Safety Speed Cut Thermwood Corporation ECabinet Systems

Cabinetmaking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Critique my CNC-cut box designs

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Critique my CNC-cut box designs

2/20/18       
Gene Davis

And right up front, these are cut using eCabinets software, making use of blind dados.

And furthermore, they are always assembled on a jobsite by the carpenters who then install them.

Take a look at the two images, showing a base cabinet. The left and right sides are dadoed and grooved to house the tenons of the deck, top stretchers, middle stretcher, and 1/4" back.

The 5/8" rear nailer is pocket screwed to the sides. Zip-R screws are used at all joints. No glue anywhere. A few staples go in at the back, angled through the 1/4 piece and into sides and deck.

This means we are assembling using three tools: impact gun for screwing, stapler, and a drill for placing any needed holes.

Wall cabinets are similar except the top is one piece, there are no mid stretchers, and we do a bottom nailer in addition to the top one.


View higher quality, full size image (1031 X 896)


View higher quality, full size image (1125 X 807)

2/20/18       #3: Critique my CNC-cut box designs ...
Bill

I don’t see holes for the screws at the joints why?

2/20/18       #4: Critique my CNC-cut box designs ...
JP Member

This is Mozaik. The holes for the screws are really handy, I just run my stepdrill right in and use a confirmat.


View higher quality, full size image (1258 X 910)


View higher quality, full size image (1402 X 816)

2/20/18       #5: Critique my CNC-cut box designs ...
Gene Davis

I'm looking at this design because it is EXACTLY what CabParts does and they ship a lot of KD cabinets. The difference is this: CabParts end-bores parts so joinery is all by dowels, or if requested, dowels plus confirmats.

We can't end-bore. Parts are cut on a Thermwood router. The blind dados are doing what the dowels do for the CabParts design, and that is to align and register parts for ease of assembly.

2/20/18       #6: Critique my CNC-cut box designs ...
Jared Emery

Lots of ways to skin a cat, but here are a few suggestions to make life easier by dropping the staple gun and drill. Rattle gun method only:

1. Make your nailers identical to your drawer stretchers (eliminates pocket hole step). Tenon those suckers in.

2. Add CNC screw holes as per JP & Bill. I use a 4mm bit, but I'll hazard a guess that maybe you can't do this easily because eCabinets usually means there's a Thermwood with no drill block in the equation. It's worth getting a drill-chuck toolholder for predrilled screw holes though.

3. Eliminate the stopped dado's rear notch on stretchers & nailers (makes tenons longer to prevent twist during assembly, also identifies which edge to band)

4. Pop a couple holes through your top nailer to screw through it, through the back, and into the rear top stretcher. It locks the back in, which squares the cabinet and eliminates the need for staples.

2/24/18       #7: Critique my CNC-cut box designs ...
Derrek

Website: http://closetdr.com

We do very similar a few things we do different.
Pre drill assembly screw holes with 3mm bit in sides. This gives a standard as where and how many screws are needed for cabinet.
Finished ends held on with rafix.
Biggest thing we did was get rid of the 1/4" back and nailer. We went to 3/4" back. Less parts in cabinet, nest better yield, and price of material wasnt much different.
We also eliminated the nail gun, its easier to make a misteake and shoot a shiner, pre srilled screws go straight every time

2/25/18       #8: Critique my CNC-cut box designs ...
Geoffrey Wirth  Member

Website: Possessionwood.com

How are you processing the cabinet bottom with the tenon cut from the outside and a dado for the back inside? I just moved to cnc nested based production and am going to a 3/4” back after using 1/4” and nailer for years.

2/26/18       #9: Critique my CNC-cut box designs ...
Gene Davis

The bottom requires a part flip. The shop that cuts these adds a cost per flip, but it's pretty nominal and the cutter says it's pretty standard to be flipping some parts.

Using 5/8 mel for the nailers fits in with the CNC-cut drawerbox thing we do, which is a design using 5/8 for the four sides, and 1/4 for the bottoms. Part flips are needed for the drawerbox fronts and backs, but again, the cost is pretty minimal, and these d'boxes come in way under the cost of dovetailed wood boxes.

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Limtech Industries, Inc. Lamello