Torsion Box Doors

2/25/16       
SG

My shop has a job involving a fair number of good-size doors (4'-5.5' w. x 9.5' h.) which we were intending to construct as torsion boxes with shop-sawn veneer for rails/stiles and panels to simulate a typical cope/stick door. We have already built a number of radius doors for this job with this technique, and it has worked admirably, though is admittedly time-consuming. There is a desire on the part of those overseeing the job to make the process more expedient by substituting a single solid piece on top of the core (which is Baltic Birch, by the way) to simulate the stiles/rails, rather than building up plywood and veneering, and also by using a single piece of .25" stock for the panels, rather than laminating two .125" pieces, as per the radius doors. I am concerned on both counts that this will compromise the stability of the doors, esp. in the case of the rail/stile pieces, which would be something like .375-.5" thick.

Attached pdf shows how radius doors were built.

I would appreciate any informed opinions on the subject.

Click the link below to download the file included with this post.

Door_Section.pdf

2/26/16       #2: Torsion Box Doors ...
David R Sochar Member

I have always made my radius plan doors in solids. Flat stiles, a bit over thick, sawn rail stock, often with 1/8" veneer facings, and stave built panels. Once assembled the stiles can be handplaned to a slight radius.

"There is a desire on the part of those overseeing the job to make the process more expedient..." Tell me about it. It just is not an expedient process, in my opinion. If we did it every day, we could get better, but we don't have the call for it.

Your method is built up - smaller parts assembled and overlaid to get to the goal. My method with solids is dealing with larger parts and reducing them to get to the same place. Two basic forms of working wood. Both work. Neither can be called expedient, though.

I will say that the solids method is strongly derived from the same way we make all our conventional doors. Mortise and tenon, cope and stick profiles, etc. This makes it remarkably familiar to the maker so it is not as foreign as lots of loose, thin parts to get there. This helps quite a bit.

Conventional build methods also allow the same design elements to be easily incorporated into the door so it can mate well with a run of more conventional doors in the same project.

The photos show one of a pair of 2-14 x 42 x 96 Alder pocket doors. They look good, but the compound curve panel raise was one hair raising and losing set-up and effort.


View higher quality, full size image (1800 X 1350)


View higher quality, full size image (1350 X 1800)

3/1/16       #3: Torsion Box Doors ...
Mark

You didn't say what species the veneer was, and do I understand correctly, the center core is Baltic birch?
Anyway, can you lay up the S&R stock and panels separately and assemble in the usual fashion? Might save you some time.

3/3/16       #4: Torsion Box Doors ...
Gary

I'll say it again David: You still need to consider teaching a class and in this case it would be radius doors! If you don't have the space maybe team up with Calhoon ?
Great work and great photos; thanks for sharing.

3/3/16       #5: Torsion Box Doors ...
SG

I appreciate the responses thus far, but none speak to the primary question, which is the concern about replacing the built-up plywood and veneer that simulates rails and stiles with a single solid piece of wood on the order of a .5" thick, as well as having .25" single-piece panels. Perhaps I should have been more explicit - but we are done with the radius doors and will now be building a number of flat doors that are 4'-5.5' wide, and they've been specified using this torsion box construction, not solid (the narrower doors will be solid).

Though there are a lot of parts involved, the torsion box allows a large, stable doors to be built with few heroics (can't imagine how much a 2.25" x 5.5' x 9.5' door in solid white oak would weigh) and the results are very good and very predictable. Being able to resaw solid stock and keep color and grain going on a door of this size is really a nice aesthetic feature, too.

I'm concerned that allowing expedience to dictate a less-than-best-practice of laminating thicker parts as if they were veneer with come back to bite us on this.

3/3/16       #6: Torsion Box Doors ...
David R Sochar

My point concerned the fact that it is best to try for continuity in process throughout a project or product.

You mention these doors are 'specified' with thick layers of "veneer" so that may ease your concerns, but your question is valid.

In my experience, and as born out here and elsewhere, veneer becomes more like solid wood around 1/4" thick. Exposure, species, cut, substrates, finish and probably more can affect that number quite a bit. As well as EMC, the relative humidity where it will live, and the moisture content once it leaves the shop.

There are no absolutes. I have gotten away with things I should not have, and have been bit where I felt safe.

I can say that what you describe is out of my comfort zone for most situations. I appreciate the weight savings attempt, but a fork truck should be hero along with some hefty straps. I am not sure you are saving that much weight.

3/4/16       #7: Torsion Box Doors ...
Kevin Jenness

Given that the "stiles" appear to be only 4" wide you can probably use a solid buildup there without incident, assuming careful milling and appropriate MC. I would be more suspicious of the 1/4" buildup of the "panels" inviting surface checking due to excess thickness, whether one or two layers of solid wood. Obviously the proof is in the pudding and you have had success with the first iteration. If you are comfortable with that thickness, I don't think using one layer will make any difference. For a far more laborious but less problematic solution you could make the "panels" of edgebanded veneered mdf.

I will say I would not choose baltic birch as the sandwich skins as it is so often squirrely, but it seems to work for you. What are you using for the core lamination? I have used foam, expanded cardboard and Plascore in the past for different applications.

3/4/16       #8: Torsion Box Doors ...
Kevin Jenness

(What I meant to say) The stile/rail buildup is problematic in solid wood and your original layup is technically more correct, but you can probably get away with it if limited to 4" width, depending on the species and all the other considerations David mentions. I would be more concerned with wider sections laminated to a stable core.

3/4/16       #9: Torsion Box Doors ...
Mark

Like David said, at that thickness the materials are prone to move like solid stock.

If they want the materials to be that thick, get them to sign off on it. At least you won't have to cover the doors if it fails and cracks

3/8/16       #10: Torsion Box Doors ...
SG

To respond to latest points:

1 - Weight savings is pretty significant, actually. A rough calculation of these doors in solid WO yields 135 lbs. - though we haven't weighed the torsion box versions, they are certainly no more than 80 lbs. With a hinged (i.e. cantilevered) structure, the lesser weight is a real boon for ultimate stability of the door, which also benefits from having the entirety of the "panel" playing a role in the diaphragm, something a solid wood panel does not.

2 - We used Okoume ply for skins - this is a nice product, if any of you are unfamiliar, mostly sold to the boat-building crowd. Available in larger than standard dimensions, a lot of different thicknesses. It is fairly soft, but is a nice flat, consistent panel.

3 - Core is a 6" grid of 1" thick Baltic Birch, parts all notched to snap together off the router. We use a hinge mortising bit w/bearing to square up notches. Important to make the fit just a little loose (.015), otherwise parts start wedging themselves into curves.

4 - Stiles are actually 5.25" wide.

Thank you for the thoughtful responses. I agree that the thicker "veneers" are likely to be problematic, and will be sure they understand it will be their oversight if there are issues with them.

3/8/16       #11: Torsion Box Doors ...
Kevin Jenness

I misunderstood the role of the baltic birch. That sounds like a good layup. I used 6mm ocoume and 4" foam last year to build a pair of 4 'x 7' 6" doors skinned with western red cedar. Nice material to work with.

I like that method of assembling the core grid. Wouldn't you save time cutting the notches deeper or cutting dogbone notches on the router to avoid the squaring operation? I have done the notching on ganged parts with a dado set on a sliding saw, but the cnc router is no doubt the way to go, especially with curved doors.


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory