Subject: Re: Balanced construction with mirror on one side

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Balanced construction with mirror on one side

4/28/14       
Fred Wildnauer  Member

Website: http://www.fawildnauerwoodwork.com

We had some large painted slab cabinet doors warp after the mirror was glued to one side. We used moisture resistant MDF as the substrate. The doors were painted on all sides and edges before the glass contractor attached the mirror. The mirror was attached using Gunther mirror mastic following Gunther's instructions. I am convinced that the warping was the cause of an unbalanced condition. I am trying to figure out a way to balance the mirror with something that won't double the weight of the door and allow installation of euro hinges. Any ideas?

4/28/14       #2: Balanced construction with mirror o ...
Brian T

You may want to try a heavy laminate on one side. Maybe a chem metal aluminum panel.

I would first be more inclined to go with a ply substrate over mdf. Moisture resistant won't help in this application.

If possible I would do a sample with 1'' veneer grade ply and mirror.

If you get that to cup from a mirror on the face I will be surprised.

Let us know how it goes.

4/29/14       #3: Balanced construction with mirror o ...
Fred Wildnauer  Member

Website: http://www.fawildnauerwoodwork.com

I have been asking around other shops in my area. Everybody has a different idea of what when wrong and how to fix it. One other cabinetmaker suggested your solution only using a uniform laminate product (baltic birch or apple ply). I hesitate to use a substrate with more wood as this is a bathroom with a large tub. I like your idea of the heavy laminate on the back. I am limited to 1" thick doors because we are using 170 degree euro hinges. One thought was to go the other direction and use hollow core construction with a heavy laminate on the back and mirror on the front. We could use inserta style hinges. We would adhere the heavy laminate on the back with the same mirror mastic used on the mirror. Thoughts?

4/29/14       #4: Balanced construction with mirror o ...
Fred Wildnauer  Member

Website: http://www.fawildnauerwoodwork.com

I forgot to mention that the mirror is 1/4" thick beveled so whatever this final solution is is limited in thickness and weight by that mirror. I think I will try a sample with the 1" as you suggest.

5/3/14       #5: Balanced construction with mirror o ...
JeffD

I had the same problem with a large closet door a couple years back. I had used 1/4" mirror w/ beveled edges glued on to mdf with adhesive from the glass shop and added a laminate backer to the back side. It warped after a couple months and I spent a lot of time trying to figure out how to force it back to straight….unsuccessfully.

In the end I re-made the whole door. I built a frame out of 4"-5" wide mahogany and then filled the centers in with a grid kind of like a torsion box construction. Glued it up and sanded it flat and then applied a laminate to one side and the mirror to the other. It came out flat and to my knowledge still is to this day. And I know this particular client will let me know if anything happened!

I uses SOSS hinges for this application though I'm sure euro hinges would work just fine with it as well. In my application the mirror had to look as if it was mounted to the wall and the application was too heavy for euro hinges. The bonus of the mahogany frame was that is was much lighter than the mdf so not as much stress on the hinges.

good luck,
JeffD

5/3/14       #6: Balanced construction with mirror o ...
Fred Wildnauer  Member

Website: http://www.fawildnauerwoodwork.com

Thanks. That is the solution I came up with too. I am going to use uniform laminate birch for the frame hollowed out so that it makes a 4" frame. I will fill the hollowed out section with structural honeycomb material (Nida-Core which is used in boat building). I am glad to hear that you used laminate on the back as that was my choice but I was not sure it was a good balance to the mirror. Did you glue the laminate on with mirror mastic? I was thinking I had to use the same glue on both sides. Mirror mastic works with laminate but it will be a bit tricky to get flat. I was thinking thicker material (acrylic sheet or solid surface) applied in a press. Thoughts anyone?

5/3/14       #7: Balanced construction with mirror o ...
JeffD

I used DMEasy spray contact for the laminate and had the glass guys glue the mirror with that same mastic.

I doubt it's really a balanced construction at all. I think it's more that the solid mahogany is much harder for the laminate to "pull" than mdf which has little resistance. Oh and my frame was only about 13/16" thick FWIW.

JeffD

5/3/14       #8: Balanced construction with mirror o ...
Fred Wildnauer  Member

Website: http://www.fawildnauerwoodwork.com

Am I reading you right in that you glued the mirror on with contact cement?

6/30/14       #9: Balanced construction with mirror o ...
Rich  Member

Website: http://www.hausmann.com

I would not glue the mirror to the door use either clips or aluminum moulding so that the mirror is loose and can move independent of the door.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Excel Wood Products