Solid Wood Machining

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Panel glue up options

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Panel glue up options

7/4/20       
Nate Member

My low volume production of table legs involves 2 glue-ups to get to a solid block to CNC: a panel glue up, then facing the glued panels and face-gluing. One man shop.
My current process is: mitre saw to length, plane for (relative) flatness, table saw to width (no feeder), jointer for square edges for panel glue up, edge glue & dry, then plane again for flat glue prep, then flat glue.
This is inefficient and takes a long time to the point where glue ups are not feeding the CNC enough and its sitting idle.
I need to increase the glue up speeds, and I'm looking to spend some money on equipment to speed up operation. I dont want to over-invest and go for 4-sided planer, Straight line rip saw right out of the gate, is there an in-between to up my production from what I have without spending in those huge machines? I was thinking to do a 2 sided planer and sliding table saw as a start. Thoughts?

7/4/20       #2: Panel glue up options ...
Leo G Member

Cut to length, edge joint your stock, rip to width, glue up, use the CNC to flatten and shape your stock.

7/5/20       #3: Panel glue up options ...
RichardP

More info from you would get some help from others.
You have a cnc?
What size is the panel you are making?
What does the leg look like?
How many do you make a month or week or year?

7/5/20       #4: Panel glue up options ...
Dustin Orth

Are you mechanically inclined? If so, look at the auction market for a moulder. Smaller one would do you fine. A straight line rip can also be had, both used big ones or some of the smaller imports. Whats your budget? Do you have power? Whats your dust collection set up? Do you plan on expanding at all? Can you out source these glue ups to a bigger shop? Is it possible to outsource and order, say 10 sets and stock them? Is it worth spending a bunch of money on equipment or paying someone else to do it for you, then you spend the time building your client base while your CNC is cutting legs? Just some questions for you to think about.

7/6/20       #5: Panel glue up options ...
Tom Gardiner

Consider buying your stock D4S. I get some material S2S for the price of $80/lin ft. I can also have straightlined for about the same. It's a big time saver.
I keep on looking at used Quattromats but subbing out is so much cheaper and I don't have the space for another machine

7/6/20       #6: Panel glue up options ...
MarkB Member

Not sure Im following your process or requirements accurately but if I am close my process would be:

1. Bring in material S2S SLR 1E oversize to leave you enough material to not have to do the initial process of "planing for relative thickness". That is a waste of time and a waste of chip handling in a shop your size. Bigger shop wouldnt care. Me I like making work not handling chips.

We pay $80/MBF for S2S and SLR1E so they handle all the chips and the off falls from straight lining. That would cost us hundreds and hundreds of time, tooling, and disposal dollars, in house.

2. Glue line rip on table saw with feeder

3. Glue up

4. Flatten (face joint) on CNC with as large a cutter as possible (we run a 3.5" 5z cutter)

5. Flip, surface other side

6. Face glue panels

7. Do whatevers next.

The CNC flattening is not the fastest in the world but its being done while were doing something else so its a good option as we too dont have room for other large tooling. Molder isnt going to help much. Leave your stock rough/oversized for thickness before its edge glued and flatten it all at once. Eliminate the planer everywhere you can if your CNC will handle the flattening (10HP minimum).

7/7/20       #7: Panel glue up options ...
Jared E

MarkB, do you do anything special to hold down the panels for flattening on CNC, aside from scraping glue off? I need to surface wood blanks almost dead flat on one side before they will stay put on the spoilboard.

7/7/20       #8: Panel glue up options ...
MarkB Member

We either put them face down (surface bottom side with squeezout/drips first) or paint scraper on the bottom side and run that side down whichever is flatter/sits better. We cage them in with scraps (melamine or laminate drops) on the cnc with vac. If one is a real rocker and wont sit relatively flat we just run a couple screws in the edge of the scraps we cage them in with and clip the heads off at an angle leaving a barb/point that we tap into the edge of the glueup and kick on the vac. That way the glueup is sitting there solid not being pulled down by the vac and we deck it off, then flip, vac hold down no scraps, deck other side.

7/7/20       #9: Panel glue up options ...
Jared E

Good trick, didn't know that one. Thanks.

7/9/20       #10: Panel glue up options ...
Nate Member

Thank you all - based on this thread, found a bigger outfit that has the equipment to do and gave me decent price for finished block. Will go that route until I get my volumes up..thank you!

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors