Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Straight lining

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Straight lining

10/30/14       
Dave Member

Has anyone had success straight lining with a table saw and material feeder. Right now we have to send out all of our material to be straight lined and am looking for a reasonable alternative besides a dedicated straight line rip saw.

10/30/14       #2: Straight lining ...
Brian T

Without the upper and lower rollers it will not work. I tried it years ago with a 4 roll feeder and double wide wheels on a table saw with no good results.

Your lumber supplier doesn't offer straight lining s4s or s3s.

A good jointer is typically a lot more affordable and space saving then a SLR.

10/30/14       #3: Straight lining ...
Geoff

A possible solution would be to use a shaper, off set fence, straight cutter and a power feed. I don't have a SLR saw and this is how I do it if I have a lot of bowed wood. Basically it is a sideways joiner with a power feed.

10/31/14       #4: Straight lining ...
Mark Elliott Member

Dave,

Before I got a SLR I used to straight line on my slider.

With a 10' slider you could get a glue line quality cut right off of the saw.

If you don't have one, it's another reason to help build a case to get one.

Mark

11/1/14       #5: Straight lining ...
Todd Scholl

We use our vertical panel saw.

11/2/14       #6: Straight lining ...
dustin orth

Website: http://customwoodmontrose.com

Make yourself a plywood T with the overall length the material you want to straightline. The T should be an even dimension so you can set you fence at ripped dimension plus jig width, the up or vertical piece is the stabilizer so the plywood doesn't sag. This actually creates an inverted T. The one that we had was 12' long and was replaced with a SLR. To use this set the board with the points against the jig and holding the jig, then proceed forward into the saw. This means you have to set the fence every time you need to cut a different width, bummer.
Another method would be a long plywood sled with a miter slot and a piece at the front the you bump into. I put some screws into the head piece to help hold the cut material from moving around. This method works well for material 8' or less unless you end join plywood or use some other material for the sled. Benefits of this way is you set your board onto the sled, line it up with the edge of the jig which is the blade cut line, hold the board down and cut the edge. I used this method for a while and liked this way better than the inverted T but the jig is quite large and requires your out feed table to have a miter slot the entire length and some sort of support going into the saw as well. Wish I had a video link for this but don't remember ever seeing one. Dustin

11/2/14       #7: Straight lining ...
Rob

Many years ago I made a sled to straight-line on my shaper, the guide groove in it was much longer than my unisaw. I took two 8 ft pieces of plywood a bit wider than the widest piece I needed to machine and joined them for a 16' sled. I attached a strip to engage the guide groove on the bottom, this is your reference so it has to be carefully aligned. The inside edge was trimmed so it would be right off the cutter to give a quick visual reference of stock removal. I then laminated a 36 grit strip of the floor sanding paper you can buy from rental centers. With the help of roller stands for support the board was placed on top and then fed into a Power feeder the sandpaper prevented the piece from moving resulting in a dead straight cut. I also climbed cut to prevent tearout. Slow but perfect results and easy to make. I don't know why this wouldn't work on a table saw, particularly if it has a large table.

11/3/14       #8: Straight lining ...
DAClark Member

Straight-lining is not the first consideration when parting-out random stock, and in many cases, it is not even necessary. A lot of good wood can be lost in the process.
I want to know what I am building first. If it is a set of frame and panel cabinet doors, I know I will need (x) stiles of a common length, and an equal number of rails of custom length, and a certain bd.ft. of material for the panels. I know my numbers.
As I cut to rough dimension for length, this is when I begin the selection process. I weed out the defects. I match colors and grains, choose cup up or down, and cutting a trim length and width of the chosen parts, loosely placing them on the bench or a pallet in juxtapositional order of assembly.
Once the parts are roughed out, stresses in the wood are relieved, and I begin the machining processes by passing the stiles and rails through the door pattern on the shaper. Each pass is a joining action, my part is straight. I use the shaper to cut a glue-line on the panel assemblies, another joining action.
With the straight-line as the first part of the process, many times the parts cannot be flip-flopped for the best selection. Know what you are cutting!! This process also produces a minimum of cut scrape if you're paying attention.
And think about it...if you cut 2" off any length of 8-12" wide board, what happens to your straight-line then? As I have learned, straight-lining a whole bunk of wood at once is busy work for factory workers, not woodworkers.

11/4/14       #10: Straight lining ...
Rob

"As I have learned, straight-lining a whole bunk of wood at once is busy work for factory workers, not woodworkers."

As this is a professional website, I think most here understand the difference between the need to straight-line a "bunk" of lumber for molding or shaping a run of random long lengths and getting out a cut list for a piece of furniture or millwork.

I mean no offense, but the lecture is unnecessary, not to mention off subject for this gentleman's post.

11/5/14       #11: Straight lining ...
doug mclaren  Member

i have used many methods but what works best for me is an eight foot long fence clamped both front and rear and a powerfeeder. cutting with bow away from fence/blade. i do also keep a 12 foot straight edge for occasional skill saw cuts when required. i m mainly ripping for mouldings or beams .

11/9/14       #12: Straight lining ...
chip geraghty

Website: http://chip-withthegrain.com

I own a helical head jointer and straight line (when needed) long lengths up to 16 ft with an auxiliary sled (a straight piece of poplar), which i wax with paste wax to reduce friction. Its quicker and more accurate than the (dangerous) jointer method. Simply set your feeder as you would to rip, and let the board overhang what you want trimmed...done safely in one pass.

12/7/14       #13: Straight lining ...
Larry

Not a current solution for Dave, But, 9 years ago I finally bit the bullet & bought a straight line rip. What a huge time saver it has been. I had no idea what it would do for me until I had one. With the correct blade, I get a great quality edge for direct gluing. One pass no matter how much needs to be removed. The laser shows me exactly where the blade will be cutting. Normal feed speed is 99'/min. My saw only has 15hp so I have to slow the feed a bit for 8/4. I have an Extrema and haven't had any problems. I'd never go back to not having one.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)