Architectural panel what?

5/1/19       
Paul Chabot Member

To cut architectural panels [EPS, Foam, MDF] with a wave pattern [on a router] and coat them with a texture/chop gun using a polymer - plaster, stucco or concrete. Laminate grass cloth or veneer onto a wave panel using vacuum bag technology.
What do ya think?

5/3/19       #2: Architectural panel what? ...
MarkB Member

Sounds like its kinda been done. We cut texture panels fairly often but at least for us in the architecture world its been moved on. Its a bummer as they are fun do design and nice to cut. Tons of work to finish. And a lot of technical issues depending on the material chosen.

5/3/19       #3: Architectural panel what? ...
Paul Chabot Member

I think there are lots of interpretations of this form of millwork. We install much 3form. They sold 25 million dollars of architectural panels here in Florida last year. I think this type of work is selling plus 40 million per year here in Fl. Good to know I am not the only one who sees opportunity.

5/6/19       #4: Architectural panel what? ...
MarkB Member

I dont disagree but there is way more that just the panels with regards to 3form. Im not saying its not a market to pursue and you may have the architects ear and the capacity to implement all the samples, engineering, fixturing and mounting, drawings, submittals, and so on. So run with it.

My market for this is usually someone looking for something completely unique and we still have to come up with the engineering, finish samples, mockups, and so on, for a non-production run where the architect or designer has for the most part seen something they think is cool but dont want to pay the euro/current offering, prices and are trying to source locally for a modest project cheaper.

The panels and panel processing to me is about 1/10 the cost of the panel. The marketing, sales, glossy flyers, handouts, physical samples, engineering and engineered approvals, are the remaining 70% leaving you scraping for your 20.

5/6/19       #5: Architectural panel what? ...
Paul Chabot Member

We have samples in more than a dozen architects hands here in Tampa bay. The layered complexity of our panels is unique. You are correct about 3Form, a lot of product is injected Lexan type stuff. Outside of my manufacturing box. We are not in the phone book and we do not advertise.

5/6/19       #6: Architectural panel what? ...
Hen Bob Member

So what is the goal here? To get others to start making them or to sell your product?

5/6/19       #7: Architectural panel what? ...
MarkB

Hen Bob, that's pretty much been my head scratcher. Every architect within 30 miles of our shop is aware they can have one off of a kind panels in their jobs for clients and it's rare. 3form here is used in elevator cabs.

5/21/19       #8: Architectural panel what? ...
Craig Burgess Member

Website: https://protoolsadviser.com/best-table-saw/

I made wood panels for one Israeli businessman, he really loves the wave-like style. This really does not complicate the work, plus there is a demand for woodworkers who can do it. I had to buy a new cutting table (link below) but keep in mind that it produces 4800 RPM with 15 amps of power.

Best table saw

5/23/19       #9: Architectural panel what? ...
Hen Bob Member

This makes much more sense now..

5/23/19       #10: Architectural panel what? ...
Paul Chabot Member

I was wondering about what other (CNC) shops thought about this kind of 3d architectural panel work. I just saw "broken glass" panels on a job. There were 5 sheets of painted MDF. What $100 in materials? The client paid $5000 for them. It made me curious about going beyond MDF door and cabinet part production. Thank You all for commenting.


View higher quality, full size image (3241 X 2210)


Post a Response
  • Notify me of responses to this thread
  • Subscribe to email updates on this Forum
  • To receive email notification of additions to this forum thread,
    enter your name and email address, and then click the
    "Keep Me Posted" button below.

    Please Note: If you have posted a message or response,
    do not submit this request ... you are already signed up
    to receive notification!

    Your Name:
    E-Mail Address:
    Enter the correct numbers into the field below:
     

    Date of your Birth:



    Return to top of page

    Buy & Sell Exchanges | Forums | Galleries | Site Map

    FORUM GUIDELINES: Please review the guidelines below before posting at WOODWEB's Interactive Message Boards (return to top)

  • WOODWEB is a professional industrial woodworking site. Hobbyist and homeowner woodworking questions are inappropriate.
  • Messages should be kept reasonably short and on topic, relating to the focus of the forum. Responses should relate to the original question.
  • A valid email return address must be included with each message.
  • Advertising is inappropriate. The only exceptions are the Classified Ads Exchange, Machinery Exchange, Lumber Exchange, and Job Opportunities and Services Exchange. When posting listings in these areas, review the posting instructions carefully.
  • Subject lines may be edited for length and clarity.
  • "Cross posting" is not permitted. Choose the best forum for your question, and post your question at one forum only.
  • Messages requesting private responses will be removed - Forums are designed to provide information and assistance for all of our visitors. Private response requests are appropriate at WOODWEB's Exchanges and Job Opportunities and Services.
  • Messages that accuse businesses or individuals of alleged negative actions or behavior are inappropriate since WOODWEB is unable to verify or substantiate the claims.
  • Posts with the intent of soliciting answers to surveys are not appropriate. Contact WOODWEB for more information on initiating a survey.
  • Excessive forum participation by an individual upsets the balance of a healthy forum atmosphere. Individuals who excessively post responses containing marginal content will be considered repeat forum abusers.
  • Responses that initiate or support inappropriate and off-topic discussion of general politics detract from the professional woodworking focus of WOODWEB, and will be removed.
  • Participants are encouraged to use their real name when posting. Intentionally using another persons name is prohibited, and posts of this nature will be removed at WOODWEB's discretion.
  • Comments, questions, or criticisms regarding Forum policies should be directed to WOODWEB's Systems Administrator
    (return to top).

    Carefully review your message before clicking on the "Send Message" button - you will not be able to revise the message once it has been sent.

    You will be notified of responses to the message(s) you posted via email. Be sure to enter your email address correctly.

    WOODWEB's forums are a highly regarded resource for professional woodworkers. Messages and responses that are crafted in a professional and civil manner strengthen this resource. Messages that do not reflect a professional tone reduce the value of our forums.

    Messages are inappropriate when their content: is deemed libelous in nature or is based on rumor, fails to meet basic standards of decorum, contains blatant advertising or inappropriate emphasis on self promotion (return to top).

    Libel:   Posts which defame an individual or organization, or employ a tone which can be viewed as malicious in nature. Words, pictures, or cartoons which expose a person or organization to public hatred, shame, disgrace, or ridicule, or induce an ill opinion of a person or organization, are libelous.

    Improper Decorum:   Posts which are profane, inciting, disrespectful or uncivil in tone, or maliciously worded. This also includes the venting of unsubstantiated opinions. Such messages do little to illuminate a given topic, and often have the opposite effect. Constructive criticism is acceptable (return to top).

    Advertising:   The purpose of WOODWEB Forums is to provide answers, not an advertising venue. Companies participating in a Forum discussion should provide specific answers to posted questions. WOODWEB suggests that businesses include an appropriately crafted signature in order to identify their company. A well meaning post that seems to be on-topic but contains a product reference may do your business more harm than good in the Forum environment. Forum users may perceive your references to specific products as unsolicited advertising (spam) and consciously avoid your web site or services. A well-crafted signature is an appropriate way to advertise your services that will not offend potential customers. Signatures should be limited to 4-6 lines, and may contain information that identifies the type of business you're in, your URL and email address (return to top).

    Repeated Forum Abuse: Forum participants who repeatedly fail to follow WOODWEB's Forum Guidelines may encounter difficulty when attempting to post messages.

    There are often situations when the original message asks for opinions: "What is the best widget for my type of shop?". To a certain extent, the person posting the message is responsible for including specific questions within the message. An open ended question (like the one above) invites responses that may read as sales pitches. WOODWEB suggests that companies responding to such a question provide detailed and substantive replies rather than responses that read as a one-sided product promotion. It has been WOODWEB's experience that substantive responses are held in higher regard by our readers (return to top).

    The staff of WOODWEB assume no responsibility for the accuracy, content, or outcome of any posting transmitted at WOODWEB's Message Boards. Participants should undertake the use of machinery, materials and methods discussed at WOODWEB's Message Boards after considerate evaluation, and at their own risk. WOODWEB reserves the right to delete any messages it deems inappropriate. (return to top)


  • Forum Posting Help
    Your Name The name you enter in this field will be the name that appears with your post or response (return to form).
    Your Website Personal or business website links must point to the author's website. Inappropriate links will be removed without notice, and at WOODWEB's sole discretion. WOODWEB reserves the right to delete any messages with links it deems inappropriate. (return to form)
    E-Mail Address Your e-mail address will not be publicly viewable. Forum participants will be able to contact you using a contact link (included with your post) that is substituted for your actual address. You must include a valid email address in this field. (return to form)
    Subject Subject may be edited for length and clarity. Subject lines should provide an indication of the content of your post. (return to form)
    Thread Related Link and Image Guidelines Thread Related Links posted at WOODWEB's Forums and Exchanges should point to locations that provide supporting information for the topic being discussed in the current message thread. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related Link that directs visitors to an area with inappropriate content will be removed. WOODWEB reserves the right to delete any messages with links or images it deems inappropriate. (return to form)
    Thread Related File Uploads Thread Related Files posted at WOODWEB's Forums and Exchanges should provide supporting information for the topic being discussed in the current message thread. Video Files: acceptable video formats are: .MOV .AVI .WMV .MPEG .MPG .MP4 (Image Upload Tips)   If you encounter any difficulty when uploading video files, E-mail WOODWEB for assistance. The purpose of WOODWEB Forums is to provide answers, not to serve as an advertising venue. A Thread Related File that contains inappropriate content will be removed, and uploaded files that are not directly related to the message thread will be removed. WOODWEB reserves the right to delete any messages with links, files, or images it deems inappropriate. (return to form)
    Doucet Machinery ExFactory