spray booth -- 1 -- 
2/7

i use a 27x13x10 shop built ( not a bought auto booth) spray booth with a Chicago AVS 122 1450 rpm exhaust fan for my woodwork spraying. I have added a make up air unit how does this change the fpm pull and requirements of the exhaust fan? Can some one explain this please. I have horrible turbulence and overspray landing all the way back on the floor to the make up intake. Airflows down both walls with reverse flow in the centre off the booth
Jeff
2/7 #2: spray booth ...

We'll need some numbers of air flow and size of make up unit to be accurate. Also no idea where the make up unit is located, and if you have internal ducting in the booth to get the exhaust drawing off the floor or just the end of the booth. It sure sounds like you don't have enough inlet to match your exhaust fan.If you have 3 phase on the exhaust fan, you can add a VFD to get variable speed and tune accordingly.
2/7 #3: spray booth ...

Thanks Ric. The MUA is used so can't read any markings other than it is a ICG 208v single phase. I have the MAU entering the wall on one side of the both at chest level into 20x20 internal ducting that came with multiple register type vents. i have done hours of blocking off restricting partial and have now gone to plugging all and cutting a 20x20 on the right and 20x20 on the left. Exhaust is on the opposite wall of the booth boxed into a 6'x3'x20" filter box chest level.i was told variable speeds on these were not doable . Sorry don't have any other info.
2/8 #4: spray booth ...

Open some doors. You need more air, plain and simple. What is your 1450rpm fan rated for cubic feet per min? To stop the turbulence (negative pressure) you need more available air than outgoing. Gentle is good.
good luck
2/8 #5: spray booth ...

thanks for your reply. I have a H-Vac guy coming to check it out hopefully soon.
2/8 #6: spray booth ...

If the airflow is going through the 10x13 area you need a 13,000 CFM fan.
If the airflow is going through the 27x13 area you need a fan that can move 27,000 CFM.
Either way, both are big fans. I have a 18x9 area I'm moving air through and have 17,000 CFM.
2/8 #7: spray booth ...

Hi Leo Happy New Year to ya. I believe the exhaust is maxed out at 3300cfm and the MUA is at 2500 max i have pulleyed up and down and back and forth to get were it is now . I have heard more than once that over spray is going to happen nothing you can do>> I can't except that .. I spray 5-6 feet away from my exhaust filter bank in what looks like a open booth and the over spray is still getting pulled back over the whole booth????
2/8 #8: spray booth ...

on line Virtual Air Flow Calculator..CSG Net work.com. So 3510 cubic feet x 45 air exchanges per hour=every 1.3 min. shows 2632 cfm fan required? i think i have the fpm figure of 10x13x100=13,000 but it still list a 3500cfm fan??
2/8 #9: spray booth ...

100 feet per minute will keep the overspray to a minimum. Some of the corners will have turbulence in them, just the nature of the beast.
2/9 #10: spray booth ...

Velocity of the air is what is killing you. You don't have to spray in a wind tunnel. "If" you had an open back you would empty your booth roughly every minute. You're essentially trying to suck 3000cf of air through 5.5sqft of opening (130sqft back wall if I figure right). That won't ever work. You'll also have to consider your exhaust ducting. Is it impeded or is it a straight shot. If impeded that can create back pressure as well. Expand your intake and spray closer to your exhaust filters. I use the 20x20x2.5 fiberglass filters which grab a lot of the overspray before it has time to bounce. If the overspray is not bouncing violently off the walls it will fall harmlessly to the floor.
good luck
2/9 #11: spray booth ...

PS, If you really want to get into it (I built surfboard sanding rooms in another life) you can get a smoke tester or improvise one to check airflow. A nice even/gentle flow in the right direction is what you want.
I'm done :-0
2/9 #12: spray booth ...

Thanks Bart i will make the exhaust bank bigger it is the cheapest thing to try .
2/10 #13: spray booth ...

What Leo is saying is the correct design for an open face spray booth. You want 100 cfm per square foot of the opening size to your booth. What diameter is the fan on your exhaust air from your booth? A 24 inch diameter fan is approximately 7000 cfm depending on how fast you have it running. Your Air Makeup has to have larger cfm than your exhaust fan, so for this example you would need a 7500 cfm makeup air.
You want your booth to be in a slight positive pressure. According to the numbers you are using your makeup air unit is to small for your exhaust fan.
2/10 #14: spray booth ...

Thanks Scott and yes in the perfect world positive pressure would be great but this unit came as a set and used so it was still more than i could afford but the seller got it installed for me and now i'm trying to tune it. I will try and send a video of what is happening . I like the air flow that is moving over the door racks it is a excellent drier just seems the air flow is all intake then when it gets to within 8 feet of the exhaust it just runs out and the exhaust does not take over and grab it to pull it out. I spray right in front of the filters about 5-6 feet away and have built a roof and tapered walls to simulate a open booth in order to help the exhaust grab the flow and keep it moving out.
2/10 #15: spray booth ...

I spent all day yesterday just baffling the MUA to give me what is now on the video hope you can see it.I will build the exhaust bank bigger today. Then i will do a black spray test with new white sheets to see what the overspray is doing.
View higher quality, full size image (3264 X 2448)
2/10 #16: spray booth ...

Looks like a nice set up. Off the top I'd say some of your intake air is bouncing off the angled walls and swirling a bit. Personally I would extend the fiberglass filters to the floor and to the sides of the exhaust to catch more of the overspray. Mine go floor to ceiling. You'd be surprised how much gets collected. You could put 1/2"x 2" ribs 20" on ctr and staple filters to the walls inside the angled wall in your booth.
cheers
2/10 #17: spray booth ...

So you can see the video. Shows not available on my screen ? Yes i do love my job but having a more productive booth would make my life a lot easier. I will make the filter area the full size of the wall and the H-Vac guy is coming out today to get real time cfm.....then discuss options. really want to keep that airflow over the the dry racks-fingers crossed.
2/11 #18: spray booth ...

buy yourself a dwyer vaneometer. very cheap about$35 measures air speed. very useful.
2/11 #19: spray booth ...

Thanks Chris i do have a gauge that i have used plus a light piece of thread taped to the end of a stir stick. These are showing me my turbulence i just don't know how to tune it? I have a good demo on video that i have it tuned to now but can't figure out how to get it posted.
2/12 #20: spray booth ...

Jeff - if you can send the video file to us or let me know where the file is located, we can try to put it up for you. If it is on You Tube, for example, I can easily put it up here.
The Staff at WOODWEB
2/12 #21: spray booth ...

sent..fingers crossed
2/12 #22: spray booth ...

Here's the video -
If you are seeing this message, your version of flash needs to be upgraded to view this video. Click here to get the latest version of the Flash player. |
2/14 #23: spray booth ...

Thank you Woodweb Staff that was a lot of work to get it to work...what a great bunch of awesome people to be apart of .
Jeff
PS. Did a spray test with the setup as is and have some overspray going down half way along the non dry rack wall. Almost there.
2/14 #24: spray booth ...

in the photo it shows your table with ducting under it. Is this hooked up to an exhaust fan also?
might be better with a simple stand and the exhaust filters all the way to the ground.
2/14 #25: spray booth ...

Chris the metal duct is the MUA unit the table is there to hold the quart cans on white paper to show overspray . This baffling on the MUA gives me flow down the wall and also down the centre of the booth up until the edge of my spray test sheet. the air flow at the table on the string shows 2.2mph- then the middle shows 1.2 and then at the entrance door and beginning of exhaust goes to.2mph. The MUA comes into the wall towards the left of the duct at the 20x20 square then deflects left and right. The top ducts and bottom is what gave me air flow down the centre of the booth.. which was completely reversed going right back to the MUA unit with out them.
2/14 #26: spray booth ...

Sorry Chris thought you were responding to the video. The table is hooked up to a 4000cfm dust collector . I use this as a down draft table to catch any bounce back to the under side of the doors..works perfect. Yes i will take the exhaust filters to the floor.Had a chat with the H-Vac guy and will upgrade to a 6000-8000 cfm exhaust fan with a adjustable speed... wow what a journey to fix what seems as easy as Air In Air Out !!!
2/14 #27: spray booth ...

your table with the dust collector doesn't sound too safe to me.
I would do something with your lights too.
Get hold of NFPA code 33.
will give you guidance on spray booth set up and safety requirements for lighting and fire safety.
2/14 #28: spray booth ...

The table if filtered at multiple places and shows no dust what so ever at the blades at 15 feet away or the plumbing. It was a attempt on grabbing over spray which will not be a issue with a new exhaust fan set up...so i hope
2/14 #29: spray booth ...

Wow that is a loud environment. Not sure what your ducting options are but I would look into a belt driven variable speed fan (30-36" w/sealed explosion proof motor ). Move lots (8-12Kcfm) of air quietly. After watching the video I still think you have a static-negative pressure situation ie..you need more air.
good luck
2/14 #30: spray booth ...

It sounds a lot louder on the video than real time. I spray with a full fresh air Sata hood setup so all i hear is the hiss of the fresh air.
2/14 #31: spray booth ...

determine what size you exhaust filter bank will be. multiply this by 100. This will be the cfm needed for your exhaust.
your air make up needs to be about 10% more.
100 CFM is the required air speed for a booth across face of booth.
2/14 #32: spray booth ...

My new filter bank will be 6'x6' x100= 3600 exhaust H-Vac figures with filters and piping i'm at 2800-2900ish. Filter bank right now is 6'x3'x100=1800..?I wish it was that easy. I do welcome the reply i'll be damned if this booth isn't going to get fixed!!
1 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|