVLP gun with a 2.0 tip for that.
Thanks,
Pat
12/14 #9: Anyone use ML Campbell Aqualente Pi ...

Thanks Joe. They list 40 - 50 seconds at 77 F. Maybe it's been colder when you've used it, or maybe it's not really 40 - 50. I've seen that on some other products listed at 45 seconds and I measured 60+. I've been thinking about buying an air assisted HVLP gun; this might be the project that justifies buying it.
John
12/14 #10: Anyone use ML Campbell Aqualente Pi ...

I'm in southeast Virginia. I heat/cool the spray booth to 74 year round. I'm using the 409F(best) and 411F(ok). The F tip is just for waterborne and has a pre-atomizer in the tip. Helps but, I have to thin the Primer to about 45 and the pigmented/clear to 35-37 to get a good flow and to atomize better. Also have to increase the air to the tip. More waste, but works better.
12/14 #11: Anyone use ML Campbell Aqualente Pi ...

Thanks for all your help Joe. Looks like I'll probably need to get that air assisted gun I've been thinking about.
John
12/15 #12: Anyone use ML Campbell Aqualente Pi ...

I might be showing my ignorance here, but isn't a CAT CPR gun with 3M PPS a gravity system? A cup gun is a gravity gun, right?
I have that same setup, (along with the Bobcat AAA) and I'd hate to think how many people I've told the wrong info to!
12/15 #13: Anyone use ML Campbell Aqualente Pi ...

Pdub
My CPR gun is not a gravity feed. The cup is on the bottom and I use the PPS. I wish I had gone with the gravity feed, but I was steered to my set up by the local rep. It works very good, but the cup does get in the way at times.
I also use the CAT AAA with the bobcat. I rarely use the CPR anymore. Most for something that doesn't require more than on cup of finish.
12/15 #14: Anyone use ML Campbell Aqualente Pi ...

Pdub,
Gravity means the cup is on top of the gun.
The other kind is siphon feed.
Pat
12/15 #15: Anyone use ML Campbell Aqualente Pi ...

Gotcha. Didn't know they made a PPS for a "bottom cup" gun. Heck, I didn't even know they made bottom cup guns any more!
I hear you on using the AAA more than the CPR. With the AAA, I feel like it's hard to lay down a bad finish. It's just annoying when you need to spray 1 piece and have to mix up enough product to fill the hoses/ pump and then clean the whole mess out vs.
Mix 16 oz. in the PPS and throw it away!
12/16 #16: Anyone use ML Campbell Aqualente Pi ...

How much you guys paying per gallon of primer? Gallon tinted topcoat? Is it true gallon or less?
12/16 #17: Anyone use ML Campbell Aqualente Pi ...

$48 for primer, $62 for tinted. Full gallons.
12/17 #18: Anyone use ML Campbell Aqualente Pi ...

I enjoyed using pigmented Aqualente. I found the booth temp was very important. Don't shoot It cold or it will turn out poorly. I had a hard time matching mid and dark tone colors. They matched them in clear paint--which did not cover well and ended up need more coats of paint. I switched to PPGs Breakthrough. Really good product. Does not dry as fast but if sprayed right can have a nice finish. It is indoor and outdoor so would work great in a bathroom.
1/3 #19: Anyone use ML Campbell Aqualente Pi ...

Durability is "a notch" below that of real conversation vanish or catalyzed lacquer? Um, no. The difference in durability of a waterborne system to a catalyzed solvent system is light years apart. Still. After years of so-called next generation waterbornes the differences in durability haven't been bridged or even broached. It's still all hype. Scratch the waterborne with your fingernail after it's one month of full cure and see and feel for yourself.
And what about reversability? Waterborne finishes come off in a gooey mess.
Those are just two criteria to consider. But that romanticized notion of "a notch below" is fiction and wishful thinking.
1/3 #20: Anyone use ML Campbell Aqualente Pi ...

Daniel,
I tried the fingernail test. Nothing happened. What should one expect to see? As for reversability and the gooey mess, are you talking about using a chemical stripper? Or sanding? Never tried a stripper on it, but I have sanded a fully cured finish a few times with no problem.
I realize "notch" is a somewhat vague measurement, but "light years"? I've only been doing this for a dozen years, so I haven't achieved true Curmudgeon status yet. I have however used WB during all those years and have witnessed a big improvement over that time.
Solvent-based products have their own set of issues, including pot/shelf life, mil thickness limits, blushing, mixing issues, nasty, explosive fumes... I could go on if you like.
Cheers,
Pat
1/3 #21: Anyone use ML Campbell Aqualente Pi ...

I would only be talking about chemical finish removal, to sand off a finish is a destructive attack on the substrate as well as inefficient.
Mil thickness? Valspar Zenith has to be under 6 dry mils. Sherwin-Williams Kem Aqua has to be less than 5 dry mils.
There are pluses and minuses to every finish type. As finishers we have to prioritize those pluses and minuses, and that means first recignizing them and acknowledging them for what they are.
Yes, if you're talking about durability and holdout, light years isn't the hyperbole that it sounds like to you.
Your cost-benefit analysis of what you do is your mileage. And even if there is an appreciable consensus of finishers who share your same good experiences with coalescing finish systems there are still plenty of folks and factories who have studied them, weighed them for all their worth, and still elect to use solvent systems. The overwhelming majority of furniture manufacturers have yet to switch, both those few who remain in America, and those many who now manufacture overseas.
2/3 #22: Anyone use ML Campbell Aqualente Pi ...

A suggestion for mixing the primer with heavy solids.
We purchased a HarborFreight air-driven paint mixer (about $130).
We use this for MLCampbell's MagnaClaw Primer. This product also has a lot of solids that we could never completely mix with a stir stick. We shake the gallon cans for about 5 minutes, then turn the can over and shake for another 5 minutes. (Yes, we know the container sits in the shaker sideways. It may be overkill, but it keeps the boss happy!) When we check the bottom of the gallon there are no solids on the bottom.
We also use this when we add flow enhancer to our topcoat when needed. The topcoat gallon only contains about 120 ounces (that leaves room for our distributor to add color tint) so there is some room to add the flow enhancer. Again we shake the container for about 10 minutes.
Why 10 minutes? That was a quick bit of trial and error. We guessed at 10, found that the results were great, and left it at that. While the gallon is shaking, we are doing something else anyway. Besides, we were probably spending that time anyway with the stir stick, but not getting good results. Now the product is mixed very well with a consistent method.
0 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|