Wood NetWork

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Min. depth for tall freestanding shelving units

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Min. depth for tall freestanding shelving units

1/28/14       
Matt

A repeat customer has asked me to build some freestanding shelving units for home goods showroom in Ny. He wants a big chunky rustic unit 70 w x 80"h x 18"d. The units are to sit on cast iron foundry casters. They are also to have 3/4" ply backs that will have hang hooks screwed into from the back side, so he will have display options on from and back.

My worry is the stability of the units. I figure I will have about 16" between centers front to back on the casters. As said earlier they are 80" tall. Did I mention the frame and shelves are made of 8/4 red oak? If one starts to fall there will be no stopping it...

Thoughts?

1/28/14       #2: Min. depth for tall freestanding sh ...
Dave Edgerton  Member

Would be better if there was a skirt that was say 1/8 off the floor and the casters hidden inside. at least if it starts to tip there is something there to block it. Otherwise put a thin slot so it can be picked up with a dolly and moved. IN commercial setting i could see those things going over and killing someone.

1/29/14       #3: Min. depth for tall freestanding sh ...
David R Sochar Member

If this is for retail display, educate your customer and explain how his liability insurance will exclude this cabinet before it hits the floor and crushes that kid.

Use this as an opportunity to show your customer that your professional knowledge can prevent him from having problems, and propose a fix when you discuss the issues with the original design. A wider base is my first thought.

"Signing off" of some sort of document means nothing, as a liability lawyer will only see it as a clear sign all parties were aware of the potential hazard, but chose to officially ignore it. You will be sued, but since they follow the money, once you are cleaned out, they will go to your customer.

You might also check with your insurance carrier to see what your liability insurance says about these things.

Anti-Tip Article

1/29/14       #4: Min. depth for tall freestanding sh ...
Matt

Thanks for the replies. The shelves aren't technically in a retail setting. The showroom is to display new styles for national chain purchasers to peruse. There shouldn't be any children in there. That being said it is still a concern.

The customer definitely wants to see the casters so I can't hide them.

At this point I think we will need to modify design to include a deeper base, or make the entire unit deeper.

OR incorporate fasteners to tie them together and and make sure the customer understands to have at least 2 in a run tied together to make a 90 degree turn.... Make sense?

1/29/14       #5: Min. depth for tall freestanding sh ...
scott

The chunky rustic foundry look will allow you to put the casters on some sort of steel or wood "outrigger" construction to get a larger spread and still work into the industrial design theme, I'm assuming a lot here but that's how I'd initially approach it. Or, to get a little wacky, & if it's for display & not to be moved, attach it directly to the floor with some plates & rods out of sight & underneath the bottom floor. Goofy but effective.
18" is definitely too narrow, the offset of the caster will constrict this much more than the 16" OC hoped for.

1/29/14       #6: Min. depth for tall freestanding sh ...
Dave Edgerton  Member

what if you make them double sided to add depth and have more display area on the back side?

1/29/14       #7: Min. depth for tall freestanding sh ...
Matt

Scott, you're right, oc would actually be 14" with the casters I am looking at, but the outer edge would be 16". This is with the edge ofthe mounting plate flush with the front and rear edges of the bottom. I also like the outrigger idea.

Dave, customer wants a solid back so that either: hang Hooks can be attached so quilting can be displayed, or, the units can be positioned next to each other forming a solid "wall" that a bed can be set in front of to display bedding textiles.

I definitely like the idea of setting them up back to back. Possibly making 6-8 of these so some may be positioned this way.

Thanks. Matt

1/30/14       #8: Min. depth for tall freestanding sh ...
mark

Swivel casters? If so, the base could shrink further.

1/30/14       #9: Min. depth for tall freestanding sh ...
Matt

Good point Mark. Swivel casters are a definite no go.

1/31/14       #10: Min. depth for tall freestanding sh ...
Alan F.

Mount the casters to a 1/2" plate steel that is 18 x 70 and that will add 250+/- lbs. to the base of the fixture. If a mockup seems unstable go to 3/4" or 1" plate.

1/31/14       #11: Min. depth for tall freestanding sh ...
Matt

I hadn't thought of lowering the cog. Slick.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Excel Wood Products