Fighting the vacuum bag -- 0 -- 
9/28

I would like some ideas on how you guys deal with loading vacuum bags. In this case I'm loading as many small panels as possible. I've tried ropes down from above with spring clamps holding the 2 ends open, but still fighting trying to get things in. Mine is capable of holding a 4x8 sheet. One day I'll be found suffocated inside the thing! Thanks for your ideas.
9/28 #2: Fighting the vacuum bag ...

You climb in after your parts. Going in head first and trying to drag the parts in behind you is asking for trouble.
9/28 #3: Fighting the vacuum bag ...

I like to have a thin sheet of something already in the bag before loading the actual parts. I then just prop the front open with a couple of sticks, to get started, especially when working alone. But I also have a short length of 1.5" pvc in there to act as a roller, which takes care of the bottom corners snagging. It will have made it's way toward the open end by the time the parts are in, so easy to retrieve then.
9/28 #4: Fighting the vacuum bag ...

Keith, do you push the pvc ahead of the work; with the work,as you load, there by not snagging the corners? Good advice.
9/28 #5: Fighting the vacuum bag ...

No, I place it back about one foot back from the front edge, then as it rolls along, it is holding that front end up, so there is no weight on the bottom digging in. A little tugg on each side takes care of the top , like slipping in under the covers when you go to bed.
By the time you advance 8', it will end up about 3' from the back end, where it is easy to retrieve.
9/28 #6: Fighting the vacuum bag ...

If you do enough large parts, you might consider acquiring a flip-top press.
I found myself laminating a number of workpieces that were 6-8' long and 24-30" wide. I now have a 5'x10' flip-top table. No need to "climb into the bag" to arrange anything.
9/29 #7: Fighting the vacuum bag ...

Yes Charles, that would be nice, but with the space I have in the shop vs the no. of times I use it, not worth changing. I'm geared up shop wise for maybe 2 or 3 jobs at once and too many machines. A drop down table with flip press may be the answer 1 day. Need to find the wall space.
Did consider the flip press when I purchased the system, not sure what happened back then. I had a bigger shop at that time though.
Today I loaded 8 cabinet panels sitting them on 2 different plywood pcs, like loading a pizza oven, went OK. I cover with mesh material over non stick fabric, so keeping all that neat is the trick.
9/30 #8: Fighting the vacuum bag ...

Without knowing what your parts are or how they relate, I will offer two suggestions.
1. Run two bags off one pump with a valve manifold to isolate the bags while loading/unloading. This can reduce the number of individual parts per load. An extra bag and a couple of valves are not too expensive if you are in production. You can use smaller setups if pressed for space.
2. Gang together related parts with their veneer skins and handle them as units. If you have a drawer bank, for instance, lay the blanks up together with door bumpers for spacers with a common veneer top and bottom sheet, and cut apart with a knife after pressing. In this way you can lay up multiple parts on a common "cookie sheet" with a common top platen. If you are using pva glue and two bags, you can maintain a reasonable flow, cutting and seaming while parts are in the presses.
Your process using fabric and breather mesh seems overly complicated for flat panels. I have used similar materials for sharp curves, but for flat work we usually use 1/4" melamine coated particleboard for platens. Air evacuation is achieved by a grooved MCP platen inside the bag underneath the MCP "cookie sheets" that parts are loaded in on. Multiple parts can be problematic as the bag tries to shift things around during suckdown, but consolidation of parts using spacers and common platens works best for me.
All that said, life has been easier since we went to frame presses.
9/30 #9: Fighting the vacuum bag ...

Kevin,I'm guessing you round over the platen sheets to protect the bag from puncture? Or maybe just soften the corners? This seems necessary.
10/1 #10: Fighting the vacuum bag ...

Yes, we break the edges and soften the corners of the cover sheets, as well as laying a sheet of poly over all to keep glue squeezeout off the membrane.
10/2 #11: Fighting the vacuum bag ...

Get a 4 x 8 x 1/4" sheet of melamine. This will sit on top of your platen inside the bag. It can slide in and out. Pull it almost all of the way out, resting on sawhorses, to load a bunch of small panels. Then slide the whole shooting match into the bag. No sticks required. We ran our vacuum press this way for many years and it works great. It's easy to keep the 1/4" sheet clean, and you can throw it away if it gets glue on it. Also, always press your pieces face down, so that the substrate acts as a platen.
Good Luck,
Paul Downs
10/2 #12: Fighting the vacuum bag ...

All good information. Nothing like a good forum to toss and receive ideas. Thanks
0 -- 
Buy & Sell Exchanges | Forums | Galleries | Other Resources | Site Map
Buy and Sell Exchanges
Job Opportunities and Services Exchange
Employment opportunities and services within the woodworking industry
Lumber Exchange
A worldwide buy/sell exchange for lumber and wood products
Machinery Exchange
A worldwide buyer and seller exchange for woodworking machinery and equipment.
Classified Ad Exchange
Classified advertising for the woodworking industry (for advertisements that do not include machinery, lumber products and employment listings)
Forums
Adhesives Forum
Discussing topics related to adhesives within the woodworking industry
Architectural Woodworking Forum
Discussing quality standards and production of architectural wood products
Business and Management Forum
A forum for the discussion of business topics: from sales and marketing to dealing with difficult customers.
Cabinet and Millwork Installation Forum
Discussing all aspects of installation issues encountered by cabinet and millwork installers.
Cabinetmaking Forum
Discussing 32mm and face frame cabinet construction including fabrication, casegoods design, and installation.
CAD Forum
Shedding light on the all-too-often shadowy world of CAD.
CNC Forum
Discussing CNC (computer numerically controlled) woodworking equipment, software, and automated product manufacturing.
Dust Collection, Safety and Plant Operation Forum
Discussing topics related to maintaining a safe and productive working environment.
Professional Finishing Forum
Finishing issues for the production environment
Forestry Forum
The science and art of forest cultivation and timber management, planting, surveying, tree diseases, silviculture and timber harvesting
Professional Furniture Making Forum
Helping professional furniture makers improve quality, save time, and increase profits
Laminating and Solid Surfacing Forum
Issues related to laminating and solid surface materials and processes
Commercial Kiln Drying Forum
Discussions covering issues faced be commercial drying operations that process at least 750,000 bd. ft. of lumber per year
Sawing and Drying Forum
Discussing topics related to primary processing and drying of lumber
Solid Wood Machining Forum
Discussing topics related to the machining of solid wood
Value Added Wood Products Forum
Learn how to improve your output, find new markets, and boost sales of your lumber products
Veneer Forum
Discussing topics related to veneer processing, manufacturing, and fabrication
WOODnetWORK
An electronic discussion group for woodworkers throughout the world
Galleries
Project Gallery
Where professional woodworkers can post examples of their work
Sawmill Gallery
Professional primary processing companies display and describe their sawmill facilities
Shop Gallery
Professional woodworkers display and describe their shop facilities, products and equipment
Shopbuilt Equipment Gallery
Professional woodworker's jigs, rigs, and shopbuilt equipment
Other Resources
Industry News
Late-breaking news from all sectors of the wood industry
Video Library
Index of industrial woodworking related digital videos on the web
Auctions, Sales and Special Offers
Advertisers offering woodworkers discounted prices on good and services, and announcements of upcoming auctions
FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)
WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
A valid email return address must be included with each message.
Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
Subject lines may be edited for length and clarity.
"Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
(return to top).
Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.
You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.
WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.
Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).
Libel: Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.
Improper Decorum: Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).
Advertising: The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).
Repeated Forum Abuse:
Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.
There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).
The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)
Forum Posting Form Guidelines
|
Your Name
|
The name you enter in this field will be the name that appears with your post or response (return to form).
|
Your Website
|
Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
|
E-Mail Address
|
Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
|
Subject
|
Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
|
Thread Related Link and Image Guidelines
|
Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
|
Thread Related File Uploads
|
Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .FLV .MP4 (Image Upload Tips) If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
|
|
|
|