Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Rejuvinating Molder feed rollers

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Rejuvinating Molder feed rollers

6/12/16       
Ron Member

Has anyone used wd-40 to rejuvenate slipping feed rollers on a delta 4 roll feeder ? I would think the question is perminant to any feed roller ? Mine are slipping, and I've cleaned them / slightly sanded them, but they still slip. I've read wd-40 will help. This particular feeder is several years old but hasn't gotten a lot of use. Any suggestions here? It has the original delta model 36-839 wheels.

6/12/16       #3: Rejuvinating Molder feed rollers ...
JeffD

Sounds like the kind of tip you'd get on April 1st, "spray some oil on those wheels and they'll grip great!"

So no, I would never spray oil on my feeder wheels.....ever! If you want to get them gripping a little better for the short term, use a little solvent on a rag and wipe them down well. Then hit them with the coarsest sandpaper you have on hand, 60 or 80 grit work fairly well. Then repeat as often as needed.....which will be far too often.

The real solution is to replace them with Poly wheels from a company like Western Roller. Then you can get back to work and worry about something else as they'll go many, many, many years with no worry.

good luck,
JeffD

6/13/16       #4: Rejuvinating Molder feed rollers ...
Bruce H

Replacing them would be the best option. In the short term spray on some contact cement, let dry and then use. It will last a while, do it again if necessary.

6/14/16       #5: Rejuvinating Molder feed rollers ...
gary

We sand them on the edge sander with like new results. You can easily see the glaze come off and immediately feel the difference. It takes more than a slight sanding to rejuvenate them but don't get carried away.

As a bonus it also cleans the sander belts.

6/14/16       #6: Rejuvinating Molder feed rollers ...
Ron Member

gary, how in the world do you sand the rolles on the edge sander without flat spots and keeping them the same diameter... i would like to know that trick. And thanks for the response..

6/14/16       #7: Rejuvinating Molder feed rollers ...
gary

A light touch and a close eye. We have We have 80 grit on the sander and it seems to work well.

I am careful of my fingers and start by slowly rotating the wheel as I very lightly touch it to the belt. Rotate as far as I can, pull away regrip and repeat untill I am all the way around. May sound questionable but it has worked for me for years. So little material is removed that becoming out of round has never been an issue.

I suppose one could make a simple jig with an axle to mount the wheel to as it is rotated it into the belt.

6/14/16       #8: Rejuvinating Molder feed rollers ...
gary

In my first response I mentioned it takes more than a slight sanding. By hand or orbital sanding it does take more than a slight sanding. With the edgesander it only takes a light sanding to get the job done.

One time I did replaced rollers with poly wheels and they do work but it is so fast and easy to edgesand them that is what I do now.

6/14/16       #9: Rejuvinating Molder feed rollers ...
Chuck Rankin

Hi Ron:

Jeff D has recommended a good option. The system he mentions uses a reusable aluminum hub and replaceable tires that are available in a range of hardness durometers.

Here is a page from our website with additional information. This is something I've sold for over 30 years.

best regards,

Chuck Rankin
Wood Tech Enterprises, Inc.
Our website: www.woodtechtooling.com
P.O. Box 2226
Fairview, NC 28730 USA

1-800-TOOLING (866-5464)
Phone: 828-628-4414
Fax: 828-628-4490


View larger image

Stock Feeder Hubs & Tires

6/14/16       #10: Rejuvinating Molder feed rollers ...
Ron Member

I dont have time to order new ones at the moment, so i tried the 80 grit paper. That roughed them up pretty good, and they worked like new.. not sure if i trust myself using the edge sander on them. Im pretty sure i would get flat spots
. But it certainly is an option i may try at some point..maybe when i do order new rollers andi dont have anything to lose.
Thanks again everyone...im back in production mode.

6/15/16       #11: Rejuvinating Molder feed rollers ...
Dr. David Rankin

A few things to consider:

1. Make sure the rollers are the same diameter . If not, then replacing is needed.

2. The use of rubbing alcohol or paint thinner will help the grip of the rollers as it cleans the fine residue from the surface.

3. Oils will increase the the slipping on the work piece.

4. If the roller is missing areas, then replace to prevent possible kickback.

Be Safe,

Dr. David Rankin

6/19/16       #12: Rejuvinating Molder feed rollers ...
Dan / drbwoodworks

We have tried everything over the years , now we just buy new ones from Western roller . The green polyurethane ones work the best for us. Even over time they don't get glazed like the ones that come on the feeder. Actually I just picked up another feeder yesterday off Craig's list , the machine was never used but sat for six years, and the wheels are hard , shiny and slippery. So I will be ordering new ones this week from western.

9/12/16       #13: Rejuvinating Molder feed rollers ...
Jay White

Have you ever heard of fedron. It is a rubber rejuvenater. I first used it when I worked for a copier company in the 80's. Its very strong. All you do is put some on a rag push it agianst the roller and run the feed. Will soften those wheels quick. Just don't spill any on a plastic surface. Will eat it up. Good luck

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)