Sawing and Drying

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject:

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Converting my LT15 from gas to Electric

8/11/16       
Keith Newton

I've been reading in the knowledge base about the HP difference, but have to wonder about the RPMs.
My Kohler gas engine looks to run at 3500 rpms. I can pick up a 10 hp 3ph 1750 rpm with aluminum TEFC housing very cheap.
I have 600 amp 3 ph service at my shop, so having the power supply isn't an issue.

What I'm wondering is will that lower rpm be an issue, or does the drop in rpms while sawing with the gas engine get on down close to that, or do I need to plan on getting a 3500 electric to keep my blade speed up.

I can't go any larger with my motor drive pulley, due to the housing, and I don't know if they make another stepped pulley where the band is on a larger diameter, while the drive belt would be on a smaller diameter?

I can't seem to find the RPM'S for the electric motors on the Woodmizer site.
Are any of you running on electricity, and what RPM's does your motor run at?

8/11/16       #3: Converting my LT15 from gas to Elec ...
Bob Hardin Member

If you can't change the pulleys, I think you need to get a 3600 rpm motor. I don't see how running your saw at half speed will work. What is the hp of your Kohler motor now? Bob

http://hardinsindustries.com

8/11/16       #4: Converting my LT15 from gas to Elec ...
Keith Newton

Thanks Bob, My Kohler is 13 hp, with a 5" pulley.
I called Woodmizer this morning to ask what the rpms is on the 10 hp electric that they show on their site. And even though he was in parts department, it didn't show in his computer, so he couldn't tell me anything, even how much it weighed.

I did go ahead and picked up the motor this morning, with the understanding that I could return it if I can't make it work. Now that I have it to measure, I can see how it can be mounted closer toward the drive side, since it is narrower than the gas engine, which will allow me to use at least an 8" pulley on the motor, without making any modification to the housing.

And if I chose to cut the little housing cap part off above the drive belt, then fabricate a taller one, I could go on up to a 10" to get the same fpm to the blade.

I'd still like to hear from anyone using an electric motor what theirs is. Or even anyone running gas or diesel with a tachometer, what are your rpms when under load. I don't have a tac, but just go by ear to determine feed rate, striving to make a decent size chip, without overloading the motor, so I know my gas engine isn't running at full rpms, but I don't know how much lower.

8/11/16       #5: Converting my LT15 from gas to Elec ...
P-O Member

I have some experience as maybe can help. In my log band saw the cutting speed is 28 meter per sec. It is a common speed for a lot of wood cotting tools. I have also used a log band saw with about the half speed, 16 m/sec. I think it works very good. You can expect a little slower feed but your blades will keep its sharpenes much longer.
The blade will cut a coarser saw dust and will stay fresh longer. I think you would try your electrical motor with a minimum of changes in your saw.
Good luck.

8/11/16       #6: Converting my LT15 from gas to Elec ...
Keith Newton

Thanks for the feedback P-O, I like the sound of that. I just took a closer look at it again, and I'm sure I can get an 8" motor pulley in there without changing the saw.
This would get me 2/3 of the desired or higher blade speed, while delivering more foot-pounds of power to the blade.

The new motor already has a 5" pulley on it, which is the same as the Koehler, so I can give it a try without even buying a new belt.

8/11/16       #7: Converting my LT15 from gas to Elec ...
Bob Hardin Member

After you do this Keith, I hope you publish the results comparing the gas to the electric power wise. I have developed large single phase motors to replace gas engines. I would like to hear about real world experience. Bob

http://hardinsindustries.com

8/12/16       #8: Converting my LT15 from gas to Elec ...
P-O Member

I want to add that I had a log band saw, years ago, with a two cyl Koeler, 19 Hp motor. The saw I have today has a 7,5 kW electric 3-phase motor. The saws are of the same size and the blade/cutting speed is nearly the same. I can say that the saw I have today, performs better. I have read that the manufactures of bigger log saws, reccomends to dubble the horse power, if you would go from electric to diesel motor. To change from a gasolin engine to an electric motor with 50% lower hp you would still have better performance.
In my oppinion the electic motor has a much better "answer" for load variations. Its torq character is better for log sawing.

8/12/16       #9: Converting my LT15 from gas to Elec ...
Bob Hardin Member

Thank you PO for that information. 7.5 KW is about 10 HP. The advise I usually give is that if you are going from gas to electric is that you can reduce the size by about 50 percent. If anyone else wants to chime in,feel free to. Bob

http://hardinsindustries.com

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)