Architectural Woodworking

You are not logged in. [ Login ] Why log in
(NOTE: Login is not required to post)

Post a Response
The staff at WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at any WOODWEB Forum. Participants should undertake the use of machinery, materials and methods discussed after considerate evaluation, and at their own risk.
Your Name:
Your Website:
Email Address:
Subject: Re: Springback Formula For Arched Jambs

Message:

(read message guidelines).
Note: Do not use the below fields to advertise your business - only for links related to the discussion.
Thread Related Link URL:
Thread Related Link Title:
  To "point" to an image (picture) from another website, provide the URL (Web Address) of the file ( include ONE reference to http:// )
Thread Related Image URL:

Date of your Birth:

Upload a Thread Related File:
File Types: Image (gif-jpg-png-bmp), PDF, Sketchup, Video (mov avi wmv mpeg mpg mp4 ogg). (Image Upload Tips)

I have read the Site User Agreement and agree with the Terms

  <= Check to receive e-mail notification of responses

Message Thread:

Springback Formula For Arched Jambs

4/22/20       
Gary

Does anyone suggest a spring back formula that has been accurate ? Mr. B.H. Davis ?
I am referring to laminated arched head jambs and how to determine how much to over- bend the laminations to allow for how much they spring back when removed from the mold.

4/22/20       #2: Springback Formula For Arched Jambs ...
MarkB Member

No BH here but in the bit we've done there is no formula other than experience (we don't have) and doing a mock up and adjusting from there once, twice, or 42 times.

4/22/20       #3: Springback Formula For Arched Jambs ...
Leo G Member

Use thin enough material and there isn't a spring back. 1/16" works very well, 3/32" you get a bit of springback.

Plus it depends on the glue too. Using a stiff epoxy and you get much less. Use a PVA glue and you get more. If you use PVA let it dry for 12 hours.

4/23/20       #4: Springback Formula For Arched Jambs ...
pat gilbert

If you use plastic resin glue there will be very little spring back

4/23/20       #5: Springback Formula For Arched Jambs ...
Eddie

No formula here,We use 1/8'' layers of MDF with PVA glue for the top piece, very little spring back, but to help with the situation, we mount the casing to one side of the Casing opening, that corrects any little spring.

4/23/20       #6: Springback Formula For Arched Jambs ...
Fred Frehner Member

Website: http://www.rivercity.ca

On low flat arches for exterior doors we use 1/4" laminations with PUR glue.
Our head jambs are for most of it 2 part units 3/4" inner and 1"1/2 outer jamb.
For the spring back on the outer jamb we use,
-the with of jamb (part) / 3 X radius.
-For the spring back on the inner jamb we use,
2 X with of jamb (part) / 3Xradius.
As for any heavy curves arches or round jambs we use 1/8 laminations.
There are just to many factors to have a formula that fits for all, and there is simply no substitutes for experience.

4/23/20       #8: Springback Formula For Arched Jambs ...
David R Sochar Member

You will be chasing the elusive formula for some time, since there is none. Even if you have one that works, change the radius, or the species, or any variable, and it is no longer predictive.

We solved this one 30 years ago when faced with building 40 interior doors with arched head jambs - in about 7 or 8 different radii. Bent lamination was too variable, so we came up with something else.

Brick laid and lined head jambs is the better way. Saw (or pattern shape) out a bunch of scrap on radius, clip the ends so they butt on radius, and stack them up, staggering the joints (brick laid). Once that is glued to the correct over width and chord length, the face can be cleaned up with scrapers and sanders. Then a 1/8" (or thinner, or thicker) piece of nice wood is clamped to the assembly with cauls and allowed to set up.

We made a jig (named the "Angel" jig after its inventor) to facilitate clamping up these brick laid heads. We also made a "swingometer" to bandsaw radii reliably and accurately. This not used much now, as I prefer to just use the shaper to size the inside radius on radius perfectly. One can also make the curved elements over size and glue them all up, then saw out on radius.

The photo below shows the jig, tho that is an unusual arched head assembly, and not a very good representation of what I am talking about.....

This makes a rigid head, even at 3/4" thick. Do not try to force thicker wood liners onto thinner brick laid arches. This can distort your otherwise rigid head. Keep it all easy.

Some might call it an "engineered" arched head.


View higher quality, full size image (900 X 675)

4/25/20       #9: Springback Formula For Arched Jambs ...
BH Davis  Member

Website: http://www.bhdavis.net

Gary,

I apologize for the delay in seeing this thread. Now that I'm retired I don't check in on Woodweb every day any more. It seems I'm busier in retirement than I ever was when working !!

Giving advice on radius work is now awkward for me because as is typically the case I have a non-compete agreement with the new owner of my company. So where in the past I could measure what I wanted to share against my own business interests now it is against someone else's interests so I'm a bit more restricted.

However I will send you a PM and see if I can give some guidance on the spring back issue. Publicly I'll just say that for years we kept a record of the spring back we got with different materials, radii and adhesives. Since curved jambs were made on a near daily basis you can imagine that list what quite extensive.

BH Davis

4/25/20       #10: Springback Formula For Arched Jambs ...
Gary

So I completed my arched jamb and by a hunch I over-bent it by 3/16". After taking it off the mold the spring back was a little less than an 1/8" which will be fine. I added the data to my list of laminations and will be using it for reference. Thank you all for your input !

 

Buy & Sell Exchanges | Forums | Galleries | Site Map

FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Sponsors

    Become a Sponsor today!